Thermal behavior of a phenolic resin for brake pad manufacturing

被引:35
作者
Menapace, C. [1 ]
Leonardi, M. [1 ]
Secchi, M. [2 ]
Bonfanti, A. [3 ]
Gialanella, S. [1 ]
Straffelini, G. [1 ]
机构
[1] Univ Trento, Dept Ind Engn, Via Sommar 9, I-38123 Trento, Italy
[2] Univ Trento, Dept Phys, Via Sommar 14, I-38123 Trento, Italy
[3] Brembo SpA, Via Europa 2, I-24040 Stezzano, BG, Italy
关键词
Brake pad; Phenolic resin; Thermogravimetric analysis; Thermal degradation; Polycondensation; PIN-ON-DISC; WEAR CHARACTERISTICS; FRICTION MATERIALS; DEGRADATION; STABILITY; MECHANISM; KINETICS;
D O I
10.1007/s10973-019-08004-2
中图分类号
O414.1 [热力学];
学科分类号
摘要
The high-temperature behavior of a fast curing commercial phenolic resin, used as a binder in commercial car brake pads, has been investigated. The research comes from the fact that a temperature in excess of 300 degrees C can be reached on the surface pad in case of severe braking conditions. At this temperature, the decomposition of the resin may not only result in detrimental effects for the braking capability of the pads, but also result in a significant increase in their wear rate. The phenolic resin alone and in association with other pad ingredients (master batch), and the friction material, obtained after curing treatments, were analyzed. The main degradation steps of the phenolic resin were identified, as concerns the relevant chemical decomposition processes. The degradation of the methylene and phenol groups turned out to be the most important in terms of mass loss. In the master batch and in the consolidated friction material, the onset temperature of these processes is influenced by the presence of the other ingredients, with particular regard to some metal components. A reduction of the resin degradation onset temperature of 51 degrees C was observed between the pure resin and the friction material.
引用
收藏
页码:759 / 766
页数:8
相关论文
共 35 条
[1]  
Anderson A.E., 1992, ASM HDB, V18, P569
[2]  
[Anonymous], 1975, Introduction to Infrared and Raman Spectroscopy
[3]   Impact of different nanoparticles on the thermal degradation kinetics of phenolic resin nanocomposites [J].
Asaro, L. ;
D'Amico, D. A. ;
Alvarez, V. A. ;
Rodriguez, E. S. ;
Manfredi, L. B. .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2017, 128 (03) :1463-1478
[4]   Composites as friction materials: Recent developments in non-asbestos fiber reinforced friction materials - A review [J].
Bijwe, J .
POLYMER COMPOSITES, 1997, 18 (03) :378-396
[5]   General equation for the determination of the crystallite size La of nanographite by Raman spectroscopy [J].
Cançado, LG ;
Takai, K ;
Enoki, T ;
Endo, M ;
Kim, YA ;
Mizusaki, H ;
Jorio, A ;
Coelho, LN ;
Magalhaes-Paniago, R ;
Pimenta, MA .
APPLIED PHYSICS LETTERS, 2006, 88 (16)
[6]   Effect of polymerization on the boson peak, from liquid to glass [J].
Caponi, S. ;
Corezzi, S. ;
Fioretto, D. ;
Fontana, A. ;
Monaco, G. ;
Rossi, F. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2011, 357 (02) :530-533
[7]   A novel thermal degradation mechanism of phenol-formaldehyde type resins [J].
Chen Yangfei ;
Chen Zhiqin ;
Xiao Shaoyi ;
Liu Hongbo .
THERMOCHIMICA ACTA, 2008, 476 (1-2) :39-43
[8]  
Chen YZ, 2014, BIORESOURCES, V9, P4063
[9]   Study on thermal degradation of phenolic resin [J].
Chen, Zhiqin ;
Chen, Yangfei ;
Liu, Hongbo .
INFORMATION ENGINEERING FOR MECHANICS AND MATERIALS RESEARCH, 2013, 422 :24-+
[10]   Structure-charring relationship in phenol-formaldehyde type resins [J].
Costa, L ;
diMontelera, LR ;
Camino, G ;
Weil, ED ;
Pearce, EM .
POLYMER DEGRADATION AND STABILITY, 1997, 56 (01) :23-35