Chloride binding in sound and carbonated cementitious materials with various types of binder

被引:99
作者
Saillio, Mickael [1 ,2 ]
Baroghel-Bouny, Veronique [1 ]
Barberon, Fabien [2 ]
机构
[1] Paris Est Univ, IFSTTAR, Mat & Struct Dept, F-77447 Marne La Vallee, France
[2] Bouygues Travaux Publ, PIM, F-78114 Magny Les Hameaux, France
关键词
Concrete; Carbonation; Si-29 and Al-27 NMR spectroscopy; Chloride binding; SCM; AL-27 MAS NMR; CONCRETE; CEMENTS; PHASES;
D O I
10.1016/j.conbuildmat.2014.05.049
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Carbonation and chloride ingress are the main causes of reinforced concrete structures degradation. Usually, these two phenomena are studied individually. Here, chloride ingress has been investigated on sound and carbonated cementitious materials (cement pastes and concrete). The supplementary cementitious materials (SCM) are fly ash, slag and metakaolin. The materials were carbonated by exposure to accelerated conditions (1.5% CO2 and 65% RH) in laboratory. Chloride binding isotherms of sound and carbonated samples were assessed by the equilibrium method (exposure to various alkaline NaCl solutions). The microstructure was characterized not only by usual techniques such as XRD and TGA-DTA, but also by Si-29 and Al-22 NMR spectroscopy. The results show that carbonated samples bind less chlorides than sound ones. The use of a combination of various techniques of microstructural characterization reduces the number of the possible explanations of these findings. In carbonated materials, both the quantity of Friedel's salts and of chlorides bound by C-S-H decrease. The first decrease can be explained by a lack of portlandite and modification of aluminate phases equilibrium. The second decrease seems to be due to a modification of the C-S-H (change of surface charge) during the carbonation process. Moreover, differences according to the nature and the amount of supplementary cementitious materials (SCM) were observed. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:82 / 91
页数:10
相关论文
共 34 条
  • [1] A new aluminium-hydrate species in hydrated Portland cements characterized by 27Al and 29Si MAS NMR spectroscopy
    Andersen, MD
    Jakobsen, HJ
    Skibsted, J
    [J]. CEMENT AND CONCRETE RESEARCH, 2006, 36 (01) : 3 - 17
  • [2] [Anonymous], 2002, RFGC
  • [3] Arliguie G, 2007, GRANDUBE MEASURES AS
  • [4] Arya C., 1990, Cement Concr. Res., V20, P290
  • [5] Impact of chloride on the mineralogy of hydrated Portland cement systems
    Balonis, Magdalena
    Lothenbach, Barbara
    Le Saout, Gwenn
    Glasser, Fredrik P.
    [J]. CEMENT AND CONCRETE RESEARCH, 2010, 40 (07) : 1009 - 1022
  • [6] Formation and properties of C-S-H-PEG nano-structures
    Beaudoin, James J.
    Drame, Harouna
    Raki, Laila
    Alizadeh, Rouhollah
    [J]. MATERIALS AND STRUCTURES, 2009, 42 (07) : 1003 - 1014
  • [7] BEAUDOIN JJ, 1990, CEMENT CONCRETE RES, V20, P875, DOI 10.1016/0008-8846(90)90049-4
  • [8] Carbonation of CH and C-S-H in composite cement pastes containing high amounts of BFS
    Borges, Paulo H. R.
    Costa, Juliana O.
    Milestone, Neil B.
    Lynsdale, Cyril J.
    Streatfield, Roger E.
    [J]. CEMENT AND CONCRETE RESEARCH, 2010, 40 (02) : 284 - 292
  • [9] Durability properties of concrete containing 50% and 65% slag
    Bouikni, A.
    Swamy, R. N.
    Bali, A.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2009, 23 (08) : 2836 - 2845
  • [10] The system CaO-Al2O3-CaCl2-H2O at 23±2°C and the mechanisms of chloride binding in concrete
    Brown, P
    Bothe, J
    [J]. CEMENT AND CONCRETE RESEARCH, 2004, 34 (09) : 1549 - 1553