Electrophoretic deposition of magnesium silicates on titanium implants: Ion migration and silicide interfaces

被引:20
作者
Afshar-Mohajer, M. [1 ]
Yaghoubi, A. [2 ]
Ramesh, S. [1 ]
Bushroa, A. R. [1 ]
Chin, K. M. C. [1 ]
Tin, C. C. [1 ]
Chiu, W. S. [3 ]
机构
[1] Univ Malaya, Fac Engn, Dept Mech Engn, Ctr Adv Mfg & Mat Proc, Kuala Lumpur 50603, Malaysia
[2] Univ Malaya, Ctr High Impact Res, Kuala Lumpur 50603, Malaysia
[3] Univ Malaya, Dept Phys, Low Dimens Mat Res Ctr, Kuala Lumpur 50603, Malaysia
关键词
Ceramic-metal interface; Bioactive coating; Forsterite; Magnesium oxide; Ion exchange decomposition; Diffusion; MICRO-ARC OXIDATION; HYDROXYAPATITE COATINGS; MECHANICAL-PROPERTIES; BIOMEDICAL APPLICATIONS; CRYSTAL-CHEMISTRY; LATTICE-DYNAMICS; FORSTERITE; OLIVINE; ALLOY; MICROSTRUCTURE;
D O I
10.1016/j.apsusc.2014.04.033
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Magnesium silicates (MgxSiOy) and in particular forsterite (Mg2SiO4) owing to their low thermal expansion mismatch with metals are promising materials for bioactive coating of implants. Here, we report the electrophoretic deposition (EPD) of forsterite onto titanium substrates using different precursors. Unlike bulk samples which achieve full stoichiometry only beyond 1400 degrees C, non-stoichiometric magnesium silicate rapidly decomposes into magnesium oxide nanowires during sintering. Elemental mapping and X-ray diffraction suggest that oxygen diffusion followed by ion exchange near the substrate leads to formation of an interfacial Ti5Si3 layer. Pre-annealed forsterite powder on the other hand shows a comparatively lower diffusion rate. Overall, magnesium silicate coatings do not exhibit thermally induced microcracks upon sintering as opposed to calcium phosphate bioceramics which are currently in use. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:1 / 6
页数:6
相关论文
共 54 条
  • [31] The in vitro degradation process and biocompatibility of a ZK60 magnesium alloy with a forsterite-containing micro-arc oxidation coating
    Lin, Xiao
    Tan, Lili
    Zhang, Qiang
    Yang, Ke
    Hu, Zhuangqi
    Qiu, Jianhong
    Cai, Yong
    [J]. ACTA BIOMATERIALIA, 2013, 9 (10) : 8631 - 8642
  • [32] Liu L., 1988, ELASTIC PROPERTIES E, P358
  • [34] Severe osteolysis after third-body wear due to hydroxyapatite particles from acetabular cup coating
    Morscher, EW
    Hefti, A
    Aebi, U
    [J]. JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 1998, 80B (02): : 267 - 272
  • [35] Calcium phosphate-based coatings on titanium and its alloys
    Narayanan, R.
    Seshadri, S. K.
    Kwon, T. Y.
    Kim, K. H.
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2008, 85B (01) : 279 - 299
  • [36] Preparation and characterization of forsterite (Mg2SiO4) bioceramics
    Ni, Siyu
    Chou, Lee
    Chang, Jiang
    [J]. CERAMICS INTERNATIONAL, 2007, 33 (01) : 83 - 88
  • [37] Effects of hydroxyapatite particulate debris on the production of cytokines and proteases in human fibroblasts
    Ninomiya, JT
    Struve, JA
    Stelloh, CT
    Toth, JM
    Crosby, KE
    [J]. JOURNAL OF ORTHOPAEDIC RESEARCH, 2001, 19 (04) : 621 - 628
  • [38] Forsterite surface composition in aqueous solutions: A combined potentiometric, electrokinetic, and spectroscopic approach
    Pokrovsky, OS
    Schott, J
    [J]. GEOCHIMICA ET COSMOCHIMICA ACTA, 2000, 64 (19) : 3299 - 3312
  • [39] THE LATTICE-DYNAMICS OF FORSTERITE
    PRICE, GD
    PARKER, SC
    LESLIE, M
    [J]. MINERALOGICAL MAGAZINE, 1987, 51 (359) : 157 - 170
  • [40] Nanocrystalline forsterite for biomedical applications: Synthesis, microstructure and mechanical properties
    Ramesh, S.
    Yaghoubi, A.
    Lee, K. Y. Sara
    Chin, K. M. Christopher
    Purbolaksono, J.
    Hamdi, M.
    Hassan, M. A.
    [J]. JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2013, 25 : 63 - 69