Effect of adhesive free-end geometry on the initiation and propagation of damaged zones in adhesively bonded lap joints

被引:25
|
作者
Apalak, MK [1 ]
Engin, A
机构
[1] Erciyes Univ, Dept Mech Engn, TR-38039 Kayseri, Turkey
[2] Erciyes Univ, Grad Sch Nat & Appl Sci, TR-38039 Kayseri, Turkey
关键词
adhesive joint; geometrical non-linearity; material non-linearity; plasticity; damaged zone; stress analysis; adhesive fillet;
D O I
10.1163/156856104839293
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
In this study the effect of adhesive free-end geometry on the initiation and propagation of damaged zones in adhesively bonded single- and double-lap joints was investigated considering the material non-linear behaviour of both adhesive and adherends and the geometrical non-linearity. The damaged adhesive and adherend zones exceeding the specified ultimate strains were determined based on the modified von Mises criterion for adherends and the failure criterion, including the effects of the hydrostatic stress states for the epoxy adhesives proposed by Raghava and Cadell. The stiffness of each finite element in the damaged zones was reduced to a negligible value, thus not contributing to the overall stiffness of the adhesive joint. This simple method provides useful information on the initiation and propagation of damaged zones in both the adhesive layer and adherends. The damaged adhesive zones due to a tensile load were observed to initiate around the rounded adherend corners inside the adhesive fillets and to propagate first towards both the free surface of the adhesive fillet and across the adhesive layer, and later along the adherend-adhesive interface. The damaged adhesive zones initiate at the left free-end of the adhesive-upper adherend inter-face and at the right free-end of the adhesive-lower adherend interface and propagate along these interfaces in the large adhesive fillets. In the bending test, the damaged adhesive zones appeared only at the left free-end in tension of the adhesive-upper adherend interface for the large adhesive fillets, but around the lower adherend corner for the smaller adhesive fillets. Later, it propagated with a similar mechanism as in the tensile load. In a double-lap joint subjected to a tensile load, the damaged zone appeared around the upper adherend corner inside the right adhesive fillet in tension, and propagated first towards the free surface of the adhesive fillet and through the adhesive layer towards the adhesive-middle adherend interface, and later along this interface. For all loading conditions, increasing the adhesive fillet size caused the damaged zone initiation to occur at a larger load level. The SEM micrographs of fracture surfaces around the adhesive fillets showed that the damaged zones initiated around the adherend corner inside the adhesive fillet and propagated through the adhesive fillets.
引用
收藏
页码:529 / 559
页数:31
相关论文
共 50 条
  • [1] An investigation on the initiation and propagation of damaged zones in adhesively bonded lap joints
    Kemal Apalak, M.
    Engin, Aysel
    1889, VSP BV (17):
  • [2] An investigation on the initiation and propagation of damaged zones in adhesively bonded lap joints
    Apalak, MK
    Engin, A
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2003, 17 (14) : 1889 - 1921
  • [3] Adhesively bonded lap joints with extreme interface geometry
    Haghpanah, Babak
    Chiu, Shihung
    Vaziri, Ashkan
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2014, 48 : 130 - 138
  • [4] Material and adhesive effect in adhesively-bonded composite stepped-lap joints
    Brito, R. F. N.
    Campilho, R. D. S. G.
    Moreira, R. D. F.
    Sanchez-Arce, I. J.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART G-JOURNAL OF AEROSPACE ENGINEERING, 2020, 234 (13) : 1967 - 1979
  • [5] The effect of geometry on joint strength in adhesively bonded joints with the same adhesive area
    Akpinar, Salih
    Hacisalihoglu, Ilyas
    Calik, Ahmet
    MECHANICS OF ADVANCED MATERIALS AND STRUCTURES, 2024, 31 (12) : 2635 - 2647
  • [6] Fatigue initiation in adhesively-bonded single-lap joints
    Solana, A. Graner
    Crocombe, A. D.
    Wahab, M. M. Abdel
    Ashcroft, I. A.
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2007, 21 (14) : 1343 - 1357
  • [7] Fatigue initiation in adhesively-bonded single-lap joints
    Solana, A. Graner
    Crocombe, A.D.
    Wahab, M. M. Abdel
    Ashcroft, I.A.
    Journal of Adhesion Science and Technology, 2007, 21 (14): : 1343 - 1357
  • [8] Effect of using fibre reinforced epoxy adhesive on the strength of the adhesively bonded Single Lap Joints
    Behera, Ranjan K.
    Parida, S. K.
    Das, R. R.
    COMPOSITES PART B-ENGINEERING, 2023, 248
  • [9] Application of adhesively bonded single lap joints for fracture assessment of adhesive materials
    Akhavan-Safar, A.
    Ayatollahi, M. R.
    Bahreinian, S. A.
    da Silva, L. F. M.
    JOURNAL OF ADHESION, 2019, 95 (01): : 1 - 22
  • [10] The effect of opposing notch geometry on the tensile strength of adhesively bonded single-lap joints
    Cam, Salim
    Ozel, Adnan