Behaviour of chlorine and alkalis in the blast furnace. and effect on sinter properties during reduction

被引:13
作者
Lectard, E [1 ]
Hess, E [1 ]
Lin, R [1 ]
机构
[1] IRSID, Dept Fonte, Serv Haut Fourneau, Arcelor, France
来源
REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES | 2004年 / 101卷 / 01期
关键词
D O I
10.1051/metal:2004142
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Thermodynamic calculations have shown that chlorine can accumulate and cycle in the shaft of the blast furnace in the form of alkalis chlorides. Cycling of chlorine and alkalis in the upper part of the shaft was simulated at laboratory scale with a counter current reduction furnace (BORIS furnace) and also directly investigated at an industrial blast furnace. Experiments and calculations shown the superposition of two cycles: one "pure" alkalis cycle in a large temperature domain, and a KCl cycle on a temperature area (600-1,000degreesC). According to the trials, effects of KCl on reduction and disintegration behaviour of sinter are similar to those of "pure" alkalis.
引用
收藏
页码:31 / 38
页数:8
相关论文
共 3 条
[1]  
LIN R, 2001, INV CHLOR ALK BEH BL
[2]  
LU WK, 1980, BLAST FURN C ARL 2 4
[3]  
SCHNEIDER M, 1979, REV METALL-PARIS, V76, P621