Physical Investigations on (MoO3)x-(WO3)1-x Composite Thin Films

被引:1
作者
Srinivasarao, K. [1 ]
Prameela, Ch [2 ]
机构
[1] Sasi Inst Technol & Engn, Dept Appl Sci & Humanities, Tadepalligudem 534101, Andhra Pradesh, India
[2] Chalapathy Inst Technol, Dept Sci & Humanities, Guntur 522016, Andhra Pradesh, India
关键词
Composite Thin Films; Characterization; Flash Evaporation; Photochromism; OPTICAL-PROPERTIES; PHOTOCHROMIC PROPERTIES; MOLYBDENUM; MOO3; WO3; DEPOSITION; GROWTH;
D O I
10.18311/jsst/2019/18461
中图分类号
O59 [应用物理学];
学科分类号
摘要
Thin films of (MoO3)(x)-(WO3)(1-x) (x = 0.4, 0.6, 0.8) were deposited on glass and silicon (100) substrates by flash evaporation technique. The purpose of the flash evaporation is to prevent the decomposition of composite into individual species during thin film deposition. The films were deposited at the oxygen partial pressures of 2x10(-5), 2x10(-4) mbar and substrate temperatures of 150 degrees C, 350 degrees C. The deposited films were characterized for their structure by Graging Incidence X-ray Diffraction (GIXRD), microstructure by Field Emission Scanning Electron Microscopy (FESEM), optical property by UV-Vis spectra. The X-ray diffraction reveals that the (MoO3)(x) - (WO3)(1-x) composite thin film crystallizes in orthorhombic and monoclinic phases. At lower oxygen partial pressures of 2x10(-5) mbar and lower substrate temperatures of 150 degrees C the film crystallizes in orthorhombic and tetragonal phases. Whereas at higher substrate temperatures of 350 degrees C both orthorhombic and monoclinic mixed phases are present. The optical transmittance spectra of the films were recorded in the wavelength range 300-1100 nm. The optical energy gap of the films is 3.05 eV and increases to 3.21 eV with increase in MoO3 concentration. The width of localized states is 0.47 eV and decreasing with increasing MoO3 concentration. The oxide materials in thin film form exhibit the change in the transmittance when exposed to electro magnetic waves (EM) of visible region. In this respect the estimation of color centre concentration will give the information regarding the response of the films to change their transmittance when exposed to EM waves in the visible region. The colourcenter concentration of the films (for x = 0.4) deposited at 150 degrees C and irradiation time of 120 minutes, is 3.02 x 10(17)/cm(3) and reaches to maximum value of 4.94 x 10(17)/cm(3), (for x = 0.8) when deposited at 350 degrees C and irradiated for 150 minutes.
引用
收藏
页码:26 / 35
页数:10
相关论文
共 32 条
[31]  
Urbach F., 1996, PHYS REV, V92, P627
[32]   PHOTOCHROMIC CHARACTERISTICS OF MIXED WO3-MOO3 THIN-FILMS IN ALCOHOL VAPORS [J].
YAO, JN ;
LOO, BH ;
HASHIMOTO, K ;
FUJISHIMA, A .
BERICHTE DER BUNSEN-GESELLSCHAFT-PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 1991, 95 (05) :554-556