Annealing behaviors of vacancy in varied neutron irradiated Czochralski silicon

被引:4
作者
Chen Gui-feng
Li Yang-xian [1 ]
Liu Li-li
Niu Ping-juan
Niu Sheng-li
Chen Dong-feng
机构
[1] Hebei Univ Technol, Sch Mat Sci & Engn, Tianjin 300130, Peoples R China
[2] Tianjin Polytech Univ, Sch Informat & Commun, Tianjin 300160, Peoples R China
[3] China Inst Atom Energy, Beijing 102413, Peoples R China
来源
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA | 2006年 / 16卷
基金
中国国家自然科学基金; 高等学校博士学科点专项科研基金;
关键词
Czochralski silicon; neutron irradiation; A-center; FTIR;
D O I
10.1016/S1003-6326(06)60155-6
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The difference of annealing behaviors of vacancy-oxygen complex (VO) in varied dose neutron irradiated Czochralski silicon: (S1 5 x 10(17) n/cm(3) and S2 1.07 x 10(19) n/cm(3)) were studied. The results show that the VO is one of the main defects formed in neutron irradiated Czochralski silicon (CZ-Si). In this defect, oxygen atom shares a vacancy, it is bonded to two silicon neighbors. Annealed at 200 degrees C, divacancies are trapped by interstitial oxygen(O-i) to form V2O (840 cm 1). With the decrease of the 829 cm(-1) (VO) three infrared absorption bands at 825 cm(-1) (V2O2), 834 cm(-1) (V2O3) and 840 cm(-1) (V2O) will rise after annealed at temperature range of 200-500 degrees C. After annealed at 450-500 degrees C the main absorption bands in SI sample are 834 cm(-1), 825 cm(-1) and 889 cm(-1) (VO2), in S2 is 825 cm(-1). Annealing of A-center in varied neutron irradiated CZ-Si is suggested to consist of two processes. The first is due to trapping of VO by Oi in low dose neutron irradiated CZ-Si (S1) and the second is due to capture the wandering vacancy by VO, etc, in high dose neutron irradiated CZ-Si (S2), the VO2 plays an important role in the annealing of A-center. With the increase of the irradiation dose, the annealing behavior of A-center is changed.
引用
收藏
页码:S113 / S115
页数:3
相关论文
共 9 条
[1]  
DONNELLY SE, 2001, NUCL INSTRUM METH B, V106, P233
[2]   Defect generation in crystalline silicon irradiated with high energy particles [J].
Kuhnke, M ;
Fretwurst, E ;
Lindstrom, G .
NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2002, 186 :144-151
[3]   The effects of neutron irradiation on the oxygen precipitation in Czochralski-silicon [J].
Li, YX ;
Guo, HY ;
Liu, BD ;
Liu, TJ ;
Hao, QY ;
Liu, CC ;
Yang, DR ;
Que, DL .
JOURNAL OF CRYSTAL GROWTH, 2003, 253 (1-4) :6-9
[4]   The intrinsic gettering in neutron irradiation czochralski-silicon [J].
Li, YX ;
Liu, HY ;
Niu, PJ ;
Lu, CC ;
Xu, YS ;
Yang, DR ;
Que, DL .
ACTA PHYSICA SINICA, 2002, 51 (10) :2407-2410
[5]   Inhibition of neutron irradiation on oxidation stacking faults on the surface of Si wafers [J].
Li, YX ;
Ju, YL ;
Liu, CC ;
Xu, YS ;
Wang, HM .
JOURNAL OF CRYSTAL GROWTH, 1996, 160 (3-4) :250-252
[6]   The VO2* defect in silicon [J].
Lindström, JL ;
Murin, LI ;
Svensson, BG ;
Markevich, VP ;
Hallberg, T .
PHYSICA B-CONDENSED MATTER, 2003, 340 :509-513
[7]   Annealing mechanisms of divacancies in silicon [J].
Poirier, R ;
Avalos, V ;
Dannefaer, S ;
Schlettekatte, F ;
Roorda, S .
PHYSICA B-CONDENSED MATTER, 2003, 340 :609-612
[8]   Divacancies in proton irradiated silicon: Comparison of annealing mechanisms studied with infrared spectroscopy and positron annihilation [J].
Poirier, R ;
Avalos, V ;
Dannefaer, S ;
Schiettekatte, F ;
Roorda, S .
NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2003, 206 :85-89
[9]  
Yu Xuegong, 2003, Chinese Journal of Semiconductors, V24, P49