Ultrathin silicon dioxide layers with a low leakage current density formed by chemical oxidation of Si

被引:85
作者
Asuha
Kobayashi, T
Maida, O
Inoue, M
Takahashi, M
Todokoro, Y
Kobayashi, H
机构
[1] Osaka Univ, Inst Sci & Ind Res, Osaka 5670047, Japan
[2] Japan Sci & Technol Corp, CREST, Osaka 5670047, Japan
[3] Matsushita Elect Ind Co Ltd, Semicond Co, Technol Liaison Off, Minato Ku, Tokyo 1058586, Japan
关键词
D O I
10.1063/1.1517723
中图分类号
O59 [应用物理学];
学科分类号
摘要
Chemical oxidation of Si by use of azeotrope of nitric acid and water can form 1.4-nm-thick silicon dioxide layers with a leakage current density as low as those of thermally grown SiO2 layers. The capacitance-voltage (C-V) curves for these ultrathin chemical SiO2 layers have been measured due to the low leakage current density. The leakage current density is further decreased to similar to1/5 (cf. 0.4 A/cm(2) at the forward gate bias of 1 V) by post-metallization annealing at 200degreesC in hydrogen. Photoelectron spectroscopy and C-V measurements show that this decrease results from (i) increase in the energy discontinuity at the Si/SiO2 interface, and (ii) elimination of Si/SiO2 interface states and SiO2 gap states. (C) 2002 American Institute of Physics.
引用
收藏
页码:3410 / 3412
页数:3
相关论文
共 17 条
[1]   The valence band alignment at ultrathin SiO2/Si interfaces [J].
Alay, JL ;
Hirose, M .
JOURNAL OF APPLIED PHYSICS, 1997, 81 (03) :1606-1608
[2]  
[Anonymous], 2001, INT TECHNOLOGY ROADM
[3]   Decrease in the leakage current density of Si-based metal-oxide-semiconductor diodes by cyanide treatment [J].
Asano, A ;
Asuha ;
Maida, O ;
Todokoro, Y ;
Kobayashi, H .
APPLIED PHYSICS LETTERS, 2002, 80 (24) :4552-4554
[4]   Effects of postmetallization annealing on ultrathin SiO2 layer properties [J].
Asuha ;
Yuasa, T ;
Maida, O ;
Kobayashi, H .
APPLIED PHYSICS LETTERS, 2002, 80 (22) :4175-4177
[5]   Direct extraction of the electron tunneling effective mass in ultrathin SiO2 [J].
Brar, B ;
Wilk, GD ;
Seabaugh, AC .
APPLIED PHYSICS LETTERS, 1996, 69 (18) :2728-2730
[6]   CHEMICAL-KINETICS OF HYDROGEN AND (111) SI-SIO2 INTERFACE DEFECTS [J].
BROWER, KL ;
MYERS, SM .
APPLIED PHYSICS LETTERS, 1990, 57 (02) :162-164
[7]   ELECTRICAL CHARACTERISTICS OF AL/SIO2/N-SI TUNNEL-DIODES WITH AN OXIDE LAYER GROWN BY RAPID THERMAL-OXIDATION [J].
DEPAS, M ;
VANMEIRHAEGHE, RL ;
LAFLERE, WH ;
CARDON, F .
SOLID-STATE ELECTRONICS, 1994, 37 (03) :433-441
[8]   MICROSCOPIC STRUCTURE OF THE SIO2/SI INTERFACE [J].
HIMPSEL, FJ ;
MCFEELY, FR ;
TALEBIBRAHIMI, A ;
YARMOFF, JA ;
HOLLINGER, G .
PHYSICAL REVIEW B, 1988, 38 (09) :6084-6096
[9]   Oxide thickness dependence of energy shifts in the Si 2p levels for the SiO2/Si structure, and its elimination by a palladium overlayer [J].
Kobayashi, H ;
Kubota, T ;
Kawa, H ;
Nakato, Y ;
Nishiyama, M .
APPLIED PHYSICS LETTERS, 1998, 73 (07) :933-935
[10]   Quantum-mechanical modeling of electron tunneling current from the inversion layer of ultra-thin-oxide nMOSFET's [J].
Lo, SH ;
Buchanan, DA ;
Taur, Y ;
Wang, W .
IEEE ELECTRON DEVICE LETTERS, 1997, 18 (05) :209-211