Effect of Bulk Heat Treatment and Plasma Surface Hardening on the Microstructure and Erosion Wear Resistance of Complex-Alloyed Cast Irons with Spheroidal Vanadium Carbides

被引:18
作者
Efremenko, V. G. [1 ]
Shimizu, K. [2 ]
Pastukhova, T. V. [1 ]
Chabak, Yu. G. [1 ]
Kusumoto, K. [2 ]
Efremenko, A. V. [1 ]
机构
[1] Pryazovskyi State Tech Univ, Ul Univ 7, UA-87500 Mariupol, Ukraine
[2] Muroran Inst Technol, Mizumoto-cho 27-1, Muroran, Hokkaido 0508585, Japan
关键词
spheroidal carbides; erosive wear resistance; quenching; cryogenic treatment; hardness; martensite; austenite;
D O I
10.3103/S1068366617010056
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The results of an investigation of the effect of bulk quenching from temperature in the range of 760-1050 degrees C, cryogenic treatment (-196 degrees C) and surface plasma hardening on the abrasive-erosion wear of frugally alloyed V-Cr-Mn-Ni cast irons with spheroidal vanadium carbides have been presented in this article. It has been found that cast irons containing 5.0-7.5% V, 4.5-9.0% Cr, and 5.5-5.7% (total) of Mn and Ni after heat treatment have a 2-3-fold advantage in wear resistance compared to the prototype high-vanadium cast iron (11.9% V, 12.9% Mn). The maximum wear resistance of cast irons studied is achieved by quenching at 760 degrees C followed by plasma surface hardening, as well as quenching at 840 degrees C, followed by cryogenic treatment. These treatments result in the formation of an optimum microstructure that consists of spheroidal vanadium carbides, eutectic carbides M7C3, and a martensite-austenite matrix reinforced by secondary carbides. The increase in quenching temperature leads to an increase in the amount of residual austenite and decrease in the erosive wear resistance of cast irons.
引用
收藏
页码:58 / 64
页数:7
相关论文
共 10 条
[1]   Effect of vanadium and chromium on the microstructural features of V-Cr-Mn-Ni spheroidal carbide cast irons [J].
Efremenko, V. G. ;
Shimizu, K. ;
Cheiliakh, A. P. ;
Kozarevskaya, T. V. ;
Kusumoto, K. ;
Yamamoto, K. .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2014, 21 (11) :1096-1108
[2]   Kinetic Parameters of Secondary Carbide Precipitation in High-Cr White Iron Alloyed by Mn-Ni-Mo-V Complex [J].
Efremenko, V. G. ;
Chabak, Yu. G. ;
Brykov, M. N. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (05) :1378-1385
[3]   Matrix Microstructure and Its Micro-Analysis of Constituent Phases in As-Cast Fe-Cr-C-V Alloys [J].
Filipovic, Mirjana ;
Romhanji, Endre ;
Kamberovic, Zeljko ;
Korac, Marija .
MATERIALS TRANSACTIONS, 2009, 50 (10) :2488-2492
[4]  
Kawano Y., 2002, US Patent, Patent No. 6406563
[5]  
Kawano Y., 1999, J JPN FOUNDRY ENG SO, V1, P727
[6]   Principles of development of grinding media with increased wear resistance. Part 2. Optimization of steel composition to suit conditions of operation of grinding media [J].
Koval, A. D. ;
Efremenko, V. G. ;
Brykov, M. N. ;
Andrushchenko, M. I. ;
Kulikovskii, R. A. ;
Efremenko, A. V. .
JOURNAL OF FRICTION AND WEAR, 2012, 33 (02) :153-159
[7]  
Leshchinskii L.K., 1990, PLAZMENNOE POVERKHNO
[8]  
Shigenori N., 2008, J JPN FOUNDRY ENG SO, V80, P3
[9]  
Shigenori N., 2002, J JPN FOUNDRY ENG SO, V74, P279
[10]  
Xinba Y., 2008, WEAR, V264, P247