On the effect of a thermal treatment on the tensile and fatigue properties of weak zones of similar Ti17 linear friction welded joints and parent material

被引:20
|
作者
Garcia, J. M. [1 ]
Gaslain, F. [1 ]
Morgeneyer, T. F. [1 ]
机构
[1] PSL Res Univ, Ctr Mat, MINES ParisTech, CNRS,UMR 7633, BP 87, F-91003 Evry, France
关键词
Linear friction welding; Mechanical properties; Ti17; Ti-5Al-2Sn-2Zr-4Cr-4Mo; BETA-GRAIN-BOUNDARIES; TITANIUM-ALLOYS; MECHANICAL-PROPERTIES; TI-5AL-2SN-2ZR-4MO-4CR TI17; INITIAL MICROSTRUCTURE; RESIDUAL-STRESSES; ALPHA; BEHAVIOR; PRECIPITATION; DEFORMATION;
D O I
10.1016/j.matchar.2020.110570
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The tensile and fatigue properties and the damage mechanisms of as welded (LFW-AW) and post-weld heat treated (PWHT) similar Ti17 linear friction welded (LFW) joints as well as Ti17 parent material (PM) have been studied together with their underlying microstructures. The LFW-AW joints exhibited a depletion of the alpha phases in the weld centre zone (WCZ) and in the thermo-mechanically affected zone (TMAZ), which was previously qualified as a weak zone. Stereo Digital Image Correlation (SDIC) analysis of the strain field for monotonic loading of the PM showed strain heterogeneity that was linked by EBSD and Schmid's factor analysis to the large beta grains containing alpha precipitates. Compared to the PM tensile specimens, the LFW-AW joint highlighted lower ultimate tensile strength (UTS) and a strongly reduced and scattered macroscopic ductility. Maps and spatio-temporal graphs of normalized strain rate fields obtained by SDIC clearly highlighted localization at the weak zone. For the target fatigue life of 10(5) cycles, the fatigue strength of the AW joint was about half that of the PM with fatigue crack initiation at the beta grain boundary in the weak zones. Remarkably, the PWHT made the AW joints comparable to the PM in terms of microstructure and mechanical properties. The former weak zones recrystallized into beta grains with alpha, the UTS and fatigue strength were almost recovered, macroscopic and local ductility were enhanced, failure during monotonic and cyclic loadings occurred far from the former weak zones.
引用
收藏
页数:18
相关论文
共 31 条
  • [1] Comprehensive investigation on linear friction welding a dissimilar material joint between Ti17(α+β) and Ti17(β): Microstructure evolution, failure mechanisms, with simultaneous optimization of tensile and fatigue properties
    Guo, Zhenguo
    Ma, Tiejun
    Yang, Xiawei
    Li, Wenya
    Xu, Qiaozhi
    Li, Yixue
    Li, Ju
    Vairis, Achilles
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 909
  • [2] Linear friction welding of equiaxed Ti17 titanium alloy: Effects of microstructure evolution on tensile and impact properties
    Guo, Zhenguo
    Ma, Tiejun
    Chen, Tao
    Wang, Jiantao
    Chen, Xi
    Yang, Xiawei
    Tao, Jun
    Li, Ju
    Li, Wenya
    Vairis, Achilles
    JOURNAL OF MATERIALS SCIENCE, 2023, 58 (24) : 10189 - 10200
  • [3] Microstructure characteristics and strain hardening behaviour of Ti17 linear friction welded joints
    He, Peng
    Wu, Yunxin
    Zhang, Tao
    Wu, Zhijie
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2023, 28 (09) : 955 - 963
  • [4] Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint
    Ma, T. J.
    Li, W. Y.
    Zhong, B.
    Zhang, Y.
    Li, J. L.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2012, 17 (03) : 180 - 185
  • [5] Fatigue fracture behavior of a Ti17 joint under various heat treatment specifications prepared by linear friction welding
    Liu, Jiatao
    Li, Jinglong
    Li, Xiaoguang
    Jin, Feng
    Du, Yajie
    Shi, Junmiao
    Guo, Wei
    Xiong, Jiangtao
    MATERIALS CHARACTERIZATION, 2023, 205
  • [6] Strength, fatigue strength and toughness of dissimilar Ti17-Ti64 linear friction welded joints: Effect of soft surface contamination and depletion of α precipitates
    Garcia, J. M.
    Esin, V. A.
    Morgeneyer, T. F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 799
  • [7] Strain-controlled fatigue properties of dissimilar welded joints between Ti-6Al-4V and Ti17 alloys
    Wang, S. Q.
    Liu, J. H.
    Chen, D. L.
    MATERIALS & DESIGN, 2013, 49 : 716 - 727
  • [8] Residual stress prediction in Ti17 linear friction welds considering inhomogeneous mechanical properties of joints
    He, Peng
    Wu, Yun-Xin
    Zhang, Tao
    Jin, Jun-Long
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2024, 29 (7-8) : 405 - 415
  • [9] Study of Rotating-Bending Fatigue Properties and Strengthening Mechanism of Laser Shock Peening on Ti17 Welded Joints
    Chi, Jiaxuan
    He, Dongsheng
    Zhang, Yongxin
    Zhang, Hepeng
    Qu, Shen
    Zhang, Gongxuan
    Xu, Yanqiang
    Han, Guofeng
    Zhang, Hongqiang
    Guo, Wei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [10] Effect of friction pressure on microstructure and tensile properties of linear friction welded Ti–6Al–4V alloy joints
    Mukundhan C.
    Sivaraj P.
    Balasubramanian V.
    Sonar T.
    Petley V.
    Verma S.
    International Journal of Lightweight Materials and Manufacture, 2023, 6 (04) : 483 - 493