Accelerated weathering simulation on rheological properties and chemical structure of high viscosity modified asphalt: A temperature acceleration effect analysis

被引:32
作者
Hu, Mingjun [1 ]
Sun, Guoqiang [2 ]
Sun, Daquan [1 ]
Lu, Tong [1 ]
Ma, Jianmin [1 ]
Deng, Yue [1 ]
机构
[1] Tongji Univ, Key Lab Rd & Traff Engn, Minist Educ, Shanghai 201804, Peoples R China
[2] Beijing Univ Technol, Dept Rd & Railway Engn, Beijing 100124, Peoples R China
基金
中国国家自然科学基金;
关键词
Weathering aging; Temperature acceleration effect; High viscosity modified asphalt; Aging kinetics; Rheological property; Chemical composition; AGING PROPERTIES; BINDERS; MECHANISM; KINETICS; SURFACE;
D O I
10.1016/j.conbuildmat.2020.121120
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
High viscosity modified asphalt (HVMA) is widely used as the binder for permeable asphalt pavement. The service life of permeable asphalt pavement strongly depends on the weathering aging resistance of HVMA due to the large porosity of permeable asphalt pavement. In order to investigate the accelerated deterioration effect of temperature on the weathering aging process, a laboratory accelerated weathering aging tester was used to simulate the long-term weathering aging of HVMA at different aging temperatures (30 degrees C, 50 degrees C, and 70 degrees C) and different weathering aging days (0 similar to 12d). A series of rheological tests were conducted to study the influence of weathering aging temperature on the rheological properties of HVMA. Then, FTIR test was applied to characterize the changes in chemical composition of HVMA at different weathering aging temperatures. Furthermore, an aging kinetics model was put forward to further understand the effect of aging temperature on the weathering aging rate of HVMA. The results indicate that the weathering aging rate of HVMA is fast in the early aging stage (0 similar to 2d) and slows down in the later aging stage (2 similar to 12d). The increase of aging temperature has a significant accelerated deterioration effect on the chemo-rheological properties of HVMA during weathering aging process. At 30 degrees C aging temperature, the deteriorated rheological properties of HVMA are mainly due to the aging of solar radiation. As the aging temperature increases to 50 degrees C, the thermal aging effect of HVMA begins to appear under the stimulation of solar radiation. When the aging temperature rises to 70 degrees C, HVMA has suffered from a severe coupled aging of high temperature, solar radiation and humidity. This coupled aging effect leads to a significant asphalt oxidation and polymer degradation, which is the main reason for the severely deteriorated rheological properties of HVMA. The proposed aging kinetics model results also confirm the accelerated deterioration effect of temperature during weathering aging process. (C) 2020 Elsevier Ltd. All rights reserved.
引用
收藏
页数:15
相关论文
共 35 条
  • [31] Effect of warm mixture asphalt (WMA) additives on high failure temperature properties for crumb rubber modified (CRM) binders
    Wang, Hainian
    Dang, Zhengxia
    You, Zhanping
    Cao, Dongwei
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2012, 35 : 281 - 288
  • [32] Low-density polyethylene/ethylene-vinyl acetate compound modified asphalt: Optimal preparation process and high-temperature rheological properties
    Hong, Zhe
    Yan, Kezhen
    Wang, Min
    You, Lingyun
    Ge, Dongdong
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2022, 314
  • [33] Aging behavior of polyphosphoric acid/styrene-butadiene-styrene-modified bio-mixed asphalt based on high-temperature rheological properties and microscopic mechanism
    Yang, Xiaolong
    Liu, Guiyong
    Zhang, Haihong
    Meng, Yongjun
    Peng, Chunhong
    He, Xinyi
    Liang, Junling
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2023, 389
  • [34] Clarifying the effect of chemical structure on high-temperature resistance of polyimides based on DFT and ReaxFF based molecular dynamic simulation
    Pu, Chuanzhi
    Lin, Daolei
    Xu, Hongjie
    Liu, Fangzhou
    Gao, Hong
    Tian, Guofeng
    Qi, Shengli
    Wu, Dezhen
    [J]. POLYMER, 2022, 255
  • [35] Effect of Ultra-High Temperature Degradation on the Physical Properties and Chemical Structure of an AMPS-Based Copolymer Oil-Well Cement Additive PADIM in Aqueous Solution
    Yu, Yongjin
    Zhang, Hang
    Xu, Pu
    Zhang, Xinyang
    Wang, Haige
    Hu, Miaomiao
    Guo, Jintang
    [J]. POLYMERS, 2025, 17 (05)