摘要
In this paper, the data reduction equations for common delamination toughness tests are re-derived for use with specimens which have bonded doublers. The common toughness tests considered here are the double cantilever beam for mode I toughness; the end notch flexure (3ENF) and 4-point ENF (4ENF) for mode II toughness; and the mixed-mode bending test for testing under combined mode I and mode II loading. Because the addition of the doublers changes the bending stiffness of the specimens, these data reduction equations may need to be corrected. Doublers were added to the delamination test specimens to solve a premature failure problem. Delamination toughness is normally tested using a beam with an imbedded insert so that one end of the specimen is split into two arms. If the specimen is too thin, or if the toughness of the material is too high, an arm of the specimen may fail in bending before the delamination grows. When this occurs, the toughness of the material cannot be determined. To delay the bending failure so that delamination growth occurs, doubler plates were bonded to both top and bottom surfaces of the specimen. A doubler parameter, beta, which describes how much the use of doubler plates changed the ratio of full thickness to delaminated bending stiffnesses, was defined. When changes to the data reduction equations were required, the changes were minor when written in terms of the beta parameter. The doubler plate technique was demonstrated by measuring the mixed-mode fracture toughness of a carbon-carbon composite using test specimens which would otherwise have failed before delamination growth occurred. The doubler plate technique may solve several problems that can be encountered when testing delamination fracture toughness. Published by Elsevier Ltd.
引用
收藏
页码:1337 / 1344
页数:8
相关论文
共 16 条
[1]  
[Anonymous], 820 DREP
[2]  
*ASTM, 2001, ASTM ANN BOOK STAND, P392
[3]  
*ASTM INT, 2001, ANN BOOK ASTM STAND, P289
[4]   MODE-2 STRESS-INTENSITY FACTORS FOR CRACKED WOOD BEAMS [J].
BARRETT, JD ;
FOSCHI, RO .
ENGINEERING FRACTURE MECHANICS, 1977, 9 (02) :371-&
[5]  
CHEN L, 1999, P AM SOC COMP 14 TEC
[6]  
IRWIN GR, 1965, ASTM STP, V381, P84
[7]   Mode II fracture toughness evaluation using four point bend, end notched flexure test [J].
Martin, RH ;
Davidson, BD .
PLASTICS RUBBER AND COMPOSITES, 1999, 28 (08) :401-406
[8]  
OBRIEN TK, 1994, ASTM J COMPOS TECHNO, V15, P269
[9]  
Ratcliffe J, 2001, J REINF PLAST COMP, V20, P945
[10]   MIXED-MODE BENDING METHOD FOR DELAMINATION TESTING [J].
REEDER, JR ;
CREWS, JH .
AIAA JOURNAL, 1990, 28 (07) :1270-1276