Crack-healing during two-stage crystallization of biomedical lithium (di)silicate glass-ceramics

被引:40
作者
Belli, Renan [1 ]
Lohbauer, Ulrich [1 ]
Goetz-Neunhoeffer, Friedlinde [2 ]
Hurle, Katrin [2 ]
机构
[1] Friedrich Alexander Univ Erlangen Nurnberg FAU, Zahnklin 1, Zahnerhaltung & Parodontol, Forschungslab Dent Biomaterialien, Glueckstr 11, D-91054 Erlangen, Germany
[2] Friedrich Alexander Univ Erlangen Nurnberg FAU, GeoZentrum Nordbayern, Mineral, Schlossgarten 5a, D-91054 Erlangen, Germany
关键词
Lithium silicate; Lithium disilicate; X-ray diffraction; Glass-ceramic; Dental; Fracture toughness; SYNCHROTRON X-RAY; 3 BALLS TEST; FRACTURE-TOUGHNESS; DISILICATE GLASS; CONCURRENT CRYSTALLIZATION; RESIDUAL-STRESSES; FLEXURAL STRENGTH; BRITTLE DISCS; PART; SURFACE;
D O I
10.1016/j.dental.2019.05.013
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. The study is aimed to evaluate the two single commercially available two-step lithium-(di)silicate systems by analyzing their parent glass composition and studying the quantitative crystalline and glass phase evolution during the second stage heat-treatment. The mechanical repercussions of the crystallization firing were evaluated using strength and fracture toughness tests. Methods. XRF and ICP-OES were used to determine the oxide composition of the parent glasses in Suprinity PC (Vita Zahnfabrik) and IPS e.max CAD (Ivoclar-Vivadent). The crystalline phase of both materials was determined by quantitative XRD and the G-factor method in the partially and post-crystallization states. The oxide composition of the residual glass phase was derived by subtracting the chemistry of the crystalline phase fractions from the parent glass composition. Mechanical testing of biaxial flexural strength and fracture toughness were used to demonstrate how crack-like defects behave during crystallization. Results. The two tested lithium (di)silicate systems showed strong differences in oxide composition of the parent glass. This showed to influence the transformation of lithium metasilicate in lithium disilicate, with the former remaining in high vol.% fraction in the post-crystallization Suprinity PC. In IPS e.max CAD cristobalite precipitated at the surface during the second-heat treatment. Strength and fracture toughness tests revealed that crack in both materials, whether introduced by grinding or indentation, heal during the crystallization firing. Cristobalite seemed to have contributed to a surface strengthening effect in IPS e.max CAD. Significance. Accurate crystalline phase quantification aids in the determination of the residual glass composition in dental glass-ceramics. For both systems crystallization firing induced healing of cracks generated by CAM grinding. (C) 2019 The Academy of Dental Materials. Published by Elsevier Inc. All rights reserved.
引用
收藏
页码:1130 / 1145
页数:16
相关论文
共 64 条
  • [1] [Anonymous], 2012, NEW CONTRIBUTIONS R
  • [2] [Anonymous], 2010, C1421 ASTM
  • [3] Influence of ZrO2 on the crystallization and properties of lithium disilicate glass-ceramics derived from a multi-component system
    Apel, Elke
    van't Hoen, Christian
    Rheinberger, Volker
    Holand, Wolfram
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (2-3) : 1571 - 1577
  • [4] Beall G.H, 2012, GLASS CERAMIC TECHNO, VSecond, P86
  • [5] Belli Renan, 2016, Case Studies in Engineering Failure Analysis, V7, P71, DOI 10.1016/j.csefa.2016.10.001
  • [6] Fracture Rates and Lifetime Estimations of CAD/CAM All-ceramic Restorations
    Belli, R.
    Petschelt, A.
    Hofner, B.
    Hajto, J.
    Scherrer, S. S.
    Lohbauer, U.
    [J]. JOURNAL OF DENTAL RESEARCH, 2016, 95 (01) : 67 - 73
  • [7] Fracture toughness testing of biomedical ceramic-based materials using beams, plates and discs
    Belli, Renan
    Wendler, Michael
    Petschelt, Anselm
    Lube, Tanja
    Lohbauer, Ulrich
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (16) : 5533 - 5544
  • [8] Fracture anisotropy in texturized lithium disilicate glass-ceramics
    Belli, Renan
    Wendler, Michael
    Cicconi, Maria Rita
    de Ligny, Dominique
    Petschelt, Anselm
    Werbach, Katharina
    Peterlik, Herwig
    Lohbauer, Ulrich
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 2018, 481 : 457 - 469
  • [9] Practical and theoretical considerations on the fracture toughness testing of dental restorative materials
    Belli, Renan
    Wendler, Michael
    Zorzin, Jose I.
    Lohbauer, Ulrich
    [J]. DENTAL MATERIALS, 2018, 34 (01) : 97 - 119
  • [10] Chairside CAD/CAM materials. Part 1: Measurement of elastic constants and microstructural characterization
    Belli, Renan
    Wendler, Michael
    de Ligny, Dominique
    Cicconi, Maria Rita
    Petschelt, Anselm
    Peterlik, Herwig
    Lohbauer, Ulrich
    [J]. DENTAL MATERIALS, 2017, 33 (01) : 84 - 98