Fracture analysis of monolithic CAD-CAM crowns

被引:24
|
作者
Kashkari, Afnan [1 ]
Yilmaz, Burak [2 ]
Brantley, William A. [2 ]
Schricker, Scott R. [2 ]
Johnston, William M. [2 ]
机构
[1] Johns Hopkins Aramco Healthcare, Restorat & Esthet Dent, Dhahran, Saudi Arabia
[2] Ohio State Univ, Coll Dent, Div Restorat & Prosthet Dent, Columbus, OH 43210 USA
关键词
CAD-CAM; ceramic; fracture; lithium disilicate; lithium silicate; zirconia; ALL-CERAMIC CROWNS; LITHIUM-DISILICATE; MECHANICAL-PROPERTIES; CURING MODE; BITE FORCE; FATIGUE; CONVERSION; POLYMERIZATION; SHRINKAGE; STRENGTH;
D O I
10.1111/jerd.12462
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose The aim of this study was to compare the integrity of zirconia, lithium disilicate, and zirconia-reinforced lithium silicate CAD-CAM crowns after being subjected to cyclic loading and then subjected to static loading until fracture. Material and Methods Zirconia (Zirkonzahn), lithium disilicate (LDS, Ivoclar Vivadent AG), and zirconia-reinforced lithium silicate glass ceramic (ZLS) (Vita Suprinity, Vita Zahnfabrik) monolithic crowns were milled (n = 6). The crowns were bonded using composite resin cements and subjected to cyclic loading under wet conditions. Three specimens from each group were loaded for 10 000 cycles, and the other three specimens were loaded for 50 000 cycles with 250 N. Specimens were subjected to loading until fracture. Load-to-fracture values were analyzed with 2-way (ANOVA) and Tukey-Kramer post hoc test (alpha = 0.05). Specimens from each group were examined using an SEM. Results Mean load-to-fracture values among materials were significantly different from each other (P < 0.05). No significant effect of the number of cycles was found on the load-to-fracture values of crowns (P > 0.05). Conclusion Load-to-fracture values of zirconia were higher than those of LDS, which were higher than those of ZLS. The number of fatigue loading cycles did not affect the load-to-fracture of the tested crowns for a given material. Clinical Significance More research needs to be conducted before considering the routine use of ZLS for molars in patients with high risk of parafunctional habits.
引用
收藏
页码:346 / 352
页数:7
相关论文
共 50 条
  • [21] Fracture Resistance of CAD/CAM Monolithic Zirconia Crowns Supported by Titanium and Ti-Base Abutments: The Effect of Chewing Simulation and Thermocyclic Aging
    Yavuz, Ayse
    Buyukerkmen, Emine Beguem
    INTERNATIONAL JOURNAL OF ORAL & MAXILLOFACIAL IMPLANTS, 2023, 38 (02) : 328 - 333
  • [22] Numerical fatigue analysis of premolars restored by CAD/CAM ceramic crowns
    Homaei, Ehsan
    Jin, Xiao-Zhuang
    Pow, Edmond Ho Nang
    Matinlinna, Jukka Pekka
    Tsoi, James Kit-Hon
    Farhangdoost, Khalil
    DENTAL MATERIALS, 2018, 34 (07) : E149 - E157
  • [23] Wear resistance and abrasiveness of CAD-CAM monolithic materials
    Ludovichetti, Francesco Saverio
    Trindade, Flavia Zardo
    Werner, Arie
    Kleverlaan, Cornelis Johannes
    Fonseca, Renata Garcia
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 120 (02)
  • [24] Effect of grinding and polishing on the roughness and fracture resistance of cemented CAD-CAM monolithic materials submitted to mechanical aging
    Ludovichetti, Francesco Saverio
    Trindade, Flavia Zardo
    Adabo, Gelson Luis
    Pezzato, Luca
    Fonseca, Renata Garcia
    JOURNAL OF PROSTHETIC DENTISTRY, 2019, 121 (05) : 866.e1 - 866.e8
  • [25] Comparative Analysis of CAD-CAM Workflow Variations on the Marginal and Internal Gaps and Fatigue Behavior of Ceramic and Resin Composite Dental Crowns
    Pilecco, Rafaela Oliveira
    da Rosa, Lucas Saldanha
    Baldi, Andrea
    Machry, Renan Vaz
    Tribst, Joao Paulo Mendes
    Valandro, Luiz Felipe
    Kleverlaan, Cornelis Johannes
    Scotti, Nicola
    Pereira, Gabriel Kalil Rocha
    EUROPEAN JOURNAL OF DENTISTRY, 2025,
  • [26] Marginal and Internal Fit of Monolithic Zirconia Crowns Fabricated by Using Two Different CAD-CAM Workflows: An In Vitro Study
    Cin, Vahap
    Izgi, Ayca Deniz
    Kale, Ediz
    Yilmaz, Burak
    PROSTHESIS, 2023, 5 (01): : 35 - 47
  • [27] Effect of endodontic access simulation on the fracture strength of lithium-disilicate and resin-matrix ceramic CAD-CAM crowns
    Oguz, Ece Irem
    Kilicarslan, Mehmet Ali
    Ozcan, Mutlu
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2020, 32 (05) : 472 - 479
  • [28] Influence of preparation, fitting, and cementation on the vitro performance and fracture resistance of CAD/CAM crowns
    Rosentritt, Martin
    Preis, Verena
    Behr, Michael
    Hahnel, Sebastian
    JOURNAL OF DENTISTRY, 2017, 65 : 70 - 75
  • [29] Marginal discrepancy and fracture load of thermomechanically fatigued crowns fabricated with different CAD-CAM techniques
    Sasany, Rafat
    Yilmaz, Burak
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2023, 32 (07): : 602 - 607
  • [30] Fatigue resistance of CAD/CAM resin composite molar crowns
    Shembish, Fatma A.
    Tong, Hui
    Kaizer, Marina
    Janal, Malvin N.
    Thompson, Van P.
    Opdam, Niek J.
    Zhang, Yu
    DENTAL MATERIALS, 2016, 32 (04) : 499 - 509