Evolution and investigation of copper and gold ball bonds in extended reliability stressing

被引:20
作者
Gan, C. L. [1 ,2 ]
Classe, F. C. [1 ]
Chan, B. L. [1 ]
Hashim, U. [2 ]
机构
[1] Spans Penang Sdn Bhd, George Town 11900, Bayan Lepas, Malaysia
[2] Univ Malaysia Perlis, Inst Nanoelect Engn INEE, Perlis 01000, Kangar, Malaysia
来源
GOLD BULLETIN | 2014年 / 47卷 / 03期
关键词
Microstructure evolution; Copper and gold ball bonds; Failure mechanisms; SEM; EDX analysis; Extended reliability; Weibull plot; WIRE-BONDS; CU; INTERMETALLICS; MECHANISM;
D O I
10.1007/s13404-014-0135-z
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
This paper discusses the microstructure evolution of copper (Cu) and gold (Au) ball bonds after various extended reliability stresses such as biased highly accelerated temperature and humidity test (HAST), unbiased highly accelerated temperature and humidity test (UHAST), temperature cycling (TC), and high temperature storage life (HTSL) in BGA package. Objective of this study is to study the microstructure evolution and changes after long hours and long cycles of component reliability stressing and its predicted failure mechanisms and to determine the long-term reliability comparison with combination of bonding wires in HAST, UHAST, and TC. Secondary electron microscopy (SEM) and energy dispersive X-ray (EDX) have been carried out to understand the respective microstructure of failed samples in HAST, UHAST, TC, and HTSL long-term reliability failures. Respective failure mechanisms of copper and gold ball bonds carrion under HAST and UHAST, ball bond lifting in TC and HTSL have been analyzed and proposed. The evolution of surface morphology, including copper and gold ball bond micro cracking, gold ball bond Kirkendall microvoiding and intermetallic compound (IMC) formation, was studied in FBGA package with copper and gold ball bonds during various reliability stresses. Biased HAST, UHAST, TC, and HTSL mechanisms were proposed to explain the observed morphological changes and the resulting ball bond wear out modes after extended reliability stresses. Weibull reliability analyses have been established to compare the performance of copper and gold ball bonds under humid and dry environmental tests.
引用
收藏
页码:141 / 151
页数:11
相关论文
共 34 条
[1]  
[Anonymous], 2008, 020 JEDEC IPC STD
[2]  
[Anonymous], PLOS ONE
[3]   Fine pitch copper wire bonding in high volume production [J].
Appelt, Bernd K. ;
Tseng, Andy ;
Chen, Chun-Hsiung ;
Lai, Yi-Shao .
MICROELECTRONICS RELIABILITY, 2011, 51 (01) :13-20
[4]   What is the future of bonding wire? Will copper entirely replace gold? [J].
Breach, C. D. .
GOLD BULLETIN, 2010, 43 (03) :150-168
[5]  
Chauhan P., 2014, COPPER WIRE BONDING
[6]   Copper Wire Bonding Concerns and Best Practices [J].
Chauhan, Preeti ;
Zhong, Z. W. ;
Pecht, Michael .
JOURNAL OF ELECTRONIC MATERIALS, 2013, 42 (08) :2415-2434
[7]   Detailed investigation of ultrasonic Al-Cu wire-bonds: II. Microstructural evolution during annealing [J].
Drozdov, M. ;
Gur, G. ;
Atzmon, Z. ;
Kaplan, W. D. .
JOURNAL OF MATERIALS SCIENCE, 2008, 43 (18) :6038-6048
[8]   Detailed investigation of ultrasonic Al-Cu wire-bonds: I. Intermetallic formation in the as-bonded state [J].
Drozdov, M. ;
Gur, G. ;
Atzmon, Z. ;
Kaplan, Wayne D. .
JOURNAL OF MATERIALS SCIENCE, 2008, 43 (18) :6029-6037
[9]   Reliability Assessment and Activation Energy Study of Au and Pd-Coated Cu Wires Post High Temperature Aging in Nanoscale Semiconductor Packaging [J].
Gan, C. L. ;
Hashim, U. .
JOURNAL OF ELECTRONIC PACKAGING, 2013, 135 (02)
[10]   Reliability assessment and mechanical characterization of Cu and Au ball bonds in BGA package [J].
Gan, C. L. ;
Hashim, U. .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2013, 24 (08) :2803-2811