Effect of sintering pressure on microstructure and mechanical properties of hot-pressed Ti6Al4V-ZrO2 materials

被引:28
作者
Madeira, S. [1 ]
Pinto, A. M. P. [1 ]
Rodrigues, L. C. [3 ,4 ]
Carvalho, O. [1 ]
Miranda, G. [1 ]
Reis, R. L. [3 ,4 ]
Carames, Joao [2 ]
Silva, F. S. [1 ]
机构
[1] Univ Minho, CMEMS, Campus Azurem, P-4800058 Guimaraes, Portugal
[2] Univ Lisbon, Fac Med Dent, P-1649003 Lisbon, Portugal
[3] Univ Minho, Headquarters European Inst Excellence Tissue Engn, Bs Res Grp Biomat Biodegradables & Biomimet, AvePk, P-4806909 Taipas, GuimarBes, Portugal
[4] ICVS 3Bs PT Govt Associate Lab, Braga, Guimaraes, Portugal
关键词
Ti6Al4V; ZrO2; Metal-ceramic; Microstructure; Mechanical properties; BIOMEDICAL APPLICATIONS; INTERFACIAL REACTIONS; TI-6AL-4V ALLOY; TITANIUM-ALLOYS; STABILIZED ZIRCONIA; DENTAL IMPLANTS; COMPOSITES; 1550-DEGREES-C; EVOLUTION; PHASE;
D O I
10.1016/j.matdes.2017.02.038
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The development of new design approaches for biomedical applications using conventional and well accepted bio inert materials is an actual challenge. This study proposes a bilayered materials design approach obtained by hot pressing and is concerned with the influence of sintering pressure on the interface reaction between titanium alloy (Ti6AI4V) and zirconia (ZrO2), on density and mechanical properties of the Ti6AI4V-ZrO2. For this purpose, different sintering pressures were studied (P = 5, 20 and 100 MPa). Bilayered materials were produced by hot pressing process, at T = 1175 degrees C. Microstructural characterization showed that Ti6AI4V reacts with ZrO2 (for P >= 20 MPa) and that the interface reaction is strongly dependent on pressure. Additionally, an oxygen-deficient ZrO2 _ (x) black zirconia layer was obtained for specimens produced at P = 20 and 100 MPa as result of decreased O/Zr ratio due to Ti diffusion into ZrO2 side. Young's modulus and hardness properties were evaluated by nano indentation test. The results showed that these properties are influenced by sintering pressure, increasing with an increase on sintering pressure, with the highest improvement for specimens produced at higher pressure. (C) 2017 Elsevier Ltd. All rights reserved.
引用
收藏
页码:394 / 403
页数:10
相关论文
共 40 条
  • [1] Phase transformations during cooling in α+β titanium alloys
    Ahmed, T
    Rack, HJ
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2): : 206 - 211
  • [2] Spark plasma sintering of a commercially available granulated zirconia powder: Comparison with hot-pressing
    Bernard-Granger, Guillaume
    Addad, Ahmed
    Fantozzi, Gilbert
    Bonnefont, Guillaume
    Guizard, Christian
    Vernat, Dorothee
    [J]. ACTA MATERIALIA, 2010, 58 (09) : 3390 - 3399
  • [3] Initial stages of oxide formation on the Zr surface at low oxygen pressure: An in situ FIM and XPS study
    Bespalov, I.
    Datler, M.
    Buhr, S.
    Drachsel, W.
    Rupprechter, G.
    Suchorski, Y.
    [J]. ULTRAMICROSCOPY, 2015, 159 : 147 - 151
  • [4] Microstructural evolution and mechanical properties of the Ti-6Al-4V alloy produced by vacuum hot-pressing
    Bolzoni, L.
    Montealegre Melendez, I.
    Ruiz-Navas, E. M.
    Gordo, E.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 546 : 189 - 197
  • [5] Inductive hot-pressing of titanium and titanium alloy powders
    Bolzoni, L.
    Ruiz-Navas, E. M.
    Neubauer, E.
    Gordo, E.
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 2012, 131 (03) : 672 - 679
  • [6] Compositional Dependence of Phase Formation Mechanisms at the Interface Between Titanium and Calcia-Stabilized Zirconia at 1550°C
    Chang, Yao-Wen
    Lin, Chien-Cheng
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (11) : 3893 - 3901
  • [7] Microstructure of diffusional zirconia-titanium and zirconia-(Ti-6 wt% Al-4 wt% V) alloy joints
    Correia, RN
    Emiliano, JV
    Moretto, P
    [J]. JOURNAL OF MATERIALS SCIENCE, 1998, 33 (01) : 215 - 221
  • [8] Densification and properties of zirconia prepared by three different sintering techniques
    Dahl, P.
    Kaus, I.
    Zhao, Z.
    Johnsson, M.
    Nygren, M.
    Wiik, K.
    Grande, T.
    Einarsrud, M.-A.
    [J]. CERAMICS INTERNATIONAL, 2007, 33 (08) : 1603 - 1610
  • [9] Composites based on titanium alloy Ti-6Al-4V with an addition of inert ceramics and bioactive ceramics for medical applications fabricated by spark plasma sintering (SPS method)
    Dudek, A.
    Klimas, M.
    [J]. MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2015, 46 (03) : 237 - 247
  • [10] Microstructural characterization and formation of α′ martensite phase in Ti-6Al-4V alloy butt joints produced by friction stir and gas tungsten arc welding processes
    Esmaily, M.
    Mortazavi, S. Nooshin
    Todehfalah, P.
    Rashidi, M.
    [J]. MATERIALS & DESIGN, 2013, 47 : 143 - 150