Conceiving a feasible degradation model of polylactic acid-based composites through hydrolysis study to polylactic acid/wood flour/polymethyl methacrylate

被引:34
作者
Wan, Lu [1 ]
Li, Changxin [1 ]
Sun, Ce [1 ]
Zhou, Shuai [1 ]
Zhang, Yanhua [1 ]
机构
[1] Northeast Forestry Univ, Coll Mat Sci & Engn, Key Lab Biobased Mat Sci & Technol, Harbin, Heilongjiang, Peoples R China
基金
中国国家自然科学基金;
关键词
Polylactic acid; Model construction; Rapid hydrolysis; Composite material; POLY(LACTIC ACID); POLY(METHYL METHACRYLATE); BIODEGRADABLE POLYMERS; POLY(L-LACTIC ACID); THERMAL-PROPERTIES; GRAPHENE OXIDE; PLA; BEHAVIOR; CRYSTALLIZATION; NANOCOMPOSITES;
D O I
10.1016/j.compscitech.2019.06.002
中图分类号
TB33 [复合材料];
学科分类号
摘要
On the road of wide popularization and application of polylactic acid (PLA), its degradation performance frequently fetters the advancing feet. The work attempted to develop a (PLA & Coating-layer) @Filler [(PLA&C)@F] model composite with high-effective degradation property in order to clear the obstacles for the promotion of PLA-based-materials products and alleviate the environmental burden. Firstly, PLA/wood flour/polymethyl methacrylate composite was fabricated by melt blending PLA, wood flour and polymethyl methacrylate, and (PLA & polymethyl methacrylate) @wood flour as a demonstration model was established. Then, the degradation rate of PLA/wood flour/polymethyl methacrylate and neat PLA was evaluated by hydrolysis test. The composite of (PLA & polymethyl methacrylate) @wood flour demonstration model achieved satisfying result, its hydrolysis rate was 8.56 times faster than that of neat PLA under the same conditions. The reasons were attained through various testing methods. Lastly, the characterization of Fourier Transform Infrared Spectroscopy (FTIR), the test of differential scanning calorimetry (DSC), and the observation of scanning electron microscope (SEM) to the materials in predetermined stages were applied to determine significant pieces of real-time information. By combining various information to provide right characterization for studying super-fast hydrolysis mechanism of PLA/wood flour/polymethyl methacrylate. The development of (PLA & Coating-layer) @Filler [PLA&C)@F] model is a significant work both accelerating research and even controllable exploration of PLA-based composite degradation.
引用
收藏
页数:11
相关论文
共 62 条
  • [1] Tuning the Degradation Profiles of Poly(L-lactide)-Based Materials through Miscibility
    Arias, Veluska
    Hoglund, Anders
    Odelius, Karin
    Albertsson, Ann-Christine
    [J]. BIOMACROMOLECULES, 2014, 15 (01) : 391 - 402
  • [2] Pyrolysis-GC-MS reveals important differences in hydrolytic degradation process of wood flour and rice bran filled polylactide composites
    Azwar, Edwin
    Vuorinen, Eino
    Hakkarainen, Minna
    [J]. POLYMER DEGRADATION AND STABILITY, 2012, 97 (03) : 281 - 287
  • [3] Graphene Oxide-Templated Synthesis of Hydroxyapatite Nanowhiskers To Improve the Mechanical and Osteoblastic Performance of Poly(lactic acid) for Bone Tissue Regeneration
    Chen, Chen
    Sun, Xiaodong
    Pan, Wu
    Hou, Yi
    Liu, Rui
    Jiang, Xin
    Zhang, Li
    [J]. ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2018, 6 (03): : 3862 - 3869
  • [4] Hydrolytic degradation behavior of poly(L-lactide)/SiO2 composites
    Chen, Hai-ming
    Wang, Yang-peng
    Chen, Jie
    Yang, Jing-hui
    Zhang, Nan
    Huang, Ting
    Wang, Yong
    [J]. POLYMER DEGRADATION AND STABILITY, 2013, 98 (12) : 2672 - 2679
  • [5] Hydrolytic degradation behavior of poly(L-lactide)/carbon nanotubes nanocomposites
    Chen, Hai-Ming
    Feng, Chen-Xia
    Zhang, Wen-Bin
    Yang, Jing-Hui
    Huang, Ting
    Zhang, Nan
    Wang, Yong
    [J]. POLYMER DEGRADATION AND STABILITY, 2013, 98 (01) : 198 - 208
  • [6] Clemons CM, 2005, FUNCTIONAL FILLERS FOR PLASTICS, P249, DOI 10.1002/3527605096.ch15
  • [7] PLA-PMMA blends: A study by XPS and ToF-SIMS
    Cossement, D.
    Gouttebaron, R.
    Cornet, V.
    Viville, P.
    Hecq, M.
    Lazzaroni, R.
    [J]. APPLIED SURFACE SCIENCE, 2006, 252 (19) : 6636 - 6639
  • [8] Stimulation by Pearl of Mineralization and Biocompatibility of PLA
    Dai, Jiamu
    Bai, Jingjing
    Jin, Junhong
    Yang, Shenglin
    Li, Guang
    [J]. ADVANCED ENGINEERING MATERIALS, 2015, 17 (11) : 1691 - 1697
  • [9] Accelerated ageing and degradation in poly-L-lactide/hydroxyapatite nanocomposites
    Delabarde, Claire
    Plummer, Christopher J. G.
    Bourban, Pierre-Etienne
    Manson, Jan-Anders E.
    [J]. POLYMER DEGRADATION AND STABILITY, 2011, 96 (04) : 595 - 607
  • [10] Miscibility and crystallization behaviors of stereocomplex-type poly(L- and D-lactide)/poly(methyl methacrylate) blends
    Dong, Qinglin
    Bian, Yijie
    Li, Yi
    Han, Changyu
    Dong, Lisong
    [J]. JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2014, 118 (01) : 359 - 367