Synthesis and photoluminescent properties of YVO4:Eu3+ nano-crystal phosphor prepared by Pechini process

被引:68
作者
Chang, Yee-Shin [3 ]
Huang, Feng-Ming [3 ]
Tsai, Yeou-Yih [2 ]
Teoh, Lay-Gaik [1 ]
机构
[1] Natl Pingtung Univ Sci & Technol, Dept Mech Engn, Neipu 912, Pingtung, Taiwan
[2] Kao Yuan Univ, Dept Elect Engn, Kaohsiung 821, Taiwan
[3] Natl Formosa Univ, Dept Elect Engn, Huwei 632, Yunlin, Taiwan
关键词
Yttrium vanadate; Europium; Photoluminescence; Phosphor; Pechini process; LUMINESCENT PROPERTIES; CHEMICAL SYNTHESIS; ZNGA2O4; EU; TEMPERATURE; INTENSITIES; YVO4-EU3+; FILMS; LASER; SM3+;
D O I
10.1016/j.jlumin.2009.05.020
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
A sol-gel technique emphasizing the Pechini process has been employed for the preparation of nano-crystal Eu3+-doped YVO4 phosphor. The precursor powders were heated at 800 degrees C for 3 h to obtain good crystallinity with better luminescence. XRD results indicate that the second phase is not presented when the Eu3+ ion concentration is increased up to 50 mol%. The absorption and photoluminescent (PL) studies indicated that the energy is absorbed first by the host and then transferred to the emitting level of the Eu3+ ions. Excitation at 318 nm in terms of Eu3+ concentrations in YVO4 powders shows that the YVO4 phosphors display bright red luminescence at about 618 nm belonging to the D-5(0) -> F-7(2) electric dipole transition, and a weak band in the orange region of the D-5(0) -> F-7(1) transition at 594 nm. In addition, the time-resolved D-5(0) -> F-7(2) transition presents a single-exponential decay behavior, revealing the decay mechanism of the D-5(0) -> F-7(2) transition is a single decay component between Eu3+ ions only. The saturation of the emission intensity excited by the CTS when the Eu3+ concentration is 10 mol%. The concentration quenching is active when the Eu3+ concentration is larger than 10 mol%, and the critical distance is about 5.75 angstrom. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:1181 / 1185
页数:5
相关论文
共 46 条