Effect of testing atmosphere (air/in vacuo) on low cycle fatigue characteristics of a duplex stainless steel

被引:0
|
作者
Llanes, L [1 ]
Mateo, A
Villechaise, P
Méndez, J
Anglada, M
机构
[1] Univ Politecn Catalunya, ETSEIB, Dept Ciencia Mat & Engn Met, E-08028 Barcelona, Spain
[2] ENSMA, Mecan & Phys Mat Lab, CNRS, URA 863, F-86960 Futuroscope, France
关键词
low cycle fatigue; environment; duplex stainless steels; strain localization;
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The effect of testing atmosphere on low cycle fatigue characteristics of a duplex stainless steel has been studied at room temperature. Fatigue tests have been conducted under fully reversed plastic strain control and constant plastic strain rate in two different environments: air and in vacuo. The material has been investigated under two distinct conditions: as annealed or unaged and as thermally aged, corresponding to different dominant cyclic deformation mechanisms at the plastic strain amplitudes chosen for the study. In vacuo testing resulted in longer fatigue lives, and consequently, higher cumulative plastic strain than in air experiences for both material conditions. Although prominent fatigue micromechanisms for a given plastic strain amplitude did not seem to be affected by testing atmosphere, for both unaged and aged conditions, strain localization and cracking phenomena were enhanced in air as compared to vacuum. The experimental results were finally discussed in terms of fatigue micromechanisms-environment interactions. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:S119 / S125
页数:7
相关论文
共 50 条
  • [1] Low cycle fatigue analysis of heat treated duplex stainless steel
    Raj, Ashok J.
    Arulmani, L.
    Raguraman, D.
    Murthy, Shridhar H. N.
    Kumar, Santhosh B. H.
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2022, 8 (02) : 2385 - 2395
  • [2] Growth of short cracks during low and high cycle fatigue in a duplex stainless steel
    Alvarez-Armas, I.
    Krupp, U.
    Balbi, M.
    Herenu, S.
    Marinelli, M. C.
    Knobbe, H.
    INTERNATIONAL JOURNAL OF FATIGUE, 2012, 41 : 95 - 100
  • [3] Low-cycle fatigue behaviour of ribbed 1.4362 duplex stainless steel reinforcement
    Fu, Jian-Yu
    Ge, Xiao
    Chen, Lei
    Hui, Ying-Xin
    Qian, Hui
    Liu, Yan-Hui
    Wang, Dong-Sheng
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2024, 20
  • [4] Low cycle fatigue behaviour of duplex stainless steel: influence of isothermal aging treatment
    Sahu, J. K.
    Ghosh, R. N.
    Christ, H. -J.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2010, 33 (02) : 77 - 86
  • [5] Low cycle fatigue testing of 429EM stainless steel pipe
    Yoon, S
    Hong, SG
    Lee, SB
    Kim, BS
    INTERNATIONAL JOURNAL OF FATIGUE, 2003, 25 (9-11) : 1301 - 1307
  • [6] Stage I in low-cycle fatigue (LCF) damage in a duplex stainless steel (DSS)
    El Bartali, A.
    Marinelli, M. -C.
    Balbi, M.
    Aubin, V.
    Alvarez-Armas, I.
    Degallaix-Moreuil, S.
    MATERIAUX & TECHNIQUES, 2012, 100 (01): : 69 - 78
  • [7] Microstructure associated with crack initiation during low-cycle fatigue in a low nitrogen duplex stainless steel
    Alvarez-Armas, I.
    Marinelli, M. C.
    Malarria, J. A.
    Degallaix, S.
    Armas, A. F.
    INTERNATIONAL JOURNAL OF FATIGUE, 2007, 29 (04) : 758 - 764
  • [8] EFFECT OF TESTING ATMOSPHERE ON LOW-CYCLE FATIGUE OF HOT WORK TOOL STEEL AT ELEVATED-TEMPERATURE
    TSUJII, N
    ABE, G
    FUKAURA, K
    SUNADA, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1995, 81 (06): : 661 - 666
  • [9] EFFECT OF TESTING ATMOSPHERE ON LOW-CYCLE FATIGUE OF HOT WORK TOOL STEEL AT ELEVATED-TEMPERATURE
    TSUJII, N
    ABE, G
    FUKAURA, K
    SUNADA, H
    ISIJ INTERNATIONAL, 1995, 35 (07) : 920 - 926
  • [10] Identification and analysis of slip systems activated during low-cycle fatigue in a duplex stainless steel
    El Bartali, A.
    Aubin, V.
    Sabatier, L.
    Villechaise, P.
    Degallaix-Moreuil, S.
    SCRIPTA MATERIALIA, 2008, 59 (12) : 1231 - 1234