Effect of SiC nanoparticle concentration on the properties of oxide films formed on Ti-10V-2Fe-3Al alloy

被引:14
作者
Li, Songmei [1 ]
Yao, Wenhui [1 ]
Liu, Jianhua [1 ]
Yu, Mei [1 ]
Ma, Kun [1 ]
机构
[1] Beihang Univ, Sch Mat Sci & Engn, Beijing 100191, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti-10V-2Fe-3Al alloy; Anodic oxidation; SiC nanoparticle concentration; Wear resistance; Corrosion resistance; PLASMA ELECTROLYTIC OXIDATION; MICRO-ARC OXIDATION; TRIBOLOGICAL PROPERTIES; CORROSION-RESISTANCE; CERAMIC COATINGS; MAGNESIUM ALLOY; TITANIUM-ALLOYS; TI6AL4V ALLOY; AZ91D; ELECTRODEPOSITION;
D O I
10.1016/j.vacuum.2015.10.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ordinary and composite oxide films were formed on Ti-10V-2Fe-3Al alloy by anodic oxidation process, in the environmentally friendly electrolytes with different concentrations of SiC nanoparticle. The surface morphology and phase compositions of the oxide film were analyzed by field emission scanning electron microscopy and Raman spectrum techniques, respectively. The results showed that the oxide film was covered with rod like and rimose protuberances, being mainly composed of anatase, rutile, vanadium pentoxide, aluminum oxide and ferric oxide. The thickness was determined by SEM, increasing with a corresponding increase of SiC nanoparticle concentration. The wear resistance and corrosion resistance of the oxide films were evaluated by the ball on disc rotating wear tester and potentiodynamic polarization tests at room temperature, respectively. It was found that composite films possessed enhanced wear resistance and corrosion resistance comparing with the ordinary film. However, the wear resistance of oxide film was not better with higher concentration of SiC nanoparticle. The optimal concentrations of nanoparticle aiming at excellent wear resistance and corrosion resistance were 5 and 10 g/L, respectively. The friction coefficient and wear weight loss were 0.18 and 4.2 mg; the corrosion potential and corrosion current density were 0.665 V and 3.65 x 10(-10) A/cm(2). (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1 / 7
页数:7
相关论文
共 31 条
[1]   Abrasive wear behaviour of Si3N4/TiO2 nanocomposite coatings fabricated by plasma electrolytic oxidation [J].
Aliofkhazraei, M. ;
Rouhaghdam, A. Sabour ;
Shahrabi, T. .
SURFACE & COATINGS TECHNOLOGY, 2010, 205 :S41-S46
[2]   AC plasma electrolytic oxidation of magnesium with zirconia nanoparticles [J].
Arrabal, R. ;
Matykina, E. ;
Viejo, F. ;
Skeldon, P. ;
Thompson, G. E. ;
Merino, M. C. .
APPLIED SURFACE SCIENCE, 2008, 254 (21) :6937-6942
[3]   Corrosion resistance of the surface layers formed on titanium by plasma electrolytic oxidation and hydrothermal treatment [J].
Baszkiewicz, J ;
Krupa, D ;
Mizera, J ;
Sobczak, JW ;
Bilinski, A .
VACUUM, 2005, 78 (2-4) :143-147
[4]   Tribological characterization of microarc oxidized alumina coatings for biological applications [J].
Baxi, Juhi ;
Kar, Presenjit ;
Liang, Hong ;
Polat, Aytekin ;
Usta, Metin ;
Ucisik, Ahmet Hikmet .
VACUUM, 2008, 83 (01) :217-222
[5]   Composite electrodeposition to obtain nanostructured coatings [J].
Benea, L ;
Bonora, PL ;
Borello, A ;
Martelli, S ;
Wenger, F ;
Ponthiaux, P ;
Galland, J .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (07) :C461-C465
[6]   TRIBOLOGICAL PROPERTIES OF TITANIUM-ALLOYS [J].
BUDINSKI, KG .
WEAR, 1991, 151 (02) :203-217
[7]   In situ IR, Raman, and UV-Vis DRS spectroscopy of supported vanadium oxide catalysts during methanol oxidation [J].
Burcham, LJ ;
Deo, G ;
Gao, XT ;
Wachs, IE .
TOPICS IN CATALYSIS, 2000, 11 (1-4) :85-100
[8]  
Chen Sui-yuan, 2011, Journal of Northeastern University (Natural Science), V32, P952
[9]   Effects of hyperthermia induced crystalline aggregation on properties of TiO2 thin films [J].
Dong, G. Z. ;
Fan, H. Q. ;
Zhu, Y. N. ;
Pan, X. B. ;
Jiang, X. B. .
SURFACE ENGINEERING, 2014, 30 (08) :600-605
[10]   A comparison of corrosion, tribocorrosion and electrochemical impedance properties of pure Ti and Ti6Al4V alloy treated by micro-arc oxidation process [J].
Fazel, M. ;
Salimijazi, H. R. ;
Golozar, M. A. ;
jazi, M. R. Garsivaz .
APPLIED SURFACE SCIENCE, 2015, 324 :751-756