Influence of Chloride Concentration on Stress Corrosion Cracking and Crevice Corrosion of Austenitic Stainless Steel in Saline Environments

被引:23
作者
Yeh, Chun-Ping [1 ]
Tsai, Kun-Chao [1 ]
Huang, Jiunn-Yuan [1 ]
机构
[1] Inst Nucl Energy Res INER, 1000 Wenhua Rd, Taoyuan 32546, Taiwan
关键词
chloride concentration; crevice corrosion; relative humidity; stainless steel; stress corrosion cracking; CONCRETE CASK STORAGE; SOLUTION CHEMISTRY;
D O I
10.3390/ma13245640
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Stainless steels are used as canister materials for interim storage of spent fuel. Crevice corrosion has proved to be a safety concern of 304L stainless steel spent fuel canisters, when exposed to the saline environments of coastal sites. To study the effects of chloride concentration and test duration on the crevice corrosion behavior, and the effect of relative humidity on the initiation of discrete SCC cracks, a test program was conducted on the 304L steel specimens sprayed with synthetic sea water of 3.5 wt.%. The salt-deposited specimens, wrapped up with a crevice former to form a crevice configuration, were then exposed to an environment at 45 degrees C with a pre-set 45%, 55%, and 70% relative humidity (RH), for 400 h and 10,000 h, respectively. The surface features and crack morphology of the tested 304L stainless-steel specimens were examined by energy-dispersive spectrometry (EDS) and electron back scatter diffraction (EBSD). For the specimens deposited with a chloride concentration of 1 g/m(2), no cracks were found in the corroded regions after 400-h exposure, whereas SCC cracks were observed with the specimens tested for 10,000 h at all three pre-set relative humidity. The specimens tested at the pre-set relative humidity 45% are characterized with discrete SCC cracks, but, on the other hand, those exposed to the environments of 55% and 70% relative humidity show SCC cracks of distinct features. From the results of 10,000-h tests, it is inferred that the chloride concentration threshold for SCC initiation of 304L stainless steel at 45 degrees C is between 0.1 g/m(2) and 1 g/m(2).
引用
收藏
页码:1 / 19
页数:19
相关论文
共 29 条
[1]   Effect of chloride deposition on stress corrosion cracking of 316L stainless steel used for intermediate level radioactive waste containers [J].
Albores-Silva, O. E. ;
Charles, E. A. ;
Padovani, C. .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2011, 46 (02) :124-128
[2]   In situ monitoring of crevice corrosion morphology of Type 316L stainless steel and repassivation behavior induced by sulfate ions [J].
Aoyama, Takahito ;
Sugawara, Yu ;
Muto, Izumi ;
Hara, Nobuyoshi .
CORROSION SCIENCE, 2017, 127 :131-140
[3]   Occluded solution chemistry control and the role of alloy sulfur on the initiation of crevice corrosion in type 304ss [J].
Brossia, CS ;
Kelly, RG .
CORROSION SCIENCE, 1998, 40 (11) :1851-1871
[4]   An experimental study of crevice corrosion behaviour of 316L stainless steel in artificial seawater [J].
Cai, Baoping ;
Liu, Yonghong ;
Tian, Xiaojie ;
Wang, Fei ;
Li, Hang ;
Ji, Renjie .
CORROSION SCIENCE, 2010, 52 (10) :3235-3242
[5]   THE ROLE OF CHLORIDE-IONS IN THE IR GREATER-THAN IR-STAR CRITERION FOR CREVICE CORROSION IN IRON [J].
CHO, K ;
PICKERING, HW .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1991, 138 (10) :L56-L58
[6]   Assessing the risk of under-deposit chloride-induced stress corrosion cracking in austenitic stainless steel nuclear waste containers [J].
Cook, A. B. ;
Lyon, S. B. ;
Stevens, N. P. C. ;
Gunther, M. ;
McFiggans, G. ;
Newman, R. C. ;
Engelberg, D. L. .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2014, 49 (06) :529-534
[7]   Experimental design to study the influence of temperature, pH, and chloride concentration on the pitting and crevice corrosion of UNS S30403 stainless steel [J].
Dastgerdi, Arash Azimi ;
Brenna, Andrea ;
Ormellese, Marco ;
Pedeferri, MariaPia ;
Bolzoni, Fabio .
CORROSION SCIENCE, 2019, 159
[8]   The effect of relative humidity change on atmospheric pitting corrosion of stainless steel 304L [J].
Guo, Liya ;
Street, Steven R. ;
Mohammed-Ali, Haval B. ;
Ghahari, Majid ;
Mi, Na ;
Glanvill, Sarah ;
Du Plessis, Andrew ;
Reinhard, Christina ;
Rayment, Trevor ;
Davenport, Alison J. .
CORROSION SCIENCE, 2019, 150 :110-120
[9]   Effect of temperature, chloride ion and pH on the crevice corrosion behavior of SAF 2205 duplex stainless steel in chloride solutions [J].
Han, D. ;
Jiang, Y. M. ;
Shi, C. ;
Deng, B. ;
Li, J. .
JOURNAL OF MATERIALS SCIENCE, 2012, 47 (02) :1018-1025
[10]  
He X., 2014, NUREGCR7170 US NUCL