共 70 条
Ultrahigh room temperature electrocaloric response in lead-free bulk ceramics via tape casting
被引:26
作者:
Du, Hongliang
[1
]
Chang, Yunfei
[2
]
Li, Chunwang
[1
]
Hu, Qingyuan
[3
,4
]
Pang, Jing
[3
,4
]
Sun, Yuan
[2
]
Weyland, Florian
[5
]
Novak, Nikola
[6
]
Jin, Li
[3
,4
]
机构:
[1] Xian Int Univ, Coll Engn, Xian 710077, Shaanxi, Peoples R China
[2] Harbin Inst Technol, Sch Instrumentat Sci & Engn, Condensed Matter Sci & Technol Inst, Harbin 150080, Heilongjiang, Peoples R China
[3] Xi An Jiao Tong Univ, Minist Educ, Key Lab, Elect Mat Res Lab, Xian 710049, Peoples R China
[4] Xi An Jiao Tong Univ, Sch Elect & Informat Engn, Int Ctr Dielect Res, Xian 710049, Peoples R China
[5] Tech Univ Darmstadt, Inst Mat & Earth Sci, D-64287 Darmstadt, Germany
[6] Jozef Stefan Inst, Jamova Cesta 39, Ljubljana 1000, Slovenia
关键词:
THIN-FILM;
POLYMER NANOCOMPOSITES;
FERROELECTRIC POLYMER;
BREAKDOWN STRENGTH;
ENERGY;
PHASES;
RANGE;
D O I:
10.1039/c9tc01407a
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
Solid-state cooling technology based on the electrocaloric effect is attracting increasing attention as an important alternative to traditional cooling systems in microelectronic and integrated electronics. Leadfree bulk ceramics are considered as one of the promising candidates for middle and large-scale electrocaloric cooling because of their environment-friendliness and large heat absorption capacity. However, the room temperature adiabatic temperature change (Delta T) in lead-free bulk ceramics has long been limited by their relatively low dielectric breakdown strength (Eb o 60 kV cm(-1)), hindering their practical applications. In this work, we propose to use the tape casting technique as a practicable strategy to enhance the densification and decrease the porosity of lead-free bulk ceramics for achieving a high Eb and a large room temperature Delta T. An ultrahigh room temperature Delta T (1.6 K) was realized in a (Ba0.95Ca0.05)(Ti0.94Sn0.06) O-3 (BCTS) bulk ceramic prepared by the tape casting technique, which is 4 times larger than that of the lead-free bulk ceramics with a similar composition prepared by the conventional ceramic preparing approach. More significantly, unlike the other previously reported results, which only show high DT in an extremely narrow temperature range, Delta T of the BCTS bulk ceramic increases from 1.6 K to 2.0 K in the temperature range from 300 K to 345 K, which is comparable with that found in the lead-based bulk counterpart. Most importantly, this work opens up a new avenue to explore lead-free bulk ceramics with a large room temperature Delta T for solid-state refrigeration.
引用
收藏
页码:6860 / 6866
页数:7