The interfacial bilayer Cu6Sn5 formed in a Sn-Ag-Cu flip-chip solder joint incorporating Au/Pd metallization during solid-state aging

被引:6
作者
Liang, Chien-Lung [1 ]
Lin, Kwang-Lung [1 ]
Cheng, Po-Jen [2 ]
机构
[1] Natl Cheng Kung Univ, Dept Mat Sci & Engn, 1 Univ Rd, Tainan 70101, Taiwan
[2] Adv Semicond Engn ASE Grp, 26,Chin 3rd Rd, Kaohsiung 81170, Taiwan
关键词
LEAD-FREE SOLDERS; ELECTROLESS NI-P; INTERMETALLIC COMPOUNDS; TIO2; NANOPARTICLES; IMC GROWTH; COMPOUND; ALLOYS; AUSN4; AU; REDEPOSITION;
D O I
10.1007/s10854-018-9665-0
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
A solid-state reaction between the Sn-Ag-Cu solder and Ni metallization resulted in the formation of interfacial bilayer Cu6Sn5-based intermetallic compounds (IMCs) in a solder joint incorporating Au/Pd metallization. The layer near the Ni metallization was identified as (Cu,Ni,Au)(6)Sn-5 containing 20.3 at.% of Ni and 1.7 at.% of Au, and the layer near the solder matrix was identified as (Cu,Au,Ni,Pd)(6)Sn-5 containing 5.7 at.% of Au, 1.2 at.% of Ni, and 1.0 at.% of Pd. The electron diffraction analysis with high resolution transmission electron microscopy further characterized the interfacial bilayer IMCs as having the same hexagonal crystal structure with different crystal orientations. The kinetics study revealed that the (Cu,Ni,Au)(6)Sn-5 in the interfacial bilayer reaction products was formed during the initial reflow process, while the (Cu,Au,Ni,Pd)(6)Sn-5 layer was formed during subsequent solid-state aging. Predominant growth of the (Cu,Au,Ni,Pd)(6)Sn-5 layer was observed during solid-state aging. In contrast, the growth of the initially formed (Cu,Ni,Au)(6)Sn-5 layer was suppressed. The growth of the (Cu,Au,Ni,Pd)(6)Sn-5 layer was governed by the dissolution of the (Au,Pd)Sn-4 IMC that occurred during solid-state aging. The complete dissolution of (Au,Pd)Sn-4 resulted in a reactant-limited chemical reaction from the conversion of (Au,Pd)Sn-4 to (Cu,Au,Ni,Pd)(6)Sn-5. The development of the interfacial bilayer IMCs in the solder joint incorporating Au/Pd metallization suppressed excessive IMC growth and unfavorable phase transformation during long-term solid-state aging. The detailed mechanism of the formation of the interfacial bilayer Cu6Sn5-based IMCs was investigated in this paper.
引用
收藏
页码:15233 / 15240
页数:8
相关论文
共 33 条
  • [21] Interfacial IMC Growth and Nanomechanical Characterizations of Solder in Sn-16Sb/Cu Joints during Solid-state Aging
    Bi Xiaoyang
    Hu Xiaowu
    Li Yulong
    Jiang Xiongxin
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2019, 34 (05): : 1210 - 1219
  • [22] Formation mechanism and kinetic analysis of the morphology of Cu6Sn5 in the spherical solder joints at the Sn/Cu liquid-solid interface during soldering cooling stage
    Guo, Bingfeng
    Ma, Haitao
    Jiang, Chengrong
    Wang, Yunpeng
    Kunwar, Anil
    Zhao, Ning
    Huang, Mingliang
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2017, 28 (07) : 5398 - 5406
  • [23] In situ quantitative study of microstructural evolution at the interface of Sn3.0Ag0.5Cu/Cu solder joint during solid state aging
    Li, Hailong
    An, Rong
    Wang, Chunqing
    Jiang, Zhi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 634 : 94 - 98
  • [24] The interfacial reaction between In-48Sn solder and polycrystalline Cu substrate during solid state aging
    Tian, Feifei
    Li, Cai-Fu
    Zhou, Ming
    Liu, Zhi-Quan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 740 : 500 - 509
  • [25] Alteration of Cu3Sn growth and retention of multi-orientation Cu6Sn5 during thermal aging in Cu-xNi-yZn/Sn3.5Ag/Cu transient liquid-phase bonding
    Wu, Zih-You
    Lee, Yin-Ku
    Tsai, Su-Yueh
    Chen, Po-Yu
    Duh, Jenq-Gong
    MATERIALS CHARACTERIZATION, 2024, 207
  • [26] Suppressing the growth of interfacial Cu-Sn intermetallic compounds in the Sn-3.0Ag-0.5Cu-0.1Ni/Cu-15Zn solder joint during thermal aging
    Chen, Wei-Yu
    Yu, Chi-Yang
    Duh, Jenq-Gong
    JOURNAL OF MATERIALS SCIENCE, 2012, 47 (09) : 4012 - 4018
  • [27] Kinetic study of solid-state interfacial reactions of p-type (Bi, Sb)2Te3 thermoelectric materials with Sn and Sn-Ag-Cu solders
    Wang, Chao-hong
    Li, Mei-hau
    Chiu, Chun-wei
    Chang, Tai-yu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 767 : 1133 - 1140
  • [28] Interfacial reactions of BGA Sn-3.5%Ag-0.5%Cu and Sn-3.5%Ag solders during high-temperature aging with Ni/Au metallization
    Sharif, A
    Islam, MN
    Chan, YC
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2004, 113 (03): : 184 - 189
  • [29] Growth kinetics of IMC formed between Sn-3.5Ag-0.75Cu BGA solder and electroless Ni-P/Cu substrate by solid-state isothermal aging
    Yoon, JW
    Lee, CB
    Jung, SB
    DESIGNING, PROCESSING AND PROPERTIES OF ADVANCED ENGINEERING MATERIALS, PTS 1 AND 2, 2004, 449-4 : 893 - 896
  • [30] Solid-state interfacial reactions between Sn-3.5Ag-0.7Cu solder and electroless Ni-immersion Au substrate during high temperature storage test
    Chun, Hyun-Suk
    Yoon, Jeong-Won
    Jung, Seung-Boo
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 439 (1-2) : 91 - 96