Thermally grown oxide films and corrosion performance of ferritic stainless steels under simulated exhaust gas condensate conditions

被引:44
作者
Huttunen-Saarivirta, E. [1 ]
Kuokkala, V. -T. [1 ]
Pohjanne, P. [2 ]
机构
[1] Tampere Univ Technol, Dept Mat Sci, FI-33101 Tampere, Finland
[2] VTT Tech Res Ctr Finland, FI-02044 Espoo, Finland
关键词
Stainless steel; Oxidation; Selective oxidation; Intergranular corrosion; IR spectroscopy; EIS; SEMICONDUCTING PROPERTIES; OXIDATION RESISTANCE; PITTING CORROSION; TEMPERATURE; BEHAVIOR; ALLOY; 316L;
D O I
10.1016/j.corsci.2014.06.041
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Five ferritic stainless steels are characterized in terms of thermally grown oxide films and corrosion performance under simulated exhaust gas condensate conditions. Oxide films developed at 300 degrees C show only little variation in microstructure and properties between the alloys, whereas those evolved at 600 degrees C exhibit clear differences. Especially in alloys with >11.5 wt.% chromium, the presence and distribution of such alloying elements as titanium, silicon, niobium and molybdenum are crucial for the film properties and the overall corrosion performance. The results may be exploited in the compositional optimization of the alloys for the cold-end components of automotive exhaust system. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:344 / 365
页数:22
相关论文
共 67 条
[1]   Optimization of the electrical properties of Ti-Nb stabilized ferritic stainless steel SOFC interconnect alloy upon high-temperature oxidation: The role of excess Nb on the interfacial oxidation at the oxide-metal interface [J].
Ali-Loytty, H. ;
Jussila, P. ;
Valden, M. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (02) :1039-1051
[2]   Influence of precipitation on initial high-temperature oxidation of Ti-Nb stabilized ferritic stainless steel SOFC interconnect alloy [J].
Ali-Loytty, H. ;
Jussila, P. ;
Juuti, T. ;
Karjalainen, L. P. ;
Zakharov, A. A. ;
Valden, M. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2012, 37 (19) :14528-14535
[3]   Influence of CrN surface compound on the initial stages of high temperature oxidation of ferritic stainless steel [J].
Ali-Loytty, H. ;
Jussila, P. ;
Hirsimaki, M. ;
Valden, M. .
APPLIED SURFACE SCIENCE, 2011, 257 (17) :7783-7791
[4]  
[Anonymous], ATZ WORLDWIDE
[5]  
[Anonymous], 2010, RES MET MAT COND COR
[6]  
[Anonymous], 2006, STEEL
[7]   Comparison of influences of NaCl and CaCl2 on the corrosion of 11% and 17% Cr ferritic stainless steels during cyclic corrosion test [J].
Beom, Won-Jin ;
Yun, Kwi-Sub ;
Park, Chan-Jin ;
Ryu, Han-Jin ;
Kim, Young-Ho .
CORROSION SCIENCE, 2010, 52 (03) :734-739
[8]  
Birks N, 2006, INTRODUCTION TO THE HIGH-TEMPERATURE OXIDATION OF METALS, 2ND EDITION, P1, DOI 10.1017/CBO9781139163903
[9]   Characterization of the oxides formed at 1000 °C on the AISI 316L stainless steel -: Role of molybdenum [J].
Buscail, H. ;
El Messki, S. ;
Riffard, F. ;
Perrier, S. ;
Cueff, R. ;
Caudron, E. ;
Issartel, C. .
MATERIALS CHEMISTRY AND PHYSICS, 2008, 111 (2-3) :491-496
[10]   Influence of various gaseous environments on SiO2 formation on the 330Cb (Fe-35Ni-18Cr-1Nb-2.15Si) alloy at 900 °C [J].
Buscail, Henri ;
Issartel, C. ;
Riffard, F. ;
Rolland, R. ;
Perrier, S. ;
Fleurentin, A. .
CORROSION SCIENCE, 2012, 65 :535-541