Fracture analysis of monolithic CAD-CAM crowns

被引:24
|
作者
Kashkari, Afnan [1 ]
Yilmaz, Burak [2 ]
Brantley, William A. [2 ]
Schricker, Scott R. [2 ]
Johnston, William M. [2 ]
机构
[1] Johns Hopkins Aramco Healthcare, Restorat & Esthet Dent, Dhahran, Saudi Arabia
[2] Ohio State Univ, Coll Dent, Div Restorat & Prosthet Dent, Columbus, OH 43210 USA
关键词
CAD-CAM; ceramic; fracture; lithium disilicate; lithium silicate; zirconia; ALL-CERAMIC CROWNS; LITHIUM-DISILICATE; MECHANICAL-PROPERTIES; CURING MODE; BITE FORCE; FATIGUE; CONVERSION; POLYMERIZATION; SHRINKAGE; STRENGTH;
D O I
10.1111/jerd.12462
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose The aim of this study was to compare the integrity of zirconia, lithium disilicate, and zirconia-reinforced lithium silicate CAD-CAM crowns after being subjected to cyclic loading and then subjected to static loading until fracture. Material and Methods Zirconia (Zirkonzahn), lithium disilicate (LDS, Ivoclar Vivadent AG), and zirconia-reinforced lithium silicate glass ceramic (ZLS) (Vita Suprinity, Vita Zahnfabrik) monolithic crowns were milled (n = 6). The crowns were bonded using composite resin cements and subjected to cyclic loading under wet conditions. Three specimens from each group were loaded for 10 000 cycles, and the other three specimens were loaded for 50 000 cycles with 250 N. Specimens were subjected to loading until fracture. Load-to-fracture values were analyzed with 2-way (ANOVA) and Tukey-Kramer post hoc test (alpha = 0.05). Specimens from each group were examined using an SEM. Results Mean load-to-fracture values among materials were significantly different from each other (P < 0.05). No significant effect of the number of cycles was found on the load-to-fracture values of crowns (P > 0.05). Conclusion Load-to-fracture values of zirconia were higher than those of LDS, which were higher than those of ZLS. The number of fatigue loading cycles did not affect the load-to-fracture of the tested crowns for a given material. Clinical Significance More research needs to be conducted before considering the routine use of ZLS for molars in patients with high risk of parafunctional habits.
引用
收藏
页码:346 / 352
页数:7
相关论文
共 50 条
  • [1] In vitro analysis of the fracture resistance of CAD-CAM monolithic zirconia molar crowns with different occlusal thickness
    Sorrentino, Roberto
    Triulzio, Clementina
    Tricarico, Maria Gabriella
    Bonadeo, Giovanni
    Gherlone, Enrico Felice
    Ferrari, Marco
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 61 : 328 - 333
  • [2] Fracture Load of Monolithic CAD/CAM Ceramic Crowns Placed on Different Implant Abutments
    Meneghetti, Priscila Ceolin
    Pittas do Canto, Paulo Eduardo
    Spohr, Ana Maria
    Burnett Junior, Luiz Henrique
    INTERNATIONAL JOURNAL OF ORAL & MAXILLOFACIAL IMPLANTS, 2022, 37 (06) : 1217 - 1222
  • [3] Fatigue performance of adhesively luted glass or polycrystalline CAD-CAM monolithic crowns
    Alves, Daniela Meira
    Cadore-Rodrigues, Ana Carolina
    Prochnow, Catina
    de Lima Burgo, Thiago Augusto
    Spazzin, Aloisio Oro
    Bacchi, Atais
    Valandro, Luiz Felipe
    Rocha Pereira, Gabriel Kalil
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 126 (01) : 119 - 127
  • [4] Fracture Load of Monolithic CAD/CAM Lithium Disilicate Ceramic Crowns and Veneered Zirconia Crowns as a Posterior Implant Restoration
    Kim, Jee Hwan
    Lee, Su-Jeong
    Park, Jun Sub
    Ryu, Jae Jun
    IMPLANT DENTISTRY, 2013, 22 (01) : 66 - 70
  • [5] In vitro analysis of the fracture resistance of CAD-CAM monolithic lithium disilicate molar crowns with different occlusal thickness
    Sorrentino, R.
    Nagasawa, Y.
    Infelis, M.
    Bonadeo, G.
    Ferrari, M.
    JOURNAL OF OSSEOINTEGRATION, 2018, 10 (02) : 50 - 56
  • [6] Fatigue resistance of anterior monolithic crowns produced from CAD-CAM materials: An in vitro study
    Choo, Seung-Sik
    Ko, Kyung-Ho
    Huh, Yoon-Hyuk
    Park, Chan-Jin
    Cho, Lee-Ra
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 130 (04) : 620 - 628
  • [7] Clinical performance of chairside monolithic lithium disilicate glass-ceramic CAD-CAM crowns
    Aziz, Ahmed
    El-Mowafy, Omar
    Tenenbaum, Howard C.
    Lawrence, Herenia P.
    Shokati, Babak
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2019, 31 (06) : 613 - 619
  • [8] Effect of erosive media on microhardness and fracture toughness of CAD-CAM dental materials
    Elraggal, Alaaeldin
    Afifi, Rania
    Abdelraheem, Islam
    BMC ORAL HEALTH, 2022, 22 (01)
  • [9] Effect of the CAD/CAM Milling Protocol on the Fracture Behavior of Zirconia Monolithic Crowns
    Oliveira, Andressa Restani
    Ziglioli, Natalia Ulmi
    Marocho, Susana M. Salazar
    Satterthwaite, Julian
    Borba, Marcia
    MATERIALS, 2024, 17 (12)
  • [10] Should the load-to-fracture test for CAD/CAM monolithic molar crowns be standardized and how? A systematic review and finite element analysis
    Miranda, Nicole Cindy Fontinele
    Gialain, Ivan Onone
    Gantier-Takano, Marlene Kasumi
    Ballester, Rafael Yague
    Hernandez, Bruno Agostinho
    Fok, Alex
    Meira, Josete Barbosa Cruz
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2025, 168