Coupling of superduplex stainless steel and cast nickel-aluminium bronze in sea water

被引:5
|
作者
Francis, R [1 ]
机构
[1] Weir Mat & Foundries, Pk Works, Manchester M40 2BA, Lancs, England
来源
BRITISH CORROSION JOURNAL | 1999年 / 34卷 / 02期
关键词
D O I
10.1179/000705999101500789
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Tests have been performed at about 25 degrees C in both natural and chlorinated sea waters on couples of nickel-alminium bronze (NAB) and Zeron 100 (Z100) superduplex stainless steel. Two NAB/Z100 area ratios (1 : 1 and 1 : 10) were used in exposures of 60 days. The results in natural sea water showed severe localised corrosion of NAB both in the crevices and on open surfaces at both area ratios. In chlorinated sea water there was no corrosion at a 1 : 1 area ratio. The attack is explained in terms of the different cathodic reactions occurring in natural and chlorinated sea waters, and the metallurgical structure of: NAB. Service experiences with couples of NAB and superduplex stainless steel are described and recommendations are given for the avoidance of problems.
引用
收藏
页码:139 / 144
页数:6
相关论文
共 50 条
  • [21] The influence of nickel-aluminium bronze microstructure and crevice solution on the initiation of crevice corrosion
    Wharton, J. A.
    Stokes, K. R.
    ELECTROCHIMICA ACTA, 2008, 53 (05) : 2463 - 2473
  • [22] Electrochemical behaviour of nickel-aluminium bronze in chloride media: Influence of pH and benzotriazole
    Neodo, S.
    Carugo, D.
    Wharton, J. A.
    Stokes, K. R.
    JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 2013, 695 : 38 - 46
  • [23] Electrochemical corrosion mechanisms of nickel-aluminium bronze with different nickel contents using the rotating disc electrode
    Yang, Fenfen
    Kang, Huijun
    Chen, Zongning
    Guo, Enyu
    Zeng, Yanhua
    Wang, Wei
    Wang, Tongmin
    CORROSION SCIENCE, 2019, 157 : 438 - 449
  • [24] Observing early cavitation damage evolution from repeated laser-induced single bubbles on aluminium, austenitic steel and nickel-aluminium bronze
    de Arcaute y Lozano, C. Lopez
    Kuehlmann, J.
    Kaiser, S. A.
    Hanke, S.
    WEAR, 2023, 523
  • [25] EFFECT OF PRE-HEAT TREATMENT ON CORROSION BEHAVIOR OF NICKEL-ALUMINIUM BRONZE ALLOY
    Daroonparvar, M. R.
    Atabaki, M. Mazar
    Vakilipour, A.
    METALLURGICAL & MATERIALS ENGINEERING-ASSOCIATION OF METALLURGICAL ENGINEERS OF SERBIA, 2011, 17 (04): : 183 - 198
  • [26] Precipitation strengthening of nickel-aluminium bronze during multi-stage ageing process
    Gryziecki, J
    Latkowski, A
    ARCHIVES OF METALLURGY, 2003, 48 (02): : 151 - 160
  • [27] The role of nickel in mechanical performance and corrosion behaviour of nickel-aluminium bronze in 3.5 wt.% NaCl solution
    Yang, Fenfen
    Kang, Huijun
    Guo, Enyu
    Li, Rengeng
    Chen, Zongning
    Zeng, Yanhua
    Wang, Tongmin
    CORROSION SCIENCE, 2018, 139 : 333 - 345
  • [28] Wear and Corrosion Properties of Stellite-6 Coating Fabricated by HVOF on Nickel-Aluminium Bronze Substrate
    Mousavi, Seyed Elias
    Naghshehkesh, Nastaran
    Amirnejad, Mohabbat
    Shammakhi, Hossein
    Sonboli, Ali
    METALS AND MATERIALS INTERNATIONAL, 2021, 27 (09) : 3269 - 3281
  • [29] The role of microstructural characteristics in the cavitation erosion behaviour of laser melted and laser processed Nickel-Aluminium Bronze
    Cottam, R.
    Luzin, V.
    Moody, H.
    Edwards, D.
    Majumdar, A.
    Wong, Y. C.
    Wang, J.
    Brandt, M.
    WEAR, 2014, 317 (1-2) : 56 - 63
  • [30] Microstructures and properties of micro-alloyed nickel-aluminium bronze ingot by scandium, zirconium and strontium composite
    Xu, Xiao-Jing
    Chen, Shu-Dong
    Chu, Man-Jun
    Pan, Li
    Wei, Jian
    Shi, Guo-Fang
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2013, 23 (12): : 3381 - 3386