Influences of hot-isostatic-pressing temperature on microstructure, tensile properties and tensile fracture mode of Inconel 718 powder compact

被引:80
作者
Chang, Litao [1 ,2 ]
Sun, Wenru [1 ]
Cui, Yuyou [1 ]
Yang, Rui [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
[2] Univ Chinese Acad Sci, Beijing, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2014年 / 599卷
关键词
Powder metallurgy; Superalloy; Hot-isostatic-pressing; Prior particle boundary; Carbide; Tensile fracture; NICKEL-BASE SUPERALLOY; MECHANICAL-PROPERTIES; HEAT-TREATMENT; ALLOY; SOLIDIFICATION; PHOSPHORUS; PARTICLES; PARTS; HIP;
D O I
10.1016/j.msea.2014.01.095
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Inconel 718 powders have been hot-isostatic-pressed (HIPed) at representative temperatures to investigate the variations in microstructure, tensile properties and tensile fracture mode of the powder compact. Microstructure of the powder compacts were characterized by optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and so on. The results showed that the interdendritic precipitates inherited from the powders were partially retained in the powder compacts when the powders were HIPed at or below 1210 degrees C but were eliminated when HIPed at and above 1260 degrees C. The grain size uniformity of the powder compacts first increases and then decreases with increasing HIPing temperature. Prior particle boundaries (PPBs) were observed in the powder compacts HIPed at and below 1260 degrees C but was eliminated when HIPed at 1275 degrees C. The PPBs were decorated with carbide particles, the amount of the carbide particles at the PPBs decreases with increasing HIPing temperature. Most of the PPBs were pinned by the carbide particles in the compacts HIPed at 1140 degrees C. When the HIPing temperature was increased to 1210 degrees C and 1260 degrees C, a large number of PPBs de-pinned and moved beyond the pinning carbide particles, leading to grain growth and leaving carbide particles at the site of the original PPBs within the new grains. With increasing HIPing temperature, the 0.2% yield strength of the powder compacts at 650 degrees C decreases, the tensile elongation increases, and the tensile fracture mode changed from inter-particle dominant fracture to fully dimple ductile fracture. (c) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:186 / 195
页数:10
相关论文
共 27 条
  • [1] The effect of cooling rate on the solidification of INCONEL 718
    Antonsson, T
    Fredriksson, H
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2005, 36 (01): : 85 - 96
  • [2] High performance and high complexity net shape parts for gas turbines:: the ISOPREC® powder metallurgy process
    Baccino, R
    Moret, F
    Pellerin, F
    Guichard, D
    Raisson, G
    [J]. MATERIALS & DESIGN, 2000, 21 (04): : 345 - 350
  • [3] Bamton C., 2005, INT C HOT IS PRESS 0, P1
  • [4] Effect of heat treatment on microstructure and mechanical properties of the hot-isostatic-pressed Inconel 718 powder compact
    Chang, Litao
    Sun, Wenru
    Cui, Yuyou
    Zhang, Faqiang
    Yang, Rui
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 590 : 227 - 232
  • [5] STRENGTHENING MECHANISMS IN INCONEL-718 SUPER-ALLOY
    CHATURVEDI, MC
    HAN, YF
    [J]. METAL SCIENCE, 1983, 17 (03): : 145 - 149
  • [6] CROMPTON JS, 1986, J MATER SCI, V21, P3445, DOI 10.1007/BF02402986
  • [7] MICROSTRUCTURAL CHARACTERIZATION AND ELEMENTAL PARTITIONING IN A DIRECT-AGED SUPERALLOY (DA-718)
    FAYMAN, YC
    [J]. MATERIALS SCIENCE AND ENGINEERING, 1987, 92 : 159 - 171
  • [8] Fecht H, 2000, ADV ENG MATER, V2, P777, DOI 10.1002/1527-2648(200012)2:12<777::AID-ADEM777>3.0.CO
  • [9] 2-R
  • [10] HOT-ISOSTATIC PRESSING DIAGRAMS - NEW DEVELOPMENTS
    HELLE, AS
    EASTERLING, KE
    ASHBY, MF
    [J]. ACTA METALLURGICA, 1985, 33 (12): : 2163 - 2174