Thermal degradation mechanism and kinetics of polycarbonate/silica nanocomposites

被引:69
|
作者
Feng, Yuezhan [1 ]
Wang, Bo [1 ]
Wang, Fangfang [1 ]
Zhao, Yuanxu [1 ]
Liu, Chuntai [1 ]
Chen, Jingbo [1 ]
Shen, Changyu [1 ]
机构
[1] Zhengzhou Univ, Coll Mat Sci & Engn, Natl Engn Res Ctr Adv Polymer Proc Technol, Zhengzhou 450001, Peoples R China
基金
中国国家自然科学基金;
关键词
Polycarbonate; Silica; Nanocomposites; Thermal degradation; Kinetic analysis; A BIS(DIPHENYL PHOSPHATE); FLAME RETARDANCY; TITANIA NANOCOMPOSITES; SILICA; MORPHOLOGY; RUBBER/BISPHENOL; NANOPARTICLES; FLAMMABILITY; STABILITY; NANOTUBES;
D O I
10.1016/j.polymdegradstab.2014.05.012
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polycarbonate nanocomposites filled with pristine and modified silica were prepared by simple melt compounding. The thermal degradation behavior of composites was investigated by thermogravimetric analysis coupled with differential scanning calorimetry (TGA/DSC). To understand the thermal degradation mechanism, the chemical structures of gaseous and solid degradation products were detected by thermogravimetric analysis coupled with Fourier transform infrared spectrometry (TGA/FTIR) and X-ray photoelectron spectroscopy (XPS), respectively. Kissinger Akahira Sunose (KAS) and Flynn Wall Ozawa (FWO) methods were employed to analyze the thermal degradation kinetics. High thermal degradation temperature was obtained by incorporating both types of nanoparticles into matrix, but the maximum mass loss rate increased. According to the DSC curves for degradation process, the change of the number and position of absorption peaks meant that the degradation mechanism of composites was different from that of neat PC. The analysis for TGA chars confirmed the presence of alcoholysis reaction between PC and silica nanoparticles during the thermal decomposition. TGA/FTIR results proved that no new degradation volatiles were produced during the thermal degradation of composites, but the total amounts of all gaseous products decreased by adding silica nanoparticles. The degradation activation energies of both composites increased significantly relative to neat PC, especially for the composite with modified silica. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:129 / 138
页数:10
相关论文
共 50 条
  • [31] Flame retardancy of polycarbonate-polydimethylsiloxane block copolymer/silica nanocomposites
    Nodera, Akio
    Kanai, Toshitaka
    JOURNAL OF APPLIED POLYMER SCIENCE, 2006, 101 (06) : 3862 - 3868
  • [32] Degradation Kinetics of Polycarbonate in Supercritical Methanol
    Oh, Sea Cheon
    Shin, Hee-Yong
    Bae, Seong-Yeol
    JOURNAL OF CHEMICAL ENGINEERING OF JAPAN, 2009, 42 (09) : 700 - 704
  • [33] Thermal Degradation Kinetics of ZnO/polyester Nanocomposites
    Franco-Urquiza, E. A.
    May-Crespo, J. F.
    Escalante Velazquez, C. A.
    Perez Mora, R.
    Gonzalez Garcia, P.
    POLYMERS, 2020, 12 (08)
  • [34] Kinetics of the thermal degradation of polycarbonate films containing silver nanoparticles
    N. N. Volkova
    L. M. Bogdanova
    L. I. Kuzub
    N. N. Dremova
    Polymer Science Series B, 2015, 57 : 31 - 38
  • [35] Thermal degradation kinetics and lifetime estimation for polycarbonate/ polymethylphenylsilsesquioxane composite
    Wang J.
    Xin Z.
    Frontiers of Chemical Engineering in China, 2009, 3 (2): : 167 - 171
  • [36] Thermal degradation and flammability of nanocomposites composed of silica cross-linked to poly(methyl methacrylate)
    Hatanaka, L. C.
    Ahmed, L.
    Sachdeva, S.
    Wang, Q.
    Cheng, Z.
    Mannan, M. S.
    PLASTICS RUBBER AND COMPOSITES, 2016, 45 (09) : 375 - 381
  • [37] Non-isothermal degradation kinetics for polycarbonate/polymethylphenylsilsesquioxane composites
    Wang, Jiangbo
    Xin, Zhong
    E-POLYMERS, 2010,
  • [38] Effects of modified silica on morphology, mechanical property, and thermostability of injection-molded polycarbonate/silica nanocomposites
    Feng, Yuezhan
    Wang, Bo
    Wang, Fangfang
    Zheng, Guoqiang
    Dai, Kun
    Liu, Chuntai
    Chen, Jingbo
    Shen, Changyu
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2014, 33 (10) : 911 - 922
  • [39] Zero-order kinetics of the thermal degradation of polypropylene/clay nanocomposites
    Qin, HL
    Zhang, SM
    Zhao, CG
    Yang, MS
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2005, 43 (24) : 3713 - 3719
  • [40] Effect of Various Nanofillers on Thermal Stability and Degradation Kinetics of Polymer Nanocomposites
    Choudhury, Anusuya
    Bhowmick, Anil K.
    Ong, Christopher
    Soddemann, Matthias
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2010, 10 (08) : 5056 - 5071