Electron Emission Energy Barriers and Stability of Sc2O3 with Adsorbed Ba and Ba-O

被引:25
作者
Jacobs, Ryan M. [1 ]
Booske, John H. [1 ,2 ]
Morgan, Dane [1 ,3 ]
机构
[1] Univ Wisconsin, Interdisciplinary Mat Sci Program, Madison, WI 53706 USA
[2] Univ Wisconsin, Dept Elect & Comp Engn, Madison, WI 53706 USA
[3] Univ Wisconsin, Dept Mat Sci & Engn, Madison, WI 53706 USA
关键词
SCANDATE CATHODES; CORRELATION HOLE; SURFACE; MODEL; FILMS; OXIDE; TUNGSTEN; MECHANISM; OPERATION; SYSTEM;
D O I
10.1021/jp503320r
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study we employ density functional theory (DFT) methods to investigate the surface energy barrier for electron emission (surface barrier) and thermodynamic stability of Ba and Ba-O species adsorption (relative to formation of bulk BaO) under conditions of high temperature (approximately 1200 K) and low pressure (approximately 10(-10) Ton) on the low-index surfaces of bixbyite Sc2O3. We employ both the standard generalized gradient approximation (GGA) and the hybrid HSE functional to calculate accurate surface barriers from relaxed GGA structures. The role of Ba in lowering the cathode surface barrier is investigated via adsorption of atomic Ba and Ba-O dimers, where the highest simulated dimer coverage corresponds to a single-monolayer film of rocksalt BaO. The change of the surface barrier of a semiconductor due to adsorption of surface species is decomposed into two parts: a surface dipole component and a doping component. The dipole component is the result of charge rearrangement at the surface and described by the electrostatic Helmholtz equation. The doping component is due to charge transfer from the surface species, which changes the Fermi level and thereby changes the surface barrier. Different initial geometries, adsorption sites, and coverages were tested for the most stable low-index Sc2O3 surfaces ((011) and (111)) for both atomic Ba and Ba-O dimers. The lowest surface barrier with atomic Ba on Sc2O3 was found to be 2.12 and 2.04 eV for the (011) and (111) surfaces at 3 and 1 Ba atoms per surface unit cell (0.250 and 0.083 Ba per surface O), respectively. The lowest surface barrier for Ba-O on Sc2O3 was found to be 1.21 eV on (011) for a 7 Ba-O dimer-per-unit-cell coverage (0.583 dimers per surface O). Generally, we found that Ba in its atomic form on Sc2O3 surfaces is not stable relative to bulk BaO, while Ba-O dimer coverages between 3 and 7 Ba-O dimers per (011) surface unit cell (0.250 and 0.583 dimers per surface O) produce stable structures relative to bulk BaO. Ba-O dimer adsorption on Sc2O3 (111) surfaces was found to be unstable versus BaO over the full range of coverages studied. Investigation of combined n-type doping and surface dipole modification showed that their effects interact to yield a reduction less than the two contributions would yield separately.
引用
收藏
页码:19742 / 19758
页数:17
相关论文
共 50 条
  • [21] Virtual GaN substrates via Sc2O3/Y2O3 buffers on Si(111): Transmission electron microscopy characterization of growth defects
    Niermann, T.
    Zengler, D.
    Tarnawska, L.
    Stork, P.
    Schroeder, T.
    Lehmann, M.
    JOURNAL OF APPLIED PHYSICS, 2013, 113 (22)
  • [22] Conduction band energies and hot-electron transport characteristics of epitaxial Sc2O3/Si (111) studied by ballistic electron emission microscopy and internal photoemission
    Cai, W.
    Stone, S. E.
    Pelz, J. P.
    Edge, L. F.
    Schlom, D. G.
    APPLIED PHYSICS LETTERS, 2007, 91 (04)
  • [23] Structure and chemistry of the (111)Sc2O3/(0001) GaN epitaxial interface
    Weng, X.
    Tian, W.
    Schlom, D. G.
    Dickey, E. C.
    APPLIED PHYSICS LETTERS, 2010, 96 (24)
  • [24] Optical and scintillation properties of Sc2O3, Y2O3 and Lu2O3 transparent ceramics synthesized by SPS method
    Futami, Yoshisuke
    Yanagida, Takayuki
    Fujimoto, Yutaka
    Pejchal, Jan
    Sugiyama, Makoto
    Kurosawa, Shunsuke
    Yokota, Yuui
    Ito, Akihiko
    Yoshikawa, Akira
    Goto, Takashi
    RADIATION MEASUREMENTS, 2013, 55 : 136 - 140
  • [25] Emission and life characteristics of thin film top-layer scandate cathode and diffusion of Sc2O3 and W
    Uda, E
    Nakamura, O
    Matsumoto, S
    Higuchi, T
    APPLIED SURFACE SCIENCE, 1999, 146 (1-4) : 31 - 38
  • [26] DFT Study of the Structural and Magnetic Properties of Triple Perovskites Ba3TiRu2O9 and Ba3ZrRu2O9
    Zada, Rahman
    Ali, Zahid
    Mehmood, Shahid
    JOURNAL OF INORGANIC AND ORGANOMETALLIC POLYMERS AND MATERIALS, 2024, 34 (07) : 3115 - 3126
  • [27] Passively mode locked femtosecond Tm:Sc2O3 laser at 2.1 μm
    Lagatsky, A. A.
    Koopmann, P.
    Fuhrberg, P.
    Huber, G.
    Brown, C. T. A.
    Sibbett, W.
    OPTICS LETTERS, 2012, 37 (03) : 437 - 439
  • [28] Phase stability and transport characteristics of (ZrO2)1-x(Sc2O3)x(CeO2)y and (ZrO2)1-x-y-z(Sc2O3)x(CeO2)y(Y2O3)z solid solution crystals
    Agarkov, D. A.
    Borik, M. A.
    Bublik, V. T.
    Chislov, A. S.
    Kulebyakin, A., V
    Kuritsyna, I. E.
    Kolotygin, V. A.
    Lomonova, E. E.
    Milovich, F. O.
    Myzina, V. A.
    Osiko, V. V.
    Tabachkova, N. Yu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 791 : 445 - 451
  • [29] The laser-induced damage mechanism of amorphous and crystalline Sc2O3 films
    Kong, Pengfei
    Pu, Yunti
    Ma, Ping
    Zhu, Jiliang
    VACUUM, 2021, 191
  • [30] Key Role of Bismuth in the Magnetoelastic Transitions of Ba3BiIr2O9 and Ba3BiRu2O9 As Revealed by Chemical Doping
    Blanchard, Peter E. R.
    Huang, Zixin
    Kennedy, Brendan J.
    Liu, Samuel
    Miiller, Wojciech
    Reynolds, Emily
    Zhou, Qingdi
    Avdeev, Maxim
    Zhang, Zhaoming
    Aitken, Jade B.
    Cowie, Bruce C. C.
    Jang, Ling-Yun
    Thiam Teck Tan
    Li, Sean
    Ling, Chris D.
    INORGANIC CHEMISTRY, 2014, 53 (02) : 952 - 960