Crazing Mechanism and Physical Aging of Poly(lactide) Toughened with Poly(ethylene oxide)-block-poly(butylene oxide) Diblock Copolymers

被引:48
作者
McCutcheon, Charles J. [1 ]
Zhao, Boran [1 ]
Jin, Kailong [1 ]
Bates, Frank S. [1 ]
Ellison, Christopher J. [1 ]
机构
[1] Univ Minnesota, Dept Chem Engn & Mat Sci, Minneapolis, MN 55455 USA
基金
美国国家科学基金会;
关键词
Ductility - Ethylene - Particle size - Tensile testing - Deformation - Polyethylene oxides - Polymer blends - Refractive index - X ray scattering - Thermoplastic elastomers - Stress analysis - Morphology;
D O I
10.1021/acs.macromol.0c01759
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Sustainable polymers are important alternatives to plastics and elastomers derived from petroleum resources. Poly(lactide) (PLA), a commercially available sustainable plastic, is a well-known success story. However, PLA lacks ductility and toughness, limiting the number of potential uses. In this study, small amounts of a liquid poly(ethylene oxide)-block-poly(butylene oxide) (PEO-PBO) diblock copolymer additive were blended with PLA to enhance its toughness and ductility. The incorporated PEO-PBO diblock copolymers generated a macrophase-separated morphology with particle diameters of 0.2-0.9 mu m, and nearly matched refractive indices of PLA and PEO-PBO led to retention of optical transparency. Addition of just 1.8 wt % PEO-PBO into PLA led to a 20-fold increase in toughness, measured as the area under the stress-strain data in tension without affecting the bulk elastic modulus of the plastic. The micromechanical deformation process of the PEO-PBO/PLA blend was investigated via in situ small angle X-ray scattering during tensile testing. The total volume of the crazed material was proportional to the total surface area of the dispersed PEO-PBO particles, and both quantities increased with increasing PEO-PBO loading. Increasing the PEO-PBO loading also resulted in (A) an increase in particle size, causing a decrease in the craze initiation stress, and (B) an increase in fibril spacing, indicating a lower craze propagation stress. Furthermore, craze development was found to be independent of aging time. As a result, the PEO-PBO/PLA blend was able to remain ductile and tough for up to 114 days, exhibiting a 10-fold increase in elongation at break and toughness compared to neat PLA, which becomes brittle in less than 2 days. These results demonstrate that designing additives that promote deformation by crazing is an effective way to overcome the aging-induced embrittlement of glassy polymers.
引用
收藏
页码:10163 / 10178
页数:16
相关论文
共 108 条
[81]  
Sheth M, 1997, J APPL POLYM SCI, V66, P1495, DOI 10.1002/(SICI)1097-4628(19971121)66:8<1495::AID-APP10>3.0.CO
[82]  
2-3
[83]   THE FRACTURE PROBABILITY OF HIGH-IMPACT POLYSTYRENE [J].
SJOERDSMA, SD ;
BOYENS, JPH .
POLYMER ENGINEERING AND SCIENCE, 1994, 34 (02) :86-92
[84]   Limiting law of the reinforcement of rubber [J].
Smallwood, HM .
JOURNAL OF APPLIED PHYSICS, 1944, 15 (11) :758-766
[85]  
Sternstein S.S., 1968, Applied Polymer Symposia, P175
[86]  
Sterstein S.S., 1969, AM CHENICAL SOC POLY, V10, P1117
[87]   In-situ SAXS study of the plastic deformation behavior of polylactide upon cold-drawing [J].
Stoclet, G. ;
Lefebvre, J. M. ;
Seguela, R. ;
Vanmansart, C. .
POLYMER, 2014, 55 (07) :1817-1828
[88]   PHYSICAL AGING IN PLASTICS AND OTHER GLASSY MATERIALS [J].
STRUIK, LCE .
POLYMER ENGINEERING AND SCIENCE, 1977, 17 (03) :165-173
[89]  
Tant M.R., 1999, Structure and Properties of Glassy Polymers, V710, P242
[90]  
Theryo G., 2014, Deformation and physical aging of rubber-modified polylactide graft copolymers