High-cycle fatigue properties of beta Ti alloy 55Ti-30Nb-10Ta-5Zr, gum metal

被引:4
作者
Akita, M. [1 ]
Nakajima, M. [2 ]
Uematsu, Y. [3 ]
Tokaji, K. [3 ]
Kojima, T. [4 ]
机构
[1] Gifu Univ, Fac Engn, Gifu 5011193, Japan
[2] Toyota Natl Coll Technol, Dept Mech Engn, Toyota 4718525, Japan
[3] Gifu Univ, Dept Mech Engn, Gifu 5011193, Japan
[4] Okuma Corp LTD, Oguchi, Aichi 4800193, Japan
关键词
beta titanium alloy; corrosion fatigue; crack growth; crack initiation; fatigue; slip deformation; S-N diagram; PLASTIC-DEFORMATION; TITANIUM; MECHANISM; BEHAVIOR; EVOLUTION;
D O I
10.1111/ffe.12201
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper describes the fatigue properties of the beta titanium alloy 55Ti-30Nb-10Ta-5Zr, generally referred to as 'Gum Metal'. Rotating bending fatigue tests have been performed in laboratory air and in a 3% NaCl aqueous solution. The results obtained were compared with those of a conventional beta titanium alloy, Ti-22V-4Al. In tensile tests, 55Ti-30Nb-10Ta-5Zr indicated elasticity and microplasticity in the elastic region. Thus, the elastic modulus slightly decreased with an increasing strain, and the work hardening was minimal during plastic deformation. The mechanical properties of both of the alloys were comparable. The fatigue strength of 55Ti-30Nb-10Ta-5Zr in laboratory air was higher than that of Ti-22V-4Al, which could be attributed to the higher fatigue crack initiation resistance of 55Ti-30Nb-10Ta-5Zr than Ti-22V-4Al, while the resistance to small fatigue crack growth was similar. The fatigue strength of 55Ti-30Nb-10Ta-5Zr in laboratory air and in the 3% NaCl aqueous solution was analogous. In addition, corrosion pits were not observed in the run-out specimen in the 3% NaCl aqueous solution, indicating a high resistance of 55Ti-30Nb-10Ta-5Zr against corrosion fatigue.
引用
收藏
页码:1223 / 1231
页数:9
相关论文
共 28 条
[1]   Recent developments in microstructure/property relationships of beta titanium alloys [J].
Ankem, S ;
Greene, CA .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 263 (02) :127-131
[2]   Formation of nanocrystals due to giant-fault deformation in Gum Metals [J].
Bobylev, S. V. ;
Ishizaki, T. ;
Kuramoto, S. ;
Ovid'ko, I. A. .
SCRIPTA MATERIALIA, 2011, 65 (08) :668-671
[3]   An overview on the use of titanium in the aerospace industry [J].
Boyer, RR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 213 (1-2) :103-114
[4]   Elastic deformation behavior of multi-functional Ti-Nb-Ta-Zr-O alloys [J].
Furuta, T ;
Kuramoto, S ;
Hwang, J ;
Nishino, K ;
Saito, T .
MATERIALS TRANSACTIONS, 2005, 46 (12) :3001-3007
[5]   The mechanism of strength and deformation in Gum Metal [J].
Furuta, T. ;
Kuramoto, S. ;
Morris, J. W., Jr. ;
Nagasako, N. ;
Withey, E. ;
Chrzan, D. C. .
SCRIPTA MATERIALIA, 2013, 68 (10) :767-772
[6]   Giant faults in deformed Gum Metal [J].
Gutkin, M. Yu. ;
Ishizaki, T. ;
Kuramoto, S. ;
Ovid'ko, I. A. ;
Skiba, N. V. .
INTERNATIONAL JOURNAL OF PLASTICITY, 2008, 24 (08) :1333-1359
[7]   Nanodisturbances in deformed Gum Metal [J].
Gutkin, Mikhail Yu. ;
Ishizaki, Toshitaka ;
Kuramoto, Shigeru ;
Ovid'ko, Ilya A. .
ACTA MATERIALIA, 2006, 54 (09) :2489-2499
[8]   Plastic deformation in a multifunctional Ti-Nb-Ta-Zr-O alloy [J].
Kuramoto, S ;
Furuta, T ;
Hwang, JH ;
Nishino, K ;
Saito, T .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (03) :657-662
[9]   Elastic properties of Gum Metal [J].
Kuramoto, Shigeru ;
Furuta, Tadahiko ;
Hwang, Junghwan ;
Nishino, Kazuaki ;
Saito, Takashi .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 442 (1-2) :454-457
[10]   ELECTRONIC-STRUCTURE AND PHASE-STABILITY OF TITANIUM-ALLOYS [J].
MORINAGA, M ;
YUKAWA, N ;
ADACHI, H .
TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (06) :555-562