Improving room-temperature stretch formability of a high-alloyed Mg-Al-Ca-Mn alloy sheet by a high-temperature solution-treatment

被引:28
作者
Nakata, T. [1 ]
Xu, C. [2 ]
Yoshida, Y. [3 ]
Yoshida, K. [3 ]
Kamado, S. [1 ]
机构
[1] Nagaoka Univ Technol, 1603-1 Kamitomioka, Nagaoka, Niigata 9402188, Japan
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[3] Sumitomo Elect Ind Ltd, 1-1-1 Koyakita, Itami, Hyogo 6640016, Japan
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2021年 / 801卷
关键词
Mg-Al-Ca-Mn alloy; Rolling; Formability; Tensile property; Microstructure; Texture; MECHANICAL-PROPERTIES; MAGNESIUM ALLOY; GRAIN-SIZE; TENSILE PROPERTIES; DEFORMATION-BEHAVIOR; TEXTURE EVOLUTION; ZN; MICROSTRUCTURE; FRACTURE; ANISOTROPY;
D O I
10.1016/j.msea.2020.140399
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Various solution-treatments were applied on a rapidly solidified and subsequently rolled Mg-7.50Al-1.07Ca0.17Mn (mass%) alloy sheet, and a room-temperature stretch formability, tensile properties, microstructures, and textures of the solution-treated sheets have been investigated. Although the solution-treatment at 400 ?C gives high strengths, the sheet shows poor room-temperature stretch formability with the Index Erichsen value of 4.8 mm due to densely dispersed second phase particles. Also, the particles tend to distribute to the rolling direction, leading to limited elongation to failure of 11.0% along the transverse direction. The solution-treatment at higher temperature leads to the sparse and relatively uniform dispersion of the particles. This results in the significant improvement in the room-temperature stretch formability and ductility. The Index Erichsen increases to 6.8 mm by the solution-treatment at 450 degrees C for 4 h, and the sheet shows large elongation to failure of 19.1% and 17.1% along the rolling and transverse directions, respectively. The sheet also exhibits high strengths and in plane isotropic properties, tensile strength over 320 MPa and 0.2% proof stress of similar to 180 MPa could be obtained due to fine grain structure with the average grain size of 9.5 mu m.
引用
收藏
页数:7
相关论文
共 50 条
  • [31] Microstructure and Properties of Mg-Al-Ca-Mn Alloy with High Ca/Al Ratio Fabricated by Hot Extrusion
    Chu, Aimin
    Zhao, Yuping
    Ud-din, Rafi
    Hu, Hairong
    Zhi, Qian
    Wang, Zerui
    [J]. MATERIALS, 2021, 14 (18)
  • [32] Improving room-temperature ductility of a Mg-Zn-Ca alloy through friction stir processing
    Wang, H.
    Zhang, D. T.
    Cao, G. H.
    Qiu, C.
    [J]. JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 17 : 1176 - 1186
  • [33] Designing a low-alloyed Mg-Al-Sn-Ca alloy with high strength and extraordinary formability by regulating fine grains and unique texture
    Li, Zhi-Gang
    Miao, Yuan
    Jia, Hai-Long
    Zheng, Rui
    Wang, Ming-Hui
    Wang, Hui-Yuan
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 852
  • [34] A micro-alloyed Mg-Sn-Y alloy with high ductility at room temperature
    Wang, Qinghang
    Shen, Yaqun
    Jiang, Bin
    Tangb, Aitao
    Song, Jiangfeng
    Jiang, Zhongtao
    Yang, Tianhao
    Huang, Guangsheng
    Pan, Fusheng
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 735 : 131 - 144
  • [35] High-speed extrusion of heat-treatable Mg-Al-Ca-Mn dilute alloy
    Nakata, T.
    Mezaki, T.
    Ajima, R.
    Xu, C.
    Oh-ishi, K.
    Shimizu, K.
    Hanaki, S.
    Sasaki, T. T.
    Hono, K.
    Kamado, S.
    [J]. SCRIPTA MATERIALIA, 2015, 101 : 28 - 31
  • [36] Great room temperature stretch formability of fine-grained Mg-Mn alloy
    Somekawa, Hidetoshi
    Kinoshita, Akihito
    Kato, Akira
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 697 : 217 - 223
  • [37] Enhanced stretch formability of Mg-Al-Zn alloy sheets rolled at high temperature (723 K)
    Chino, Yasumasa
    Mabuchi, Mamoru
    [J]. SCRIPTA MATERIALIA, 2009, 60 (06) : 447 - 450
  • [38] Effect of pre-strain levels and high temperature annealing on the formability of AZ31 Mg alloy thin sheet during stretch deformation
    Wang, Lifei
    Zhang, Zhengyong
    Cao, Miao
    Zhang, Hua
    Han, Tingzhuang
    Yang, Qingshan
    Wang, Hongxia
    Cheng, Weili
    [J]. MATERIALS RESEARCH EXPRESS, 2019, 6 (08):
  • [39] Alloy Design for the Development of Heat Treatable High Strength Mg Sheet Alloy with Excellent Room Temperature Formability
    Suh, B-C
    Bian, M-Z
    Nakata, T.
    Sasaki, T. T.
    Kamado, S.
    Hono, K.
    [J]. MAGNESIUM TECHNOLOGY 2018, 2018, : 373 - 377
  • [40] Simultaneously achieving excellent mechanical properties and high thermal conductivity in a high Mn-containing Mg-Zn-Ca-Al-Mn sheet alloy
    Huang, Xinsheng
    Bian, Mingzhe
    Nakatsugawa, Isao
    Chino, Yasumasa
    Sato, Masahiko
    Yamazaki, Kazumasa
    Kido, Futoshi
    Ueda, Hironori
    Inoue, Masashi
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 887