Impacts of trace carbon on the microstructure of as-sintered biomedical Ti-15Mo alloy and reassessment of the maximum carbon limit

被引:58
作者
Yan, M. [1 ,2 ]
Qian, M. [2 ]
Kong, C. [3 ]
Dargusch, M. S. [1 ]
机构
[1] Univ Queensland, Queensland Ctr Adv Mat Proc & Mfg AMPAM, Sch Mech & Min Engn, Brisbane, Qld 4072, Australia
[2] Univ Queensland, Sch Mech & Min Engn, ARC Ctr Excellence Design Light Met, Brisbane, Qld 4072, Australia
[3] Univ New S Wales, Electron Microscopy Unit, Sydney, NSW 2052, Australia
关键词
Biomedical titanium alloys; Carbon limit; Titanium carbides; 3-D tomography; TI-MO ALLOYS; MECHANICAL-PROPERTIES; CORROSION-RESISTANCE; NEUTRON-DIFFRACTION; TITANIUM-ALLOYS; BEHAVIOR; FABRICATION; MODULUS;
D O I
10.1016/j.actbio.2013.10.034
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The formation of grain boundary (GB) brittle carbides with a complex three-dimensional (3-D) morphology can be detrimental to both the fatigue properties and corrosion resistance of a biomedical titanium alloy. A detailed microscopic study has been performed on an as-sintered biomedical Ti-15Mo (in wt.%) alloy containing 0.032 wt.% C. A noticeable presence of a carbon-enriched phase has been observed along the GB, although the carbon content is well below the maximum carbon limit of 0.1 wt.% specified by ASTM Standard F2066. Transmission electron microscopy (TEM) identified that the carbon-enriched phase is face-centred cubic Ti2C. 3-D tomography reconstruction revealed that the Ti2C structure has morphology similar to primary alpha-Ti. Nanoindentation confirmed the high hardness and high Young's modulus of the GB Ti2C phase. To avoid GB carbide formation in Ti-15Mo, the carbon content should be limited to 0.006 wt.% by Thermo-Calc predictions. Similar analyses and characterization of the carbide formation in biomedical unalloyed Ti, Ti-6Al-4V and Ti-16Nb have also been performed. (C) 2013 Acts Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1014 / 1023
页数:10
相关论文
共 52 条
[1]  
Adya N., 2005, The Journal of Indian Prosthodontic Society, V5, P126, DOI DOI 10.4103/0972-4052.17104
[2]   A study on corrosion resistance of the Ti-10Mo experimental alloy after different processing methods [J].
Alves, APR ;
Santana, FA ;
Rosa, LAA ;
Cursino, SA ;
Codaro, EN .
MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS, 2004, 24 (05) :693-696
[3]  
[Anonymous], 2011, V1301 STM INT
[4]  
[Anonymous], 2012, J APPL PHYS, DOI DOI 10.1063/1.3677761
[5]  
[Anonymous], 2011, F147208 ASTM INT
[6]  
[Anonymous], 2011, F6706 ASTM INT
[7]  
BANIA PJ, 1990, BETA TITANIUM ALLOYS, P3
[8]   Repeatability of corrosion parameters for titanium-molybdenum alloys in 0.9% NaCl solution [J].
Capela, Marisa V. ;
Acciari, Heloisa A. ;
Capela, Jorge Manuel V. ;
Carvalho, Thaisa M. ;
Melin, Maria Cecilia S. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 465 (1-2) :479-483
[9]   Effect of cooling process on the α phase formation and mechanical properties of sintered Ti-Fe alloys [J].
Chen, Bor-Yuan ;
Hwang, Kuen-Shyang ;
Ng, Ka-Lok .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (13-14) :4556-4563
[10]   Role of alloying elements in microstructures of beta titanium alloys with carbon additions [J].
Chen, ZQ ;
Li, YG ;
Hu, D ;
Loretto, MH ;
Wu, X .
MATERIALS SCIENCE AND TECHNOLOGY, 2003, 19 (10) :1391-1398