Mechanical properties and corrosion behavior of novel β-type biomaterial Zr-6Mo-4Ti-xY alloys in simulated body fluid Ringer's lactate solution for implant applications

被引:1
作者
Awwaluddin, Muhammad [1 ]
Prajitno, Djoko Hadi [2 ]
Adi, Wisnu Ari [3 ]
Kartaman, Maman [4 ]
Soemardi, Tresna P. [1 ]
机构
[1] Univ Indonesia, Fac Engn, Dept Mech Engn, Depok 16424, Indonesia
[2] Natl Nucl Energy Agcy Indonesia, Ctr Appl Nucl Sci & Technol, Jakarta, Indonesia
[3] Natl Nucl Agcy Indonesia BATAN, Ctr Sci & Technol Adv Mat, Tangerang Selatan 15314, Banten, Indonesia
[4] Natl Nucl Energy Agcy Indonesia, Ctr Nucl Fuel Technol, Jakarta 12710, Indonesia
关键词
Zr alloy; corrosion resistance; yttrium; biomaterial; Zr-6Mo-4Ti-xY; ZIRCONIUM; MICROSTRUCTURE; YTTRIUM; ELEMENT;
D O I
10.3934/matersci.2020.6.887
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To develop new biomaterials for implant applications, the novel biomaterial multi component Zr-Mo-Ti-xY (x = 1, 2, 3) alloys were developed as a solution to increase mechanical properties and a corrosion resistance and to reduce the toxicity of biomaterials for implant. This research is aimed to investigate the effects of yttrium (Y) element addition to the microstructural transformation, mechanical properties and corrosion behavior of the alloy. The Zr-6Mo-4Ti-xY (x = 1, 2, 3) alloys are made by melting the metals using a vacuum single arc melting furnace with high purity argon gas flow at atmospheric pressure and tungsten electrodes with a six-times remelted process. The hardness test was conducted using the Vickers hardness tester, the microstructure analysis was done using the optical microscopes, and the alloy compound and phases using the XRD and corrosion resistance test were carried out using the polarization method in simulated body fluid Ringer's lactate solution. The values of the hardness test of Zr-6Mo-4Ti-xY (x = 1, 2, 3) alloys are 461.8, 301.5 and 335.1 HV, respectively. The basketweave-shaped microstructure with the addition of yttrium moderately creates little grain measure. The corrosion rate of Zr-6Mo-4Ti-xY (x = 1, 2, 3) alloys which are 0.3159, 0.2705 and 0.3759 mpy respectively, are categorized as outstanding ( the corrosion resistance of <1 mpy) so that it can be considered as a potential biomaterial for implant applications.
引用
收藏
页码:887 / 901
页数:15
相关论文
共 27 条
[1]   Evaluation of corrosion resistance of implant-use Ti-Zr binary alloys with a range of compositions [J].
Akimoto, Teisuke ;
Ueno, Takeshi ;
Tsutsumi, Yusuke ;
Doi, Hisashi ;
Hanawa, Takao ;
Wakabayashi, Noriyuki .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2018, 106 (01) :73-79
[2]   Corrosion behavior of new quaternary ZrNbTiAl alloys in simulated physiological solution using electrochemical techniques and surface analysis methods [J].
Chelariu, R. ;
Trinca, L. C. ;
Munteanu, C. ;
Bolat, G. ;
Sutiman, D. ;
Mareci, D. ;
Souto, R. M. .
ELECTROCHIMICA ACTA, 2017, 248 :368-375
[3]   Effect of low-temperature pre-deformation on precipitation behavior and microstructure of a Zr-Sn-Nb-Fe-Cu-O alloy during fabrication [J].
Chen, Liangyu ;
Li, Jiuxiao ;
Zhang, Yao ;
Lu, Weijie ;
Zhang, Lai-Chang ;
Wang, Liqiang ;
Zhang, Di .
JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 2016, 53 (04) :496-507
[4]   Metallic implant biomaterials [J].
Chen, Qizhi ;
Thouas, George A. .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2015, 87 :1-57
[5]   Titanium-zirconium alloy narrow-diameter implants (Straumann Roxolid®) for the rehabilitation of horizontally deficient edentulous ridges: prospective study on 18 consecutive patients [J].
Chiapasco, M. ;
Casentini, P. ;
Zaniboni, M. ;
Corsi, E. ;
Anello, T. .
CLINICAL ORAL IMPLANTS RESEARCH, 2012, 23 (10) :1136-1141
[6]   Corrosion of Metallic Biomaterials: A Review [J].
Eliaz, Noam .
MATERIALS, 2019, 12 (03)
[7]   Cryo-rolling enhanced inhomogeneous deformation and recrystallization grain growth of a zirconium alloy [J].
He, Weijun ;
Chen, Xin ;
Liu, Na ;
Luan, Baifeng ;
Yuan, Gaihuan ;
Liu, Qing .
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 699 :160-169
[8]   Bio-corrosion study on zirconium-based bulk-metallic glasses [J].
Huang, Lu ;
Qiao, Dongchun ;
Green, Brandice A. ;
Liaw, Peter K. ;
Wang, Jianfeng ;
Pang, Shujie ;
Zhang, Tao .
INTERMETALLICS, 2009, 17 (04) :195-199
[9]  
KUTSAR AR, 1973, DOKL AKAD NAUK SSSR+, V213, P81
[10]  
Lee L, 1963, CORROSION CHARACTERI