Alkaline Stability of Benzyl Trimethyl Ammonium Functionalized Polyaromatics: A Computational and Experimental Study

被引:168
作者
Choe, Yoong-Kee [1 ]
Fujimoto, Cy [2 ]
Lee, Kwan-Soo [3 ]
Dalton, Luke T. [4 ]
Ayers, Kathy [4 ]
Henson, Neil J. [5 ]
Kim, Yu Seung [3 ]
机构
[1] Natl Inst Adv Ind Sci & Technol, Tsukuba, Ibaraki 3058568, Japan
[2] Sandia Natl Labs, Albuquerque, NM 87185 USA
[3] Los Alamos Natl Lab, Sensors & Electrochem Devices Grp, Los Alamos, NM 87545 USA
[4] Proton Onsite, Wallingford, CT 06492 USA
[5] Los Alamos Natl Lab, Los Alamos, NM 87545 USA
关键词
POLY(ARYLENE ETHER SULFONE); ANION-EXCHANGE MEMBRANES; FUEL-CELLS; DEGRADATION; IONOMER;
D O I
10.1021/cm502422h
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Alkaline stability of benzyl trimethylammonium (BTMA)-fiinctionalized polyaromatic membranes was investigated by computational modeling and experimental methods. The barrier height of hydroxide initiated aryl-ether cleavage in the polymer backbone was computed to be 85.8 kJ/mol, a value lower than the nucleophilic substitution of the alpha-carbons on the benzylic position of BTMA cationic functional group, computed to be 90.8 kJ/mol. The barrier heights of aryl aryl cleavage (polymer backbone) are 223.8-246.0 kJ/mol. The computational modeling study suggests that the facile aryl ether cleavage is not only due to the electron deficiency of the aryl group but also due to the low bond dissociation energy arising from the ether substituent. Ex situ degradation studies using Fourier transform infrared (FTIR) and H-1 nuclear magnetic resonance (NMR) spectroscopy indicated that 61% of the aryl ether groups degraded after 2 h of treatment in 0.5 M NaOH at 80 degrees C. BTMA cationic groups degraded slowly over 48 h under the same conditions. In situ degradation studies validate the calculated results: anion exchange membrane fuel cells and water electrolyzer using poly(arylene ether) membranes exhibit a catastrophic, premature failure during lifetime tests, while no sudden performance loss is observed with an ether-free poly(phenylene) membrane. Despite the gradual performance loss due to the degradation of BTMA cation functional group, the membrane electrode assembly using the poly(phenylene) membrane exhibited a lifetime of >2000 h in the alkaline water electrolyzer mode at 50 degrees C.
引用
收藏
页码:5675 / 5682
页数:8
相关论文
共 36 条
  • [1] Two-dimensional NMR spectroscopy reveals cation-triggered backbone degradation in polysulfone-based anion exchange membranes
    Arges, Christopher G.
    Ramani, Vijay
    [J]. PROCEEDINGS OF THE NATIONAL ACADEMY OF SCIENCES OF THE UNITED STATES OF AMERICA, 2013, 110 (07) : 2490 - 2495
  • [2] Polymers with pendant functional group .3. Polysulfones containing viologen group
    Avram, E
    Butuc, E
    Luca, C
    Druta, I
    [J]. JOURNAL OF MACROMOLECULAR SCIENCE-PURE AND APPLIED CHEMISTRY, 1997, A34 (09): : 1701 - 1714
  • [3] Characterization of Anion Exchange Membrane Technology for Low Cost Electrolysis
    Ayers, K. E.
    Anderson, E. B.
    Capuano, C. B.
    Niedzweicki, M.
    Hickner, M.
    Wang, C-Y
    Len, Y.
    Zhou, W.
    [J]. FUEL CELL MEMBRANES, ELECTRODE BINDERS, AND MEA PERFORMANCE, 2013, 45 (23): : 121 - 130
  • [4] AROMATIC NUCLEOPHILIC SUBSTITUTION REACTIONS
    BUNNETT, JF
    ZAHLER, RE
    [J]. CHEMICAL REVIEWS, 1951, 49 (02) : 273 - 412
  • [5] Long-range corrected hybrid density functionals with damped atom-atom dispersion corrections
    Chai, Jeng-Da
    Head-Gordon, Martin
    [J]. PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2008, 10 (44) : 6615 - 6620
  • [6] Mechanism of tetraalkylammonium headgroup degradation in alkaline fuel cell membranes
    Chempath, Shaji
    Einsla, Brian R.
    Pratt, Lawrence R.
    Macomber, Clay S.
    Boncella, James M.
    Rau, Jonathan A.
    Pivovar, Bryan S.
    [J]. JOURNAL OF PHYSICAL CHEMISTRY C, 2008, 112 (09) : 3179 - 3182
  • [7] Density Functional Theory Study of Degradation of Tetraalkylammonium Hydroxides
    Chempath, Shaji
    Boncella, James M.
    Pratt, Lawrence R.
    Henson, Neil
    Pivovar, Bryan S.
    [J]. JOURNAL OF PHYSICAL CHEMISTRY C, 2010, 114 (27) : 11977 - 11983
  • [8] The Effect of Cathode Structures on Nafion Membrane Durability
    Choi, Baeck
    Langlois, David A.
    Mack, Nate
    Johnston, Christina M.
    Kim, Yu Seung
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2014, 161 (12) : F1154 - F1162
  • [9] Cope A. C., 2011, OLEFINS AMINES HOFMA, P317
  • [10] ABINITIO DETERMINATION OF SUBSTITUENT CONSTANTS IN A DENSITY FUNCTIONAL THEORY FORMALISM - CALCULATION OF INTRINSIC GROUP ELECTRONEGATIVITY, HARDNESS, AND SOFTNESS
    DEPROFT, F
    LANGENAEKER, W
    GEERLINGS, P
    [J]. JOURNAL OF PHYSICAL CHEMISTRY, 1993, 97 (09) : 1826 - 1831