Microstructural characteristics and thermophysical properties of spark plasma sintered Inconel 738LC

被引:19
|
作者
Ogunbiyi, O. F. [1 ]
Jamiru, T. [1 ]
Sadiku, E. R. [2 ,3 ]
Beneke, L. W. [1 ]
Adesina, O. T. [1 ]
Adegbola, T. A. [1 ]
机构
[1] Tshwane Univ Technol, Dept Mech Engn Mechatron & Ind Design, Pretoria, South Africa
[2] Tshwane Univ Technol, Inst NanoEngn Res INER, Pretoria, South Africa
[3] Tshwane Univ Technol, Dept Chem Met & Mat Engn, Pretoria, South Africa
来源
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY | 2019年 / 104卷 / 1-4期
关键词
IN738LC; Spark plasma sintering; Microstructure; Laser flash; Thermal diffusivity; Thermal conductivity; MECHANICAL-PROPERTIES; THERMAL-CONDUCTIVITY; POLYCRYSTALLINE SUPERALLOY; TEMPERATURE; ALLOY; PARAMETERS; METALS; SPS; TI;
D O I
10.1007/s00170-019-03983-w
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
Nickel-based superalloys are used for turbine component parts in the power industry, aircraft engines, and in the marine sector. One such alloy that is available for these purposes is Inconel 738LC (IN738LC) nickel-based superalloy. Therefore, it is pertinent to have good structural and thermal stabilities for high-temperature applications, since these characteristics are important for its performance. In this study, spark plasma sintering technology was used to fabricate IN738LC nickel-based superalloy by using sintering temperature in the range of between 900 and 1200 degrees C. The fabricated products were characterized by using the scanning electron microscope and X-ray diffraction. There was the formation of the gamma '(Ni-3(Ti, Al)) intermetallic phase in the microstructure, which contributed to the material (Inconel 738LC) property. The solid solution elements present are chromium, cobalt, tungsten, and tantalum; these equally contribute to the structural stability of IN738LC. The density, hardness, and the predicted yield strength increased with increasing sintering temperature, while the porosity decreased with increasing sintering temperature. The thermal conductivity, which is an important thermophysical property of IN738LC, enables the evaluation of the usefulness and service life of IN738LC superalloy at high-temperature applications, was also examined. The thermal conductivity was measured by using a laser flash method in the temperature range of 100-600 degrees C. For the sintered alloy, the thermal conductivity was determined as a function of the thermal diffusivity, specific heat capacity, and density. Analysis showed inflection pattern with increase in temperature on the sample fabricated at 900, 1000, and 1100 degrees C, ; a monotonic increase with increase in temperature was observed on the sample fabricated at 1200 degrees C, ; the inflections are associated with the gamma ' precipitates dissolution and redistribution.
引用
收藏
页码:1425 / 1436
页数:12
相关论文
共 50 条
  • [21] Microstructural Investigation and Determining the Optimal Conditions for Nondestructive Testing of Inconel 738LC Superalloy Gas Turbine Blade
    Rayatpour, Masumeh
    Lalegani, Zahra
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2021, 21 (04) : 1203 - 1211
  • [22] Microstructural Investigation and Determining the Optimal Conditions for Nondestructive Testing of Inconel 738LC Superalloy Gas Turbine Blade
    Masumeh Rayatpour
    Zahra Lalegani
    Journal of Failure Analysis and Prevention, 2021, 21 : 1203 - 1211
  • [23] Wide Gap Brazing of Inconel 738LC Nickel-Based Superalloy: Metallurgical and Mechanical Characteristics
    Alinaghian, H.
    Farzadi, A.
    Marashi, P.
    Pouranvari, M.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2020, 51 (12): : 6283 - 6293
  • [24] Failure analysis of a gas turbine blade made of Inconel 738LC alloy
    Mazur, Z
    Luna-Ramírez, A
    Juárez-Islas, JA
    Campos-Amezcua, A
    ENGINEERING FAILURE ANALYSIS, 2005, 12 (03) : 474 - 486
  • [25] DAMAGE MECHANISMS OF INCONEL 738LC UNDERCREEP-FATIGUE LOADING CONDITIONS
    M.Yamamoto
    T.Ogata
    ActaMetallurgicaSinica(EnglishLetters), 1998, (06) : 470 - 476
  • [26] Microstructural evolution during transient liquid phase bonding of Inconel 738LC using AMS 4777 filler alloy
    Jalilvand, V.
    Omidvar, H.
    Shakeri, H. R.
    Rahimipour, M. R.
    MATERIALS CHARACTERIZATION, 2013, 75 : 20 - 28
  • [27] Liquation of various phases in HAZ during welding of cast Inconel 738LC
    Ojo, OA
    Richards, NL
    Chaturvedi, MC
    MATERIALS SCIENCE AND TECHNOLOGY, 2004, 20 (08) : 1027 - 1034
  • [28] Low cycle fatigue of cast superalloy Inconel 738LC at high temperature
    Obrtlik, Karel
    Chlupova, Alice
    Petrenec, Martin
    Pokak, Jaroslav
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS VII, 2008, 385-387 : 581 - 584
  • [29] Wide Gap Brazing of Inconel 738LC Nickel-Based Superalloy: Metallurgical and Mechanical Characteristics
    H. Alinaghian
    A. Farzadi
    P. Marashi
    M. Pouranvari
    Metallurgical and Materials Transactions A, 2020, 51 : 6283 - 6293
  • [30] A Study on the Effect of Process Parameters on the Properties of Joint in TLP-Bonded Inconel 738LC Superalloy
    V. Jalilvand
    H. Omidvar
    H. R. Shakeri
    M. R. Rahimipour
    Metallurgical and Materials Transactions B, 2013, 44 : 1222 - 1231