Testing and Prediction of the Strength Development of Recycled-Aggregate Concrete with Large Particle Natural Aggregate

被引:20
|
作者
Li, Changyong [1 ,2 ]
Wang, Fei [1 ,2 ]
Deng, Xiangsheng [1 ,2 ]
Li, Yizhuo [1 ,2 ]
Zhao, Shunbo [2 ,3 ]
机构
[1] North China Univ Water Resources & Elect Power, Sch Civil Engn & Commun, Zhengzhou 450045, Henan, Peoples R China
[2] North China Univ Water Resources & Elect Power, Int Joint Res Lab Ecobldg Mat & Engn Henan, Zhengzhou 450045, Henan, Peoples R China
[3] Henan Prov Collaborat Innovat Ctr Water Resources, Zhengzhou 450046, Henan, Peoples R China
关键词
recycled aggregate concrete (RAC); large particle natural aggregate; small particle recycled aggregate; fine recycled aggregate; compressive strength; splitting tensile strength; development prediction; FAIR-FACED CONCRETE; DRYING SHRINKAGE; COMPRESSIVE STRENGTH; COARSE AGGREGATE; PERFORMANCE; BEHAVIOR; SURFACE;
D O I
10.3390/ma12121891
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, a new recycled aggregate concrete (RAC) was produced with composite coarse aggregate and fine recycled aggregate. The composite coarse aggregate was mixed into continuous gradation by large particle natural aggregate with small particle recycled aggregate. To explore the time-dependent developments of the compressive strength and splitting tensile strength of this new RAC, 320 groups of cubic specimens were tested at different curing ages from 3 days to 360 days to measure the compressive and splitting tensile strengths. The amount of large particle natural aggregate varied from zero to 70% in mass of the total coarse aggregate. The water/cement ratio was taken as 0.60, 0.49, 0.41 and 0.36 to represent four strength grades of the RAC at about C20, C30, C40 and C50. Based on the tested results, the curves of the compressive and tensile strengths of the RAC that changed with curing age are plotted, which clearly exhibit that the amount of large particle natural aggregate had a rational range in different strength grades of the RAC which had better aging strength. When the RAC was no larger than C30 with a water/cement ratio of 0.60 and 0.49, the amount of large particle natural aggregate should be no more than 30%; when the RAC was no less than C40 with a water/cement ratio of 0.41 and 0.36, the amount of large particle natural aggregate should be no less than 50%. Along with the general prediction of the strength development of all the tested RAC, the optimal predictive formulas are proposed for the strength development of RAC with a rational amount of natural aggregate. Meanwhile, the strength developments of RAC with a rational amount of natural aggregate are assessed by the time-dependent models proposed by the ACI Committee 209 and CEB-FIP MC 2010.
引用
收藏
页数:19
相关论文
共 50 条
  • [1] Bond strength of FRP bars in recycled-aggregate concrete
    Godat, Ahmed
    Aldaweela, Shaima
    Aljaberi, Hamda
    Al Tamimi, Noura
    Alghafri, Ebtesam
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 267
  • [2] The introduction of recycled-aggregate concrete specifications in Japan and the research into the freezing–thawing resistance of recycled-aggregate concrete
    H. Koga
    H. Katahira
    A. Shimata
    Journal of Material Cycles and Waste Management, 2022, 24 : 1207 - 1215
  • [3] The introduction of recycled-aggregate concrete specifications in Japan and the research into the freezing-thawing resistance of recycled-aggregate concrete
    Koga, H.
    Katahira, H.
    Shimata, A.
    JOURNAL OF MATERIAL CYCLES AND WASTE MANAGEMENT, 2022, 24 (04) : 1207 - 1215
  • [4] Shear strength of recycled aggregate concrete to natural aggregate concrete interfaces
    Ceia, F.
    Raposo, J.
    Guerra, M.
    Julio, E.
    de Brito, J.
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 109 : 139 - 145
  • [5] Quality of Recycled Aggregates and Compressive Strength of No-Fines Recycled-Aggregate Concrete
    Dahri, Shakeel Ahmed
    Memon, Bashir Ahmed
    Oad, Mahboob
    Bhanbhro, Riaz
    Rahu, Ihsan Ali
    ENGINEERING TECHNOLOGY & APPLIED SCIENCE RESEARCH, 2021, 11 (05) : 7641 - 7646
  • [6] ELASTICITY AND DRYING SHRINKAGE OF RECYCLED-AGGREGATE CONCRETE
    HANSEN, TC
    BOEGH, E
    JOURNAL OF THE AMERICAN CONCRETE INSTITUTE, 1985, 82 (05): : 648 - 652
  • [7] Performance of Seawater-Mixed Recycled-Aggregate Concrete
    Younis, Adel
    Ebead, Usama
    Suraneni, Prannoy
    Nanni, Antonio
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2020, 32 (01)
  • [8] Shear strength of recycled-aggregate concrete beams with glass-FRP stirrups
    Younis, Adel
    El-Sherif, HossamEldin
    Ebead, Usama
    COMPOSITES PART C: OPEN ACCESS, 2022, 8
  • [9] Impactive Study on the Recycled Aggregate to the Strength of Recycled Aggregate Concrete
    Gao, Lin
    Xu, Guoqiang
    Shi, Yan
    Xin, Xiaofei
    PROCEEDINGS OF THE 2011 INTERNATIONAL CONFERENCE ON ENGINEERING AND RISK MANAGEMENT, 2011, : 264 - 267
  • [10] Shear strength of interfaces in natural and in recycled aggregate concrete
    Waseem, Shakeel Ahmad
    Singh, Bhupinder
    CANADIAN JOURNAL OF CIVIL ENGINEERING, 2017, 44 (03) : 212 - 222