Effect of Annealing Temperature on Structural and Magnetic Properties of Zn0.94Co0.05Cu0.01O

被引:30
作者
Heiba, Z. K. [1 ,2 ]
Arda, L. [3 ]
Mohamed, Mohamed Bakr [2 ]
Mostafa, Nasser Y. [1 ]
Dogan, N. [4 ]
机构
[1] Taif Univ, Fac Sci, Al Haweiah, Taif, Saudi Arabia
[2] Ain Shams Univ, Fac Sci, Dept Phys, Cairo, Egypt
[3] Bahcesehir Univ, Fac Arts & Sci, TR-34100 Istanbul, Turkey
[4] Gebze Inst Technol, Dept Phys, TR-41400 Gebze, Kocaeli, Turkey
关键词
Nanostructures; Magnetic properties; Microstructure; ZNO THIN-FILMS; FERROMAGNETIC PROPERTIES; SEMICONDUCTORS; SPINTRONICS; ZN1-XCOXO; NI;
D O I
10.1007/s10948-013-2197-1
中图分类号
O59 [应用物理学];
学科分类号
摘要
The doped ZnO system Zn0.94Co0.05Cu0.01O (ZCCO) was prepared as a nano-polycrystalline by a simple sol-gel process, then air annealed at different temperatures. Applying X-ray diffraction (XRD) and the Rietveld method, structural analysis showed that Co and Cu replace Zn substitutionally yielding ZCCO single phase. The refined u-fractional coordinate of Zn increases monotonically by an annealing temperature from 0.3546 at 500 A degrees C reaching 0.3722 at 800 A degrees C, very near from the ideal value 0.375. The Zn tetrahedrons become more symmetric and the distortion is gradually relieved by annealing up to 800 A degrees C. Annealing at 900 A degrees C introduces tetrahedron distortion in an opposite way. The zero field cooled (ZFC) and field cooled (FC) magnetization versus the temperature at different applied fields and the magnetization versus the applied field at different temperatures were carried out. The system exhibits a ferromagnetic behavior at room temperature. As the annealing temperature increases from 550 to 900 A degrees C, the saturation magnetization at 300 K increases from 0.0507 to 0.1088 emu/g.
引用
收藏
页码:3487 / 3493
页数:7
相关论文
共 39 条
[1]   REMEASUREMENT OF STRUCTURE OF HEXAGONAL ZNO [J].
ABRAHAMS, SC ;
BERNSTEIN, JL .
ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL CRYSTALLOGRAPHY AND CRYSTAL CHEMISTRY, 1969, B 25 :1233-+
[2]   Absence of ferromagnetism in Al-doped Zn0.9Co0.10O diluted magnetic semiconductors [J].
Alaria, J ;
Bieber, H ;
Colis, S ;
Schmerber, G ;
Dinia, A .
APPLIED PHYSICS LETTERS, 2006, 88 (11)
[3]   Enhancement of ferromagnetism upon thermal annealing in pure ZnO [J].
Banerjee, S. ;
Mandal, M. ;
Gayathri, N. ;
Sardar, M. .
APPLIED PHYSICS LETTERS, 2007, 91 (18)
[4]   Effects of rapid thermal annealing on the ferromagnetic properties of sputtered Zn1-x(Co0.5Fe0.5)xO thin films [J].
Cho, YM ;
Choo, WK ;
Kim, H ;
Kim, D ;
Ihm, Y .
APPLIED PHYSICS LETTERS, 2002, 80 (18) :3358-3360
[5]   Ferromagnetism in Cr-doped GaN: A first-principles calculation [J].
Das, GP ;
Rao, BK ;
Jena, P .
PHYSICAL REVIEW B, 2004, 69 (21) :214422-1
[6]  
Ghosh B., 2010, ARXIV10102381
[7]   XRD, XPS, optical, and Raman investigations of structural changes of nanoCo-doped ZnO [J].
Heiba, Z. K. ;
Arda, L. .
JOURNAL OF MOLECULAR STRUCTURE, 2012, 1022 :167-171
[8]   Evidence of oxygen vacancy enhanced room-temperature ferromagnetism in Co-doped ZnO [J].
Hsu, H. S. ;
Huang, J. C. A. ;
Huang, Y. H. ;
Liao, Y. F. ;
Lin, M. Z. ;
Lee, C. H. ;
Lee, J. F. ;
Chen, S. F. ;
Lai, L. Y. ;
Liu, C. P. .
APPLIED PHYSICS LETTERS, 2006, 88 (24)
[9]   Great influence of the oxygen vacancies on the ferromagnetism in the Co-doped ZnO films [J].
Huang, Bao ;
Zhu, Deliang ;
Ma, Xiaocui .
APPLIED SURFACE SCIENCE, 2007, 253 (16) :6892-6895
[10]   Experimental and theoretical investigations on magnetic behavior of (Al,Co) co-doped ZnO nanoparticles [J].
Jayakumar, O. D. ;
Achary, S. N. ;
Sudakar, C. ;
Naik, R. ;
Salunke, H. G. ;
Rao, Rekha ;
Peng, X. ;
Ahuja, R. ;
Tyagi, A. K. .
NANOSCALE, 2010, 2 (08) :1505-1511