Effect of ladle age on formation of nonmetallic inclusions in ladle treatment

被引:50
作者
Tripathi, NN
Nzotta, M
Sandberg, A
Sichen, D [1 ]
机构
[1] Royal Inst Technol, Div Met, Dept Mat Sci & Engn, SE-10044 Stockholm, Sweden
[2] Uddeholm Tooling AB, SE-68385 Hagfors, Sweden
关键词
steels; tool steels; ladle metallurgy; inclusions;
D O I
10.1179/030192304225011025
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
An experimental study was carried out at Uddeholm Tooling, Hagfors, Sweden to examine the impact of ladle glaze on the formation of non-metallic inclusions during the ladle treatment process. Steel samples were taken at various stages of the process and from ladles of different ages. Inclusion numbers were counted under an optical microscope. It was found that the total number of inclusions increased with the ladle age before deoxidation and at the end of the ladle treatment. The increase was substantial after the ladle had been used more than 18 times. Inclusions having the smallest sizes were found to make a large contribution to this increase. This observation was further confirmed by the difference between total oxygen content and dissolved oxygen content in the steel samples, which also showed an increase with ladle age. Analysis by SEM-EDX revealed two types of inclusions before casting, namely, inclusions consisting only of an oxide solution having a composition very close to 3CaO.Al2O3, and inclusions consisting of the same oxide solution as well as MgO phase. This finding was in accordance with the reported result that both 3CaO.Al2O3 and MgO were present in the slag infiltrated layer of the ladle glaze. It was concluded that ladle glaze is the foremost source of non-metallic inclusions in tool steel during ladle treatment.
引用
收藏
页码:235 / 240
页数:6
相关论文
共 30 条
[1]  
[Anonymous], 1995, Slag Atlas, V2nd
[2]   Chemical characteristics of inclusions formed at various stages during the ladle treatment of steel [J].
Beskow, K ;
Jia, J ;
Lupis, CHP ;
Du, SC .
IRONMAKING & STEELMAKING, 2002, 29 (06) :427-435
[3]   Study of the deoxidation of steel with aluminum wire injection in a gas-stirred ladle [J].
Beskow, K ;
Viswanathan, NN ;
Jonsson, L ;
Sichen, D .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2001, 32 (02) :319-328
[4]  
BESKOW K, UNPUB IRONMAKING STE
[5]   ON THE FORMATION OF NON-METALLIC INCLUSIONS IN FE-50 PCT NI TYPE ALLOYS BY DEOXIDATION WITH MN, SI, AND AL [J].
FREDRIKSSON, H ;
HAMMAR, O .
METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1980, 11 (03) :383-408
[6]  
Fuchs E, 2000, HIGH TEMP MATER PROC, V19, P333
[7]  
GORANSSON M, 2000, ISIJ INT S, V40, P1
[8]  
HANSEN T, 1997, P CLEAN STEEL 97 BAL, V2, P48
[9]  
HASSALL G, 1996, UNPUB
[10]   Modelling of ladle glaze interactions [J].
Hassall, GJ ;
Bain, KG ;
Jones, N ;
Warman, MO .
IRONMAKING & STEELMAKING, 2002, 29 (05) :383-389