Evolution of precipitates in ZK60 magnesium alloy during high strain rate deformation

被引:43
作者
Yang, Yang [1 ,2 ,3 ]
Wang, Zhen [1 ]
Jiang, Lihong [1 ]
机构
[1] Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] Cent S Univ, Key Lab, Minist Educ Nonferrous Met Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[3] China Acad Engn Phys, Inst Fluid Phys, Mianyang 621900, Peoples R China
基金
中国国家自然科学基金;
关键词
High strain rate; Precipitates; TEM; ZK60 magnesium alloy; MG-ZN ALLOY; SELF-ORGANIZATION; ALUMINUM-ALLOY; HEAT-TREATMENT; SHEAR BANDS; MICROSTRUCTURE; BEHAVIOR; STEEL; STABILITY; TORSION;
D O I
10.1016/j.jallcom.2017.02.158
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
High strain rate(6.2 x 10(4) s(-1)) loading of ZK60 magnesium alloy was carried out with radial collapse of a thick-walled cylinder technology. The evolution of precipitates in solution-treated and peak-aged ZK60 magnesium alloy during high strain rate deformation was studied by transmission electron microscopy (TEM) for the first time. A large number of elongated rod-like phase were precipitated in solution-treated sample after impacting; the rod-like phases in peak-aged sample experienced shortening and thinning, and some of which finally transformed into spherical-like phases, namely the rod-like phases were preliminarily dissolved into the matrix. Based on thermodynamics and kinetics analyses, the high strain rate, high density dislocation, high shear stress and adiabatic temperature rise induced by explosive impact process make it possible for precipitates to precipitate and dissolve preliminarily within about 3.1 mu s. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:566 / 571
页数:6
相关论文
共 50 条
  • [21] Effect of Rolling Process on Microstructures and Mechanical Properties of High Strain-Rate Rolled ZK60 Magnesium Alloy
    Xvhui Feng
    Youping Sun
    Xvhuang Feng
    Jiangmei He
    Siyu Wan
    Russian Journal of Non-Ferrous Metals, 2020, 61 : 658 - 666
  • [22] Cyclic deformation and fatigue of extruded ZK60 magnesium alloy with aging effects
    Dong, Shuai
    Jiang, Yanyao
    Dong, Jie
    Wang, Fenghua
    Ding, Wenjiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 615 : 262 - 272
  • [23] An experimental study on cyclic deformation and fatigue of extruded ZK60 magnesium alloy
    Yu, Qin
    Zhang, Jixi
    Jiang, Yanyao
    Li, Qizhen
    INTERNATIONAL JOURNAL OF FATIGUE, 2012, 36 (01) : 47 - 58
  • [24] Effect of cryogenic cooling on texture and microstructural evolution of ZK60 magnesium alloy during machining
    Dinesh, S.
    Senthilkumar, V
    Asokan, P.
    MATERIALS RESEARCH EXPRESS, 2019, 6 (09)
  • [25] Effect of Grain Size on Dynamic Compression Behavior and Deformation Mechanism of ZK60 Magnesium Alloy
    Liu, Xuanyu
    Mao, Pingli
    Zhou, Le
    Wang, Xueting
    Wang, Zhi
    Wang, Feng
    Wei, Ziqi
    Liu, Zheng
    METALS, 2023, 13 (02)
  • [26] Strength Improvement in ZK60 Magnesium Alloy Induced by Pre-deformation and Heat Treatment
    Chen Xianhua
    Liu Lizi
    Pan Fusheng
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2016, 31 (02): : 393 - 398
  • [27] Effect of heat treatment on adiabatic shear susceptibility in ZK60 magnesium alloy
    Yang, Yang
    Jiang, Lihong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 664 : 146 - 154
  • [28] Multiaxial fatigue of extruded ZK60 magnesium alloy
    Albinmousa, Jafar
    Adinoyi, Muhammed J.
    Merah, Nesar
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2019, 42 (10) : 2276 - 2289
  • [29] Research on the homogenization of ZK60 magnesium alloy ingot
    Zhang, DF
    Peng, J
    Jiang, B
    MAGNESIUM - SCIENCE, TECHNOLOGY AND APPLICATIONS, 2005, 488-489 : 341 - 344
  • [30] Evolution of Microstructure, Texture and Mechanical Properties of ECAP-Processed ZK60 Magnesium Alloy
    Khoubrou, Iraj
    Nami, Bahram
    Miresmaeili, Seyyed Mehdi
    Yazdani, Milad
    METALS AND MATERIALS INTERNATIONAL, 2025, 31 (01) : 227 - 236