摘要
Purpose This study aimed to investigate the effect of five porcelain repair systems on shear bond strength in composite and zirconia infrastructures and to identify the bond failure mode after thermocycling. Materials and Methods Disk-shaped zirconia samples (n=50) were divided into five groups (n=10) according to repairing system type. Each repair system was applied to the zirconium samples and a hybrid composite was used for repairing. Shear bond testing of all groups was carried out using a universal testing machine after thermocycling. Results Repair systems demonstrated no significant difference in repairing zirconia except Single Bond. Single Bond was the weakest in repairing the infrastructures. The highest and lowest mean bond strength values for the zirconia groups were 18,91 MPa and 3,63 MPa, respectively. Conclusion The three repair systems, Ivoclar, Clearfil, and Bisco, were more effective than the Single Bond and Ultradent repair systems in repairing zirconia, and their bond failure modes were both mixed and adhesive.
引用
收藏
页码:55 / 60
页数:6
相关论文
共 46 条
[1]   Influence of different surface treatments on the short-term bond strength and durability between a zirconia post and a composite resin core material [J].
Akgungor, Gokhan ;
Sen, Deniz ;
Aydin, Murat .
JOURNAL OF PROSTHETIC DENTISTRY, 2008, 99 (05) :388-399
[2]   LONG-TERM RESIN BONDING TO ZIRCONIA CERAMIC WITH A NEW UNIVERSAL PRIMER [J].
Attia, Ahmed ;
Kern, Matthias .
JOURNAL OF PROSTHETIC DENTISTRY, 2011, 106 (05) :319-327
[3]   Influence of surface conditioning and cleaning methods on resin bonding to zirconia ceramic [J].
Attia, Ahmed ;
Lehmann, Frank ;
Kern, Matthias .
DENTAL MATERIALS, 2011, 27 (03) :207-213
[4]  
Barragan Goncalo, 2014, Oral Health Dent Manag, V13, P155
[5]  
Burke F J T, 2002, Dent Update, V29, P398
[6]   Effect of surface pre-treatments on the zirconia ceramic-resin cement microtensile bond strength [J].
Casucci, Alessio ;
Monticelli, Francesca ;
Goracci, Cecilia ;
Mazzitelli, Claudia ;
Cantoro, Amerigo ;
Papacchini, Federica ;
Ferrari, Marco .
DENTAL MATERIALS, 2011, 27 (10) :1024-1030
[7]   Comparison of Alternative Adhesive Cementation Concepts for Zirconia Ceramic: Glaze Layer vs Zirconia Primer [J].
Cura, Cenk ;
Oezcan, Mutlu ;
Isik, Guel ;
Saracoglu, Ahmet .
JOURNAL OF ADHESIVE DENTISTRY, 2012, 14 (01) :75-82
[8]   Characterization of glass-infiltrated alumina-based ceramics [J].
Della Bona, Alvaro ;
Mecholsky, John J., Jr. ;
Barrett, Allyson A. ;
Griggs, Jason A. .
DENTAL MATERIALS, 2008, 24 (11) :1568-1574
[9]  
Della Bona A, 2008, J AM DENT ASSOC, V139, p8S
[10]  
Prado Ricardo Alves do, 2005, Braz. Dent. J., V16, P202