Microstructural evolution and mechanical performance of Al-Cu-Li alloy joined by friction stir welding

被引:21
作者
Naumov, Anton [1 ]
Isupov, Fedor [1 ]
Rylkov, Evgenii [1 ]
Polyakov, Pavel [1 ]
Panteleev, Mikhail [2 ]
Skupov, Aleksey [2 ]
Amancio-Filho, Sergio T. [3 ]
Panchenko, Oleg [1 ]
机构
[1] Peter Great St Petersburg Polytech Univ, St Petersburg 195251, Russia
[2] Fed State Unitary Enterprise, All Russian Sci Res Inst Aviat Mat, Moscow 105005, Russia
[3] Graz Univ Technol, A-8010 Graz, Austria
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2020年 / 9卷 / 06期
关键词
Friction stir welding (FSW); Al-Cu-Li alloy; Microstructural characteristics; Mechanical properties; Fracture behavior; Numerical simulation; Fractography; X-ray microtomography; TEM observations; HEAT-TREATMENT; WELDED-JOINTS; TEMPER CONDITION; SI ALLOYS; AA7075; MG;
D O I
10.1016/j.jmrt.2020.10.008
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The objective of this study was to develop the technology of butt friction stir welding (FSW) for Al-Cu-Li alloy sheets of 1.4 mm thick after hot rolling and subsequent quenching. This initial state of the alloy was chosen in order to provide heat treatment of the received joints after FSW. The TEM observation was performed for the base material and different zones of the joints in order to determine the precipitates and dislocations density and distributions. The grain size in the stir zone (SZ) was increased; the width of the softened region was narrowed down with the decreasing of linear energy. The differences in mechanical properties of the FSWed joints were explained by analysis of microstructural changes and tensile fracture surfaces, supported by the results of the numerical simulation of the temperature distribution and material flow. The fracture of the high linear energy FSW joints occurred in the SZ along the remnant oxide line (ROL), while the low linear energy FSW joint raptured in the transition between HAZ and TMAZ on the AS, where lower hardness value was detected. (C) 2020 The Author(s). Published by Elsevier B.V. This is an open access article under the CC-BY-NC-ND license.
引用
收藏
页码:14454 / 14466
页数:13
相关论文
共 42 条
[31]  
Olea CW, 2008, AA2024T351, P156
[32]   Microstructural and mechanical characterization of laser beam welded AA6056 Al-alloy [J].
Pakdil, M. ;
Cam, G. ;
Kocak, M. ;
Erim, S. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (24) :7350-7356
[33]  
Rajendran C., 2016, Journal of the Mechanical Behaviour of Materials, V25, P89, DOI 10.1515/jmbm-2016-0011
[34]   Comparative Analysis of the Mechanical Properties of the Friction Stir Welding Joints of Various Aluminum Alloys [J].
Ryl'kov, E. N. ;
Isupov, F. Yu ;
Naumov, A. A. ;
Panchenko, O., V ;
Zhabrev, L. A. .
RUSSIAN METALLURGY, 2019, 2019 (13) :1531-1536
[35]   Wear Mechanism for H13 Steel Tool During Friction StirWelding of CuCrZr Alloy [J].
Sahlot, Pankaj ;
Mishra, R. S. ;
Arora, Amit .
FRICTION STIR WELDING AND PROCESSING X, 2019, :59-64
[36]   Characteristics of the kissing-bond in friction stir welded Al alloy 1050 [J].
Sato, YS ;
Takauchi, H ;
Park, SHC ;
Kokawa, H .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 405 (1-2) :333-338
[37]  
Shiganov I. N., 2017, Welding International, V31, P481, DOI 10.1080/09507116.2016.1268768
[38]  
Thomas WM, 1991, G.B. Patent application, Patent No. [91259788, 9125978.8]
[39]   Effect of Pre and Post Weld Treatment on the Mechanical Properties of Friction Stir Welded AA6061-T6 Joint [J].
Verduzco Juarez, Julio C. ;
Garcia Hernandez, Rafael ;
Dominguez Almaraz, Gonzalo M. ;
Correa Gomez, Erasmo ;
Villalon Lopez, Juan J. .
INTERNATIONAL JOURNAL OF AUTOMOTIVE AND MECHANICAL ENGINEERING, 2020, 17 (02) :7882-7889
[40]   Precipitates and intermetallic phases in precipitation hardening Al-Cu-Mg-(Li) based alloys [J].
Wang, SC ;
Starink, MJ .
INTERNATIONAL MATERIALS REVIEWS, 2005, 50 (04) :193-215