Morphology evolution of primary Mg2Si in Al-20Mg2Si-0.1Ca alloys prepared with various solidification cooling rates

被引:15
作者
Wang, Hui-Yuan [1 ,2 ,3 ]
Yu, Hong-Chen [2 ,3 ]
Li, Chao [2 ,3 ]
Zha, Min [1 ,2 ,3 ]
Wang, Cheng [2 ,3 ]
Jiang, Qi-Chuan [2 ,3 ]
机构
[1] Jilin Univ, State Key Lab Automot Simulat & Control, 5988 Renmin St, Changchun 130025, Peoples R China
[2] Jilin Univ, Key Lab Automobile Mat, Minist Educ, Nanling Campus,5988 Renmin St, Changchun 130025, Peoples R China
[3] Jilin Univ, Sch Mat Sci & Engn, Nanling Campus,5988 Renmin St, Changchun 130025, Peoples R China
关键词
SI ALLOYS; THERMOELECTRIC PROPERTIES; CA ADDITION; GROWTH; MELT; MICROSTRUCTURE; BEHAVIOR; PRECIPITATION; MICROCRYSTALS; TEMPERATURE;
D O I
10.1039/c7ce00028f
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The morphology evolution of primary Mg2Si in the Al-20Mg(2)Si-0.1Ca alloy was investigated by a mould temperature-controlled solidification technique at various solidification cooling rates. It is found that by lowering the pre-set mould temperature, i. e. increasing the cooling rates, the influence of external factors, i. e. the adsorption of Ca atoms on {100} facets, on the morphology evolution of primary Mg2Si can be strengthened, leading to primary Mg2Si with varying morphologies. With the decrease of mould temperature from 600 to 400 degrees C and then to 200 degrees C and finally to room temperature, primary Mg2Si transformed from a mixture of an equiaxed-dendrite and an octahedron to a truncated octahedron and then to a truncated cube and finally to a cube; in contrast, primary Mg2Si still remained dendritic in the Ca-free Al20Mg(2)Si alloy. Moreover, the skeleton-type growth process of the truncated cubic primary Mg2Si in the modified alloy was identified, where growth steps with some hillocks were observed for the first time. Our study offers a simple and low-cost method to control the morphology and size of primary Mg2Si crystals in the Al-Mg-Si alloy, which is beneficial to the design of lightweight Al-Mg-Si alloys with high strength and toughness.
引用
收藏
页码:1680 / 1688
页数:9
相关论文
共 45 条
[41]   Cooling rate and microstructure of rapidly solidified Al-20 wt.% Si alloy [J].
Xu, CL ;
Wang, HY ;
Qiu, F ;
Yang, YF ;
Jiang, QC .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 417 (1-2) :275-280
[42]   Heterogeneous nucleation of Mg2Si on CaSb2 nucleus in Al-Mg-Si alloys [J].
Yu, Hong-Chen ;
Wang, Hui-Yuan ;
Chen, Lei ;
Liu, Feng ;
Wang, Cheng ;
Jiang, Qi-Chuan .
CRYSTENGCOMM, 2015, 17 (37) :7048-7055
[43]   Microstructure refinement of Mg-Al-Zn-Si alloys [J].
Yuan, GY ;
Liu, ZL ;
Wang, QD ;
Ding, WJ .
MATERIALS LETTERS, 2002, 56 (1-2) :53-58
[44]   Equilibrium pseudobinary Al-Mg2Si phase diagram [J].
Zhang, J ;
Fan, Z ;
Wang, YQ ;
Zhou, BL .
MATERIALS SCIENCE AND TECHNOLOGY, 2001, 17 (05) :494-496
[45]   Iron Phosphate Prepared by Coupling Precipitation and Aging: Morphology, Crystal Structure, and Cr(III) Adsorption [J].
Zhang, Tong B. ;
Lu, Yang C. ;
Luo, Guang S. .
CRYSTAL GROWTH & DESIGN, 2013, 13 (03) :1099-1109