The effect of thermo-oxidative ageing on crystallization, dynamic and static mechanical properties of long glass fibre-reinforced polyamide 10T composites

被引:15
作者
Wang, Jian [1 ,3 ]
Li, Lingtong [2 ]
He, Yong [1 ,3 ]
Song, Haishuo [1 ,3 ]
Chen, Xiaolang [2 ,3 ]
Gu, Jianbing [1 ,3 ]
机构
[1] Guizhou Univ, Coll Mat & Met, Dept Polymer Mat & Engn, Guiyang 550025, Guizhou, Peoples R China
[2] Southwest Jiaotong Univ, Sch Mat Sci & Engn, Minist Educ, Key Lab Adv Mat Technol, Chengdu 610031, Sichuan, Peoples R China
[3] Natl Engn Res Ctr Compounding & Modificat Polymer, Guiyang 550014, Guizhou, Peoples R China
基金
中国国家自然科学基金;
关键词
composites; thermo-oxidative ageing; performances; morphology; BEHAVIOR; BLENDS; WATER; DEGRADATION; ABSORPTION; STRENGTH; KINETICS;
D O I
10.1098/rsos.172029
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
The performances and microstructure of long glass fibre-reinforced polyamide 10T (PA10T/LGF) composites that experienced different ageing temperatures (160 and 200(degrees)C) with increasing ageing time are characterized by differential scanning calorimetry (DSC), mechanical analysis, thermogravimetric analysis (TGA) and scanning electron microscopy to probe the correlation between properties of the composites and thermo-oxidative ageing. The DSC results show that PA10T/LGF composites occur on degradation, the fracture of molecular chains and the destruction of crystallization structure, which leads to the crystallization and melting peaks of PA10T/LGF composites to shift to high temperature. On the basis of dynamic mechanical analysis data, the reduction of the interfacial bonding between the glass fibre and PA10T matrix and the motion of molecular chain segments result in the thermo-oxidative ageing of composites. According to the calculation of activation energy (E), thermo-oxidative temperature and ageing time can bring about the decline of the E value, proving the deterioration in performance of PA10T/LGF composites. In view of TGA, the increase in the thermo-oxidative temperature and ageing time promotes the degradation of PA10T/LGF composites. The tensile, flexural and notched impact strengths of PA10T/LGF composites decline with prolonging the ageing temperature and time. The surface of materials produces some microcracks and the cross-section surface of PA10T/LGF composites becomes rougher.
引用
收藏
页数:15
相关论文
共 36 条
[1]   Application of mean-field theory in PP/EVA blends by focusing on dynamic mechanical properties in correlation with miscibility analysis [J].
Aghjeh, Masoud Razavi ;
Khonakdar, Hossein Ali ;
Jafari, Seyed Hassan .
COMPOSITES PART B-ENGINEERING, 2015, 79 :74-82
[2]   Dielectric relaxation spectroscopy of reactively blended amorphous poly(ethylene terephthalate)-poly(ethylene naphthalate) films [J].
Becker, O ;
Simon, GP ;
Rieckmann, T ;
Forsythe, J ;
Rosu, R ;
Völker, S ;
O'Shea, M .
POLYMER, 2001, 42 (05) :1921-1929
[3]   Influence of the fibre/matrix interface on ageing mechanisms of glass fibre reinforced thermoplastic composites (PA-6,6, PET, PBT) in a hygrothermal environment [J].
Bergeret, A. ;
Ferry, L. ;
Ienny, P. .
POLYMER DEGRADATION AND STABILITY, 2009, 94 (09) :1315-1324
[4]   Combined Effect of Notches and Fibre Orientation on Fatigue Behaviour of Short Fibre Reinforced Polyamide [J].
Bernasconi, A. ;
Cosmi, F. ;
Zappa, E. .
STRAIN, 2010, 46 (05) :435-445
[5]   Effect of Graphene Nanosheets on the Mechanical, Electrical, and Rheological Properties of Polyamide 6/Acrylonitrile-Butadiene-Styrene Blends [J].
Bouhfid, R. ;
Arrakhiz, F. Z. ;
Qaiss, A. .
POLYMER COMPOSITES, 2016, 37 (04) :998-1006
[6]   Thermal-oxidative degradation of polyamide 6,6 containing metal salts [J].
Cerruti, Pierfrancesco ;
Carfagna, Cosimo .
POLYMER DEGRADATION AND STABILITY, 2010, 95 (12) :2405-2412
[7]   Water absorption and hygrothermal aging study on organomontmorillonite reinforced polyamide 6/polypropylene nanocomposites [J].
Chow, WS ;
Abu Bakar, A ;
Ishak, ZAM .
JOURNAL OF APPLIED POLYMER SCIENCE, 2005, 98 (02) :780-790
[8]   Dynamic Mechanical Properties of Pineapple Leaf Fiber Polyester Composites [J].
Devi, L. Uma ;
Bhagawan, S. S. ;
Thomas, S. .
POLYMER COMPOSITES, 2011, 32 (11) :1741-1750
[9]   Thermo-Mechanical Behavior of Polyamide 12-Polyamide 66 Recycled Fiber Composites [J].
Dorigato, Andrea ;
Fambri, Luca .
POLYMER COMPOSITES, 2011, 32 (05) :786-795
[10]   Influence of fiber content on the mechanical and thermal properties of Kenaf fiber reinforced thermoplastic polyurethane composites [J].
El-Shekeil, Y. A. ;
Sapuan, S. M. ;
Abdan, K. ;
Zainudin, E. S. .
MATERIALS & DESIGN, 2012, 40 :299-303