On the effect of a thermal treatment on the tensile and fatigue properties of weak zones of similar Ti17 linear friction welded joints and parent material

被引:20
|
作者
Garcia, J. M. [1 ]
Gaslain, F. [1 ]
Morgeneyer, T. F. [1 ]
机构
[1] PSL Res Univ, Ctr Mat, MINES ParisTech, CNRS,UMR 7633, BP 87, F-91003 Evry, France
关键词
Linear friction welding; Mechanical properties; Ti17; Ti-5Al-2Sn-2Zr-4Cr-4Mo; BETA-GRAIN-BOUNDARIES; TITANIUM-ALLOYS; MECHANICAL-PROPERTIES; TI-5AL-2SN-2ZR-4MO-4CR TI17; INITIAL MICROSTRUCTURE; RESIDUAL-STRESSES; ALPHA; BEHAVIOR; PRECIPITATION; DEFORMATION;
D O I
10.1016/j.matchar.2020.110570
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The tensile and fatigue properties and the damage mechanisms of as welded (LFW-AW) and post-weld heat treated (PWHT) similar Ti17 linear friction welded (LFW) joints as well as Ti17 parent material (PM) have been studied together with their underlying microstructures. The LFW-AW joints exhibited a depletion of the alpha phases in the weld centre zone (WCZ) and in the thermo-mechanically affected zone (TMAZ), which was previously qualified as a weak zone. Stereo Digital Image Correlation (SDIC) analysis of the strain field for monotonic loading of the PM showed strain heterogeneity that was linked by EBSD and Schmid's factor analysis to the large beta grains containing alpha precipitates. Compared to the PM tensile specimens, the LFW-AW joint highlighted lower ultimate tensile strength (UTS) and a strongly reduced and scattered macroscopic ductility. Maps and spatio-temporal graphs of normalized strain rate fields obtained by SDIC clearly highlighted localization at the weak zone. For the target fatigue life of 10(5) cycles, the fatigue strength of the AW joint was about half that of the PM with fatigue crack initiation at the beta grain boundary in the weak zones. Remarkably, the PWHT made the AW joints comparable to the PM in terms of microstructure and mechanical properties. The former weak zones recrystallized into beta grains with alpha, the UTS and fatigue strength were almost recovered, macroscopic and local ductility were enhanced, failure during monotonic and cyclic loadings occurred far from the former weak zones.
引用
收藏
页数:18
相关论文
共 31 条
  • [21] Effect of ultrasonic vibration on thermal and material flow behavior, microstructure and mechanical properties of friction stir welded Al/Cu joints
    Weihong Tian
    Hao Su
    Chuansong Wu
    The International Journal of Advanced Manufacturing Technology, 2020, 107 : 59 - 71
  • [22] Analysis of residual stress relief in linear friction welded Ti17 during post weld heat treatment by Norton-Bailey creep model
    He, Peng
    Wu, Yunxin
    Zhang, Tao
    Jin, Junlong
    WELDING IN THE WORLD, 2025, 69 (02) : 515 - 529
  • [23] Effect of solution treatment temperature on the ?? precipitation distribution, high temperature tensile and fatigue properties of FGH96 joints prepared by inertia friction welding
    Yang, Jun
    Li, Jinglong
    Xiong, Jiangtao
    Yan, Wenwei
    Jin, Feng
    MATERIALS RESEARCH EXPRESS, 2019, 6 (11)
  • [24] Strain-controlled fatigue properties of linear friction welded dissimilar joints between Ti-6Al-4V and Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloys
    Wen, G. D.
    Ma, T. J.
    Li, W. Y.
    Wang, S. Q.
    Guo, H. Z.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 612 : 80 - 88
  • [25] Investigation on the Effect of Friction Time on Microstructural Characteristics and Mechanical Properties of Linear Friction Welded Ti-6Al-4V Alloy Joints
    C. Mukundhan
    P. Sivaraj
    Vijay Petlay
    Shweta Verma
    V. Balasubramanian
    Journal of Materials Engineering and Performance, 2022, 31 : 5611 - 5621
  • [26] Investigation on the Effect of Friction Time on Microstructural Characteristics and Mechanical Properties of Linear Friction Welded Ti-6Al-4V Alloy Joints
    Mukundhan, C.
    Sivaraj, P.
    Petlay, Vijay
    Verma, Shweta
    Balasubramanian, V
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (07) : 5611 - 5621
  • [27] Effect of heat treatment temperatures on microstructure and mechanical property of linear friction welded joints of titanium alloys TC17 (α+ β)/TC17 (β)
    Li Xiao-hong
    Zhang Yan-hua
    Li Zan
    Li Ju
    Zhang Tian-cang
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2020, 48 (01): : 115 - 120
  • [28] Effect of Post Weld Heat Treatment on Microstructure and Properties of Linear Friction Welded Joints for Hyperoxic TC4/TC17 Dissimilar Titanium Alloys
    Chang C.
    Li J.
    Zhang T.
    Guo D.
    Cailiao Daobao/Materials Reports, 2021, 35 (10): : 10109 - 10113
  • [29] Microstructural response at the interface and its effect on the fatigue fracture behavior of rotary friction welded dissimilar titanium alloys: Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) and Ti-6Al-2Sn-4Zr-2Mo (Ti6242)
    Wang, Binwen
    Chen, Xianmin
    Yang, Jun
    Jin, Feng
    Wang, Qian
    MATERIALS RESEARCH EXPRESS, 2021, 8 (10)
  • [30] THE EFFECT OF THE HEAT TREATMENT CONDITION OF THE BASE MATERIAL ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 17-4PH STAINLESS STEEL ELECTRON BEAM WELDED JOINTS
    Nalborczyk-Kazanecka, A.
    Mrowka-Nowotnik, G.
    Pytel, A.
    ARCHIVES OF METALLURGY AND MATERIALS, 2023, 68 (04) : 1503 - 1512