Evaluation of resin adhesion to zirconia ceramic using some organosilanes

被引:158
作者
Matinlinna, Jukka P.
Heikkinen, Mo
Ozcan, Mutlu
Lassila, Lippo V. J.
Vallittu, Pekka K.
机构
[1] NIOM, Nordic Inst Dent Mat, NO-1305 Haslum, Norway
[2] Univ Turku, Inst Dent, Dept Prosthet Dent & Biomat Sci, FI-20520 Turku, Finland
[3] Univ Groningen, Fac Med Sci, Dept Dent & Oral HYg, NL-9713 AV Groningen, Netherlands
基金
芬兰科学院;
关键词
silane; silica-coating; silanization; zirconia; Bis-GMA; luting cement;
D O I
10.1016/j.dental.2005.11.035
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. This study evaluated and compared the effect of three trialkoxysilane coupling agents on the bond strength of a Bis-GMA-based unfilled resin and a dimethacrylate-based resin composite luting cement to a zirconia ceramics (Procera(R) AllZircon, Nobel Biocare, Goteborg, Sweden). Methods. Six square-shaped zirconia specimens were used for each test group, a total of 72 specimens. The specimens in each group were all assigned to air-borne alumina particle abrasion followed by tribochemical silica-coating and silanization with 1 vol% solutions of 3-methacryloyloxypropyltrimethoxysilane, 3-acryloyloxypropyltrimethoxysilane, or 3-isocyanatopropyltriethoxysilane in an ethanol-water mixture. The sample stubs were made of a Bis-GMA/MMA/DMAEMA resin or a commercial resin composite luting cement (RelyX(TM) ARC, 3M ESPE, Seefeld, Germany). They were bonded to the conditioned and silanized silica-coated zirconia specimens using polyethylene molds. All specimens were tested at dry and thermo-cycled (6000, 5-55 degrees C, 30 s) conditions. The shear bond strength of resin stubs to zirconia was measured in a universal testing machine (cross-head speed 1 mm/min). Results. in dry conditions, the highest shear bond strength was 9.7 MPa (S.D. 3.3 MPa), and for thermo-cycled samples 7.4 MPa (S.D. 2.4 MPa) was obtained with RelyX(TM) ARC cement with 3-methacryloyloxypropyltrimethoxysilane. In general, thermo-cycling decreased the bond strengths significantly for the Bis-GMA resin (ANOVA, p<0.005). The resin, cement and silanes differed significantly silanes (ANOVA, p<0.005). All samples silanized with 3-isocyanatopropyltriethoxysilane de-bonded during thermo-cycling. De-bonding was dominantly due to adhesive failure. Significance. Bonding of the experimental resin and commercial cement to silica-coated zirconia is effective with 3-methacryloyloxypropyltrimethoxysilane or 3-methacryloyloxypropyltrimethoxysilane, but not with 3-isocyanatopropyltriethoxysilane. (C) 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:824 / 831
页数:8
相关论文
共 31 条
[31]  
Wegner S M, 2000, J Adhes Dent, V2, P139