Thermal and mechanical properties of Sn-Zn-Bi lead-free solder alloys

被引:86
作者
El-Daly, A. A. [1 ]
Swilem, Y. [1 ]
Makled, M. H. [2 ]
El-Shaarawy, M. G. [2 ]
Abdraboh, A. M. [2 ]
机构
[1] Zagazig Univ, Fac Sci, Dept Phys, Zagazig, Egypt
[2] Banha Univ, Fac Sci, Dept Phys, Banha, Egypt
关键词
Lead-free solder; Sn-Zn alloy; Thermal properties; Mechanical properties; Microstructure; INTERFACIAL REACTIONS; TENSILE PROPERTIES; SHEAR-STRENGTH; MICROSTRUCTURE; TEMPERATURE; AG; AL; CU; METALLIZATION; SUBSTRATE;
D O I
10.1016/j.jallcom.2009.04.108
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Sn-Zn eutectic alloy has been considered as one of the lead-free solder materials that can replace the toxic Sn-37Pb solder without increasing soldering temperature. This study investigates the effect of Bi content on the microstructure, thermal, and mechanical properties of the eutectic Sn-Zn alloy. The results indicate that the microstructures of the Pb-free solders were eutectic. Addition of Bi decreased the melting point and heat of fusion of the solders. 1% Bi addition enhanced the solid solution effect and raised the tensile strength of the as-cast alloys. Notably, with increasing Bi content, the SnBi inter-metallic compound (IMC) precipitates and the ZnO phase are extracted from the beta-Sn matrix with non-uniform microstructure. The ZnO and SnBi IMC precipitates are considered to be the crucial reasons for rapid deterioration of the tensile properties of the specimens. Furthermore, the SnBi IMC particles are transformed into Bi-rich phase during the annealing process, which resulting in an increase of the susceptibilities of Zn to oxygen for the annealed Sn-9Zn-4Bi alloys. Compared with the other alloys, the newly developed Sn-9Zn-1Bi alloy showed some fine properties and this lead-free solder could substitute some Pb-containing solder alloys in microelectronic components packaging and interconnects. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:134 / 142
页数:9
相关论文
共 27 条
[1]   Effects of small additions of Ag, Al, and Ga on the structure and properties of the Sn-9Zn eutectic alloy [J].
Chen, KI ;
Cheng, SC ;
Wu, S ;
Lin, KL .
JOURNAL OF ALLOYS AND COMPOUNDS, 2006, 416 (1-2) :98-105
[2]   The microstructures and mechanical properties of the Sn-Zn-Ag-Al-Ga solder alloys - The effect of Ga [J].
Chen, KI ;
Lin, KL .
JOURNAL OF ELECTRONIC MATERIALS, 2003, 32 (10) :1111-1116
[3]   Microstructure and mechanical properties of Sn-8.55Zn-1Ag-XAl solder alloys [J].
Cheng, SC ;
Lin, KL .
MATERIALS TRANSACTIONS, 2005, 46 (01) :42-47
[4]   Effect of aluminum addition on tensile properties of naturally aged Sn-9Zn eutectic solder [J].
Chuang, CM ;
Lui, TS ;
Chen, LH .
JOURNAL OF MATERIALS SCIENCE, 2002, 37 (01) :191-195
[5]   Microstructural evolution of Sn-9Zn-3Bi solder/Cu joint during long-term aging at 170°C [J].
Duan, LL ;
Yu, DQ ;
Han, SQ ;
Ma, HT ;
Wang, L .
JOURNAL OF ALLOYS AND COMPOUNDS, 2004, 381 (1-2) :202-207
[6]   Creep properties of Sn-Sb based lead-free solder alloys [J].
El-Daly, A. A. ;
Swilem, Y. ;
Hammad, A. E. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 471 (1-2) :98-104
[7]  
El-Daly AA, 2008, J MATER SCI TECHNOL, V24, P921
[8]   Superplasticity in a relatively low melting point Sn-31.1Pb-3.4Zn solder alloys [J].
El-Daly, AA .
PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2003, 200 (02) :333-338
[9]   Investigations on microhardness of Sn-Zn based lead-free solder alloys as replacement of Sn-Pb solder [J].
Islam, RA ;
Wu, BY ;
Alam, MO ;
Chan, YC ;
Jillek, W .
JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 392 (1-2) :149-158
[10]   Encapsulation of lead-free Sn/Zn/Bi solder alloy particles by coating with wax powder for improving oxidation resistance [J].
Iwasaki, T ;
Kim, JH ;
Mizuhashi, S ;
Satoh, M .
JOURNAL OF ELECTRONIC MATERIALS, 2005, 34 (05) :647-654