Cavitation Erosion Corrosion Behaviour of Manganese-nickel-aluminum Bronze in Comparison with Manganese-brass

被引:0
作者
Yu, Hong [1 ]
Zheng, Yugui [1 ]
Yao, Zhiming [1 ]
机构
[1] Chinese Acad Sci, State Key Lab Corros & Protect, Inst Met Res, Shenyang 110016, Peoples R China
基金
中国国家自然科学基金;
关键词
Cavitation erosion; Marine propeller; Manganese-nickel-aluminum bronze; Manganese-brass; Synergism; Work-hardening ability; Stacking fault energy; STACKING-FAULT ENERGY; ALLOY; SEAWATER; STEELS; CAST;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The cavitation erosion corrosion behaviour of ZQMn12-8-3-2 manganese-nickel-aluminum bronze and ZHMn55-3-1 manganese-brass was investigated by mass loss, electrochemical measurements (polarization curves and electrochemical impedance spectroscopy) and the cavitation damaged surfaces were observed by scanning electron microscopy (SEM). The results showed that ZQMn12-8-3-2 had better cavitation erosion resistance than ZHMn55-3-1. After the cavitation erosion for 6 h, the cumulative mass loss of ZQMn12-8-3-2 was about 1/3 that of ZHMn55-3-1. The corrosion current density of ZQMn12-8-3-2 was less than that of ZHMn55-3-1 under both static and cavitaiton condition. The free-corrosion potentials of ZQMn12-8-3-2 and ZHMn55-3-1 were all shifted in positive direction under cavitation condition compared to static condition. In the total cumulative mass loss under cavitation condition, the pure erosion played a key role for the two tested materials (74% for ZHMn55-3-1 and 60% for ZQMn12-8-3-2), and the total synergism between corrosion and erosion of ZQMn12-8-3-2 (39%) was larger than that of ZHMn55-3-1 (23%). The high cavitation erosion resistance of ZQMn12-8-3-2 was mainly attributed to its lower stacking fault energy (SFE), the higher microhardness and work-hardening ability as well as the favorable propagation of cavitation. cracks for ZQMn12-8-3-2, i.e., parallel to the surface rather than perpendicular to the surface for ZHMn55-3-1.
引用
收藏
页码:758 / 766
页数:9
相关论文
共 24 条
[1]   The role of microstructure of nickel-aluminium-bronze alloy on its cavitation corrosion behavior in natural seawater [J].
Al-Hashem, A ;
Riad, W .
MATERIALS CHARACTERIZATION, 2002, 48 (01) :37-41
[2]   CAVITATION CORROSION BEHAVIOR OF CAST NICKEL-ALUMINUM BRONZE IN SEAWATER [J].
ALHASHEM, A ;
CACERES, PG ;
RIAD, WT ;
SHALABY, HM .
CORROSION, 1995, 51 (05) :331-342
[3]  
[Anonymous], J FLUIDS ENG
[4]  
*ASTM INT, 1985, G3285 ASTM INT, P187
[5]   Erosion and erosion-corrosion performance of cast and thermally sprayed nickel-aluminium bronze [J].
Barik, RC ;
Wharton, JA ;
Wood, RJK ;
Tan, KS ;
Stokes, KR .
WEAR, 2005, 259 (1-6) :230-242
[6]  
Brezina P., 1982, Int. Met. Rev., V27, P77
[7]  
CAO CN, 2004, CORROSION ELECTROCHE, P213
[8]  
GONZALEZ JL, 1992, P C APPL STAINL STEE, V2, P1009
[9]  
Karimi A., 1986, International Metals Reviews, V31, P1
[10]   Cavitation erosion and corrosion behavior of copper-manganese-aluminum alloy weldment [J].
Li, XY ;
Yan, YG ;
Ma, L ;
Xu, ZM ;
Li, JG .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 382 (1-2) :82-89