The effects of four primers and two cement types on the bonding strength of zirconia

被引:2
作者
Cao, Yang [1 ]
Zhang, Jia-Feng [2 ]
Ou, Xin [2 ]
Zhang, Bao [2 ]
Chen, Lei [3 ]
Deng, Xue-Hua [4 ]
机构
[1] Cent South Univ, Med Equipment Dept, Xiangya Hosp, Changsha, Peoples R China
[2] Cent South Univ, Natl Engn Lab High Efficiency Recovery Refractory, Sch Met & Environm, Changsha, Peoples R China
[3] Cent South Univ, Ctr Stomatol, Xiangya Hosp, Changsha 410008, Peoples R China
[4] Changsha Stomatol Hosp, Dept Prosthodont, Changsha, Peoples R China
关键词
Zirconia; primer; cement; thermocycling; bonding strength; SURFACE-TREATMENT; RESIN CEMENT; HEMA-FREE; CERAMICS; RELIABILITY; COMPOSITE; MONOMER;
D O I
10.21037/atm-21-4909
中图分类号
R73 [肿瘤学];
学科分类号
100214 ;
摘要
Background: To evaluate the effects of four ceramic primers and two cement types on the bonding strength and durability between zirconia and resin cement. Methods: A total of 115 polished and air-abraded zirconia blocks were randomly divided into five groups (with 23 in each group) to test the performance of various primers. Meanwhile, all primer samples were divided into two subgroups randomly to measure the difference between the two cement types. Group No treat - Clearfil SA Cement (NT-C); group No treat - RelyX Unicem Cement (NT-U); group Z-Prime Plus - Clearfil SA Cement (ZPP-C); group Z-Prime Plus - RelyX Unicem Cement (ZPP-U); group Rely X Ceramic Primer - Clearfil SA Cement (RCP-C); group Rely X Ceramic Primer - RelyX Unicem Cement (RCP-U); group Clearfil Ceramic Primer - Clearfil SA Cement (CCP-C); group Clearfil Ceramic Primer RelyX Unicem Cement (CCP-U); group Monobond-S - Clearfil SA Cement (MS-C); group Monobond-S RelyX Unicem Cement (MS-U). According to the type of cement, the specimens were randomly selected for electron microscope scanning and energy spectrum analysis, and the tightness of zirconium porcelain resin adhesive interface was observed. The bonding strength of different adhesives and aging experiments were tested by shear test mode, and the shear strength of each experimental group was analyzed by one variable three factor analysis of variance. Results: All primers in the treated groups maintained a pristine structure without micro-crack, while the non-primer treatment sample exhibited obvious micro-cracks. Furthermore, among the four primers, the sample treated with Clearfil Ceramic Primer (CCP) obtained the highest bonding strength, with a statistically significant difference (P<0.05). However, cohesive failure mainly occurred in the CCP group before thermal cycles, and mixed failure occurred after thermal cycles. Conclusions: CCP is the superior primer, and can improve the bonding strength between zirconia and resin cement. Because the thermal cycles have a significantly adverse effect on the shear bond strength, CCP can be helpful in improving the durability of the zirconia bonding strength. Furthermore, the two cement types exhibited a similar bonding performance for zirconia.
引用
收藏
页数:14
相关论文
共 33 条
[1]  
Aboushelib Moustafa N, 2008, J Prosthodont, V17, P401, DOI 10.1111/j.1532-849X.2008.00306.x
[2]   The potential of novel primers and universal adhesives to bond to zirconia [J].
Amaral, Marina ;
Belli, Renan ;
Cesar, Paulo Francisco ;
Valandro, Luiz Felipe ;
Petschelt, Anselm ;
Lohbauer, Ulrich .
JOURNAL OF DENTISTRY, 2014, 42 (01) :90-98
[3]   The bond strength of the resin-to-zirconia interface using different bonding concepts [J].
Behr, Michael ;
Proff, Peter ;
Kolbeck, Carola ;
Langrieger, Sabine ;
Kunze, Johannes ;
Handel, Gerhard ;
Rosentritt, Martin .
JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2011, 4 (01) :2-8
[4]  
Bottino MA, 2005, INT J PROSTHODONT, V18, P60
[5]   STABILITY OF THE BOND BETWEEN TWO RESIN CEMENTS AND AN YTTRIA-STABILIZED ZIRCONIA CERAMIC AFTER SIX MONTHS OF AGING IN WATER [J].
da Silva, Eduardo M. ;
Miragaya, Luciana ;
Sabrosa, Carlos Eduardo ;
Maia, Lucianne C. .
JOURNAL OF PROSTHETIC DENTISTRY, 2014, 112 (03) :568-575
[6]  
Guo L, 2010, INT J STOMATOL, V37, P651
[7]   Technique sensitivity associated with air-drying of HEMA-free, single-bottle, one-step self-etch adhesives [J].
Hiraishi, N. ;
Breschi, L. ;
Prati, C. ;
Ferrari, M. ;
Tagami, J. ;
King, N. M. .
DENTAL MATERIALS, 2007, 23 (04) :498-505
[8]   Effect of air-drying and solvent evaporation on the strength of HEMA-rich versus HEMA-free one-step adhesives [J].
Ikeda, Takatsumi ;
De Munck, Jan ;
Shirai, Kenichi ;
Hikita, Kazuhiro ;
Inoue, Satoshi ;
Sano, Hidehiko ;
Lambrechts, Paul ;
Van Meerbeek, Bart .
DENTAL MATERIALS, 2008, 24 (10) :1316-1323
[9]   Durable bonding to mechanically and/or chemically pre-treated dental zirconia [J].
Inokoshi, Masanao ;
Kameyama, Atsushi ;
De Munck, Jan ;
Minakuchi, Shunsuke ;
Van Meerbeek, Bart .
JOURNAL OF DENTISTRY, 2013, 41 (02) :170-179
[10]   Bonding to oxide ceramics-Laboratory testing versus clinical outcome [J].
Kern, Matthias .
DENTAL MATERIALS, 2015, 31 (01) :8-14