Dry sliding up to 7.5 m/s and 800 °C of thermally sprayed coatings of the TiO2-Cr2O3 system and (Ti,Mo)(C,N)-Ni(Co)

被引:49
作者
Berger, L. -M. [2 ]
Stahr, C. C. [2 ]
Saaro, S. [2 ]
Thiele, S. [3 ]
Woydt, M. [1 ]
Kelling, N. [1 ]
机构
[1] BAM, Fed Inst Mat Res & Testing, Berlin, Germany
[2] Fh IWS, Fraunhofer Inst Mat & Beam Technol, Dresden, Germany
[3] Fh IKTS, Fraunhofer Inst Ceram Technol & Syst, Dresden, Germany
关键词
Dry sliding; High-temperature; Magneli-phase; TiO2; Cr2O3; Coating; TRIBOLOGICAL PROPERTIES; TITANIUM; OXIDES;
D O I
10.1016/j.wear.2008.12.105
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Since the term 'lubricious oxides' was introduced to tribology in order to describe expected low coefficients of friction (COF) and high wear resistances in unlubricated (dry) sliding conditions numerous studies have been carried out on bulk materials and thermal spray coatings of the Ti-O system. Recently, studies were performed on the binary TiO2-Cr2O3 system, as well as with (Ti,Mo)(C,N)-NiMo cermets or TiC-based thermally sprayed hardmetal coatings, which might form beneficial titanium suboxides as a result of tribo-oxidative and/or high-temperature reactions. in this paper, we shortly summarize the characteristics and dry sliding wear resistance of thermally sprayed oxide coatings of the Ti-O and TiO2-Cr2O3 lsystems, as well as of (Ti,Mo)(C,N)-Ni(Co) hardmetat coatings. The prediction of solid lubrication properties of titanium suboxides was inspired from the planar oxygen defects present in the Magneli-phases of titania, e.g., so-called crystallographic shear planes. While such structures with some limitations can be realised in coatings, the significant disadvantage is that TiOx tends to re-oxidize in air above similar to 380 degrees C. The iso-structural phases in the TiO2-Cr2O3 phase diagram can be prepared in air and have stable oxygen content. However, as can be concluded from the phase diagram, during thermal spraying phase transformations occur as well. In this paper, the wear resistance of alumina dry sliding against APS-sprayed coatings of three compositions in the TiO2-Cr2O3 systems (compositions 75Cr(2)O(3)/25TiO(2), 27Cr(2)O(3)/73TiO(2) and 23.5Cr(2)O(3)/76.5TiO(2)) is studied from room temperature up to 800 degrees C and sliding speeds in the range of 0.1-7.5 m/s. The results are compared with those of a chromia and a titania suboxide coatings, as well as with (Ti,Mo)(C,N)-Ni(Co) coatings and bulk (Ti,Mo)(C,N)-NiMo cermets as self-mated couples. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:954 / 964
页数:11
相关论文
共 44 条
[1]  
ANDERSSON S, 1964, ARK KEMI, V21, P413
[2]   IDENTIFICATION OF TITANIUM OXIDES BY X-RAY POWDER PATTERNS [J].
ANDERSSON, S ;
COLLEN, B ;
KRUUSE, G ;
KUYLENSTIERNA, U ;
MAGNELI, A ;
PESTMALIS, H ;
ASBRINK, S .
ACTA CHEMICA SCANDINAVICA, 1957, 11 (10) :1653-1657
[3]   PHASE ANALYSIS STUDIES ON THE TITANIUM-OXYGEN SYSTEM [J].
ANDERSSON, S ;
COLLEN, B ;
KUYLENSTIERNA, U ;
MAGNELI, A .
ACTA CHEMICA SCANDINAVICA, 1957, 11 (10) :1641-1652
[4]   A HOMOLOGOUS SERIES OF MIXED TITANIUM CHROMIUM OXIDES TIN-2CR2O2N-1 ISOMORPHOUS WITH THE SERIES TINO2N-1 AND VNO2N-1 [J].
ANDERSSON, S ;
SUNDHOLM, A ;
MAGNELI, A .
ACTA CHEMICA SCANDINAVICA, 1959, 13 (05) :989-997
[5]  
*ASM, 1992, ASM HDB FRICT LUBR W, V18
[6]  
Berezhnoi A. S., 1968, DOPOVIDI AN UKRAIN B, V3, P250
[7]  
Berger L.-M., 2007, JB OBERFLACHENTECHNI, V63, P242
[8]  
Berger LM, 2004, THERMAL SPRAY 2004: ADVANCES IN TECHNOLOGY AND APPLICATION, PROCEEDINGS, P934
[9]  
Berger LM, 2001, THERMAL SPRAY 2001: NEW SURFACES FOR A NEW MILLENNIUM, P291
[10]  
BERGER LM, THERMAL SPR IN PRESS, V2